Sintered Titanium and Porous Titanium Foam Sheet, 10 µm Filtration Rating, 160 × 160 × 15 mm, 60 PPI, 1 Piece
Research-grade laboratory product
|
|||||||||||||||||||||||||||||||||||||||||||||||
|
|||||||||||||||||||||||||||||||||||||||||||||||
|
LABORATORY PROCUREMENT SUPPORT
For filtration accuracy, dimensional confirmation, material compatibility or custom configuration review, contact our technical sales team.
E-MAIL: inquiry@atomfair.com
|
|||||||||||||||||||||||||||||||||||||||||||||||
|
Manufacturer: Atomfair LLC
Brand: ATOMFAIR®
|
The sheet must not exceed 300°C service temperature to avoid structural degradation. The porous surface must be protected from crushing and contamination during handling and cleaning.
- Temperature Limit: Recommended service temperature is ≤300°C.
- Handling Constraint: Protect the porous surface from crushing and contamination.
- Cleaning Constraint: Choose backflushing, steam, ultrasonic or chemical cleaning according to the process medium and operating procedure.
- Media Compatibility: Review media compatibility, operating pressure, temperature, target flow and dimensional tolerance before quotation or installation.
Inspect the sheet for damage before installation. Protect the porous surface from crushing and contamination during handling and cleaning.
Required Equipment: Backflushing system, Steam cleaning equipment, Ultrasonic bath, Chemical cleaning agents
- Inspect the sheet
Inspect the sheet for visible damage or contamination before installation. - Select cleaning method
Select a cleaning method—backflushing, steam, ultrasonic, or chemical—based on the process medium and operating procedure. - Apply cleaning procedure
Apply the chosen cleaning procedure while protecting the porous surface from crushing. - Verify cleanliness
Verify that the sheet is free of residual contaminants before reinstallation.
How does the 60 PPI pore density affect the pressure drop and filtration efficiency for 10 µm particulate removal?
The 60 PPI structure provides a cell spacing of approximately 0.42 mm and a porosity of 35–45%, creating interconnected flow paths. The relative air permeability is 5 × 10⁻⁵ L/(cm²·min·Pa), and the general air permeability range is 1.5–800 m³/(h·m²·kPa). This combination supports low flow resistance for a 10 µm filtration rating, but the exact pressure drop depends on the fluid viscosity, flow rate, and contaminant load. The 35–45% porosity ensures open pathways while maintaining mechanical integrity.
What are the chemical compatibility and temperature limitations for this sintered titanium foam sheet in corrosive environments?
The sheet is made from titanium or titanium alloy, which offers inherent corrosion resistance in many media, but compatibility must be verified for the specific process fluid. The recommended service temperature is ≤300°C, and the product is not universally compatible with all chemicals (e.g., strong reducing acids or chloride environments may require review). The manufacturer advises confirming media compatibility, operating pressure, and temperature before installation.
What are the recommended cleaning and handling procedures to maintain the structural integrity and filtration performance of the 10 µm titanium foam sheet?
The porous surface must be protected from crushing and contamination. Approved cleaning methods include backflushing, steam cleaning, ultrasonic cleaning, and compatible chemical cleaning procedures, depending on the process medium. The metallic structure can support cutting, welding, and basic machining for integration, but care should be taken to avoid damaging the interconnected pore network. Regular cleaning according to the manufacturer's guidelines helps preserve the 10 µm filtration rating and flow characteristics.
This 10 µm, 60 PPI sintered titanium foam sheet in a 160 × 160 × 15 mm format provides an interconnected 35–45% porous metallic structure suited to filtration and separation trials, with corrosion resistance and cleanability balanced against a 300°C service ceiling and required media-compatibility checks.
Positive
- Interconnected porosity with corrosion resistance: The 35–45% porosity with approximately 0.42 mm cell spacing supports interconnected liquid and gas flow pathways, while the titanium-based structure provides corrosion resistance and thermal stability in compatible media up to 300°C.
- Cleanable and machinable metallic medium: The metallic construction permits cutting, welding, and basic machining for assembly integration, and the sheet can be cleaned by backflushing, steam, ultrasonic, or compatible chemical procedures for reuse in suitable process conditions.
Trade-offs
- Service temperature limited to 300°C: Recommended service temperature is ≤300°C, so higher-temperature process streams require separate qualification before installation.
- Porous surface needs handling protection: The porous surface must be protected from crushing and contamination during handling, and media compatibility, operating pressure, temperature, target flow, and dimensional tolerance must be reviewed before installation.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).