Sintered Titanium and Porous Titanium Foam Sheet, 10 µm Filtration Rating, 200 × 200 × 2.8 mm, 110 PPI, 1 Piece
Research-grade laboratory product
|
|||||||||||||||||||||||||||||||||||||||||||||||
|
|||||||||||||||||||||||||||||||||||||||||||||||
|
LABORATORY PROCUREMENT SUPPORT
For filtration accuracy, dimensional confirmation, material compatibility or custom configuration review, contact our technical sales team.
E-MAIL: inquiry@atomfair.com
|
|||||||||||||||||||||||||||||||||||||||||||||||
|
Manufacturer: Atomfair LLC
Brand: ATOMFAIR®
|
This document specifies handling, integration, and cleaning constraints for the sintered porous titanium foam sheet. It defines limits for surface integrity, process compatibility, and thermal service.
- Surface Integrity: Protect the porous surface from crushing and contamination before and during installation.
- Integration Processing: Cut, weld, or machine the sheet using standard metalworking methods when integrating it into an assembly.
- Process Compatibility Review: Review media compatibility, operating pressure, temperature, target flow, and dimensional tolerance before installation.
- Service Temperature Limit: Do not operate the sheet above its stated recommended service temperature.
- Cleaning Procedure Selection: Select backflushing, steam, ultrasonic, or compatible chemical cleaning according to the process medium and operating procedure.
This procedure describes the recommended handling, integration, and cleaning steps for a sintered porous titanium foam sheet. The sheet must be protected from surface damage and cleaned using process-compatible methods.
Required Equipment: Cutting tools, Welding equipment, Basic machining tools, Cleaning equipment (backflush, steam, or ultrasonic)
- Inspect the sheet
Inspect the sheet for surface damage or contamination before handling. - Confirm operating conditions
Confirm media compatibility, operating pressure, temperature, and target flow before installation. - Protect the porous surface
Protect the porous surface from crushing and contamination while integrating the sheet into the assembly. - Integrate the sheet
Integrate the sheet using cutting, welding, or basic machining methods as required by the assembly design. - Clean according to process
Clean the sheet periodically using backflushing, steam, ultrasonic, or compatible chemical methods selected for the process medium.
How does the 110 PPI pore density affect the 10 µm filtration efficiency of this titanium foam sheet?
The 110 PPI (pores per inch) indicates a cellular structure with approximately 0.23 mm cell spacing, while the 10 µm filtration rating defines the particle size retained. The 35–45% porosity ensures interconnected flow paths, and the relative air permeability of 5×10⁻⁵ L/(cm²·min·Pa) supports stable separation. The PPI and micron rating are independent parameters; both must be reviewed together to match the sheet to an assembly.
Can this 200×200×2.8 mm sintered titanium sheet be cut or welded into custom shapes for integration into existing filtration assemblies?
Yes. The metallic construction can support cutting, welding, and basic machining for assembly integration, according to the product specifications. However, the porous surface must be protected from crushing and contamination during processing. Custom dimensions are also available upon consultation with the technical sales team.
What cleaning methods are recommended for this porous titanium foam sheet to maintain its filtration performance and avoid damage?
Recommended cleaning methods include backflushing, steam, ultrasonic, and compatible chemical procedures, as stated in the product documentation. The porous surface should be protected from crushing and contamination. The choice of method depends on the process medium and operating procedure.
This sintered titanium foam sheet provides 10 µm filtration precision with a 110 PPI interconnected porous structure in a 200×200×2.8 mm format, offering corrosion resistance and thermal stability up to 300°C, but requires careful handling to avoid pore damage and verification of media compatibility and operating conditions.
Positive
- 10 µm filtration with 110 PPI structure: The 10 µm filtration rating combined with 110 PPI cellular structure provides precise solid-liquid, gas-solid, and gas-liquid separation with interconnected flow paths and low flow resistance.
- Corrosion-resistant and thermally stable titanium: Titanium-based porous construction offers corrosion resistance, heat tolerance up to 300°C, and cleanability via backflushing, steam, ultrasonic, or chemical methods for reuse in compatible media.
Trade-offs
- Temperature limit of 300°C: Recommended service temperature is ≤300°C, restricting use in high-temperature processes above this threshold without confirming material grade and compatibility.
- Requires careful handling to avoid damage: The porous surface must be protected from crushing and contamination; appropriate cleaning methods must be selected based on process medium to maintain filtration integrity.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).