Sintered Titanium and Porous Titanium Foam Sheet, 50 µm Filtration Rating, 160 × 160 × 20 mm, 40 PPI, 1 Piece
Research-grade laboratory product
|
|||||||||||||||||||||||||||||||||||||||||||||||
|
|||||||||||||||||||||||||||||||||||||||||||||||
|
LABORATORY PROCUREMENT SUPPORT
For filtration accuracy, dimensional confirmation, material compatibility or custom configuration review, contact our technical sales team.
E-MAIL: inquiry@atomfair.com
|
|||||||||||||||||||||||||||||||||||||||||||||||
|
Manufacturer: Atomfair LLC
Brand: ATOMFAIR®
|
The sintered porous titanium foam sheet requires handling and cleaning procedures that preserve its open-pore structure. Media compatibility, operating pressure, temperature, and filtration rating must be confirmed before service.
- Service Temperature Limit: Recommended service temperature is limited to 300°C.
- Handling Protection: The porous surface must be protected from crushing and contamination during handling.
- Cleaning Compatibility: Cleaning may be performed by backflushing, steam, ultrasonic, or compatible chemical procedures.
- Machining Compatibility: The metallic structure may be cut, welded, or machined for assembly integration.
- Pre-installation Review: Operating pressure, temperature, and media compatibility must be reviewed before installation.
The sintered titanium foam sheet requires protected handling to preserve its porous structure. Cleaning method selection depends on the process medium and the facility's operating procedure.
Required Equipment: Backflushing system, Steam cleaner, Ultrasonic cleaner, Chemical cleaning agents
- Inspect the sheet
Inspect the porous sheet for visible contamination, crushing, or surface damage before installation. - Protect the porous surface
Protect the porous surface from crushing and contamination during handling and assembly. - Verify service conditions
Verify media compatibility and confirm operating temperature does not exceed the recommended service limit. - Select a cleaning method
Select a cleaning method based on the process medium and the facility's operating procedure. - Apply the cleaning procedure
Apply backflushing, steam, ultrasonic, or compatible chemical cleaning to restore flow paths. - Dry before reinstalling
Allow the cleaned sheet to dry completely before reinstalling it into the assembly.
How does the 50 µm filtration rating relate to the 40 PPI pore density, and what are the implications for flow rate and retention?
The 50 µm filtration rating specifies the particle size retained, while the 40 PPI (pores per inch) describes the cellular structure density. The product has an approximate cell spacing of 0.64 mm and 35–45% porosity, providing interconnected flow paths. Higher PPI generally increases retention but may reduce flow; the relative air permeability is 1×10⁻³ L/(cm²·min·Pa). Users should review both values together to match specific separation requirements.
Can this sintered titanium foam sheet be machined or welded into custom assemblies, and what are the temperature limits for service?
Yes, the metallic construction supports cutting, welding, and basic machining for assembly integration. The recommended service temperature is ≤300°C. Media compatibility must be reviewed for corrosion resistance, as titanium provides corrosion resistance in compatible media. Custom dimensions are available upon consultation with technical sales.
What cleaning methods are recommended for this porous titanium foam sheet to maintain its filtration performance?
The sheet can be cleaned using backflushing, steam, ultrasonic, or compatible chemical procedures. The porous surface should be protected from crushing and contamination. The choice of cleaning method depends on the process medium and operating procedure. The metallic structure supports repeated cleaning and reuse.
This AF-T40-D2050 sintered porous titanium sheet is assessed for its 50 µm filtration rating, 40 PPI cellular structure, 35–45% porosity, and approximately 0.64 mm cell spacing in a 160 × 160 × 20 mm format. It is suitable for porous-metal filtration, flow-distribution, and porous-electrode evaluations where an interconnected titanium network is needed, provided the 300°C service temperature limit is respected and the porous surface is protected from mechanical damage.
Positive
- Interconnected high-vacuum sintered titanium structure: Powder-formed, high-vacuum sintered titanium with 35–45% porosity and approximately 0.64 mm cell spacing provides interconnected through-pore paths, supporting low-resistance solid-liquid, gas-solid, and gas-liquid separation.
- 50 µm rating with cleanable reusable porous metal: The 50 µm filtration rating, uniform pore distribution, corrosion-resistant titanium construction, and cleaning options such as backflushing, steam, ultrasonic, and compatible chemical procedures permit reuse in suitable filtration workflows.
Trade-offs
- Maximum recommended service temperature of 300°C: The sheet's recommended service temperature is ≤300°C, so higher-temperature streams require explicit compatibility review before installation.
- Porous surface vulnerable to crushing and contamination: The porous surface must be protected from crushing and contamination, and media compatibility, operating pressure, temperature, target flow, and dimensional tolerance must be reviewed before installation.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).