Sintered Titanium and Porous Titanium Foam Sheet, 10 µm Filtration Rating, 100 × 100 × 3 mm, 110 PPI, 1 Piece
Research-grade laboratory product
|
|||||||||||||||||||||||||||||||||||||||||||||||
|
|||||||||||||||||||||||||||||||||||||||||||||||
|
LABORATORY PROCUREMENT SUPPORT
For filtration accuracy, dimensional confirmation, material compatibility or custom configuration review, contact our technical sales team.
E-MAIL: inquiry@atomfair.com
|
|||||||||||||||||||||||||||||||||||||||||||||||
|
Manufacturer: Atomfair LLC
Brand: ATOMFAIR®
|
The sheet must be protected from crushing and contamination to preserve its porous structure and filtration integrity. Cleaning methods include backflushing, steam, ultrasonic, or compatible chemical procedures depending on the process medium.
- Service Temperature Limit: Recommended service temperature does not exceed 300°C.
- Media Compatibility Requirement: Media compatibility, operating pressure, and temperature must be reviewed before installation.
- Structural Integrity Note: The metallic construction supports cutting, welding, and basic machining for assembly integration.
Protect the porous surface from physical damage and contamination during handling and storage. Select a cleaning method appropriate for the process medium and operating procedure.
Required Equipment: Backflushing system, Steam cleaning equipment, Ultrasonic bath
- Inspect the sheet
Inspect the sheet for visible damage or contamination before installation. - Install the sheet
Install the sheet into the filtration assembly ensuring a secure seal without crushing the porous structure. - Select cleaning method
Select a cleaning method based on the process medium and operating procedure. - Clean the sheet
Clean the sheet using backflushing, steam, ultrasonic, or compatible chemical procedures as appropriate. - Verify cleanliness
Verify that the porous surface is free of residual contaminants before reuse.
How does the 110 PPI cellular structure relate to the 10 µm filtration rating in this sintered titanium foam sheet?
The 110 PPI (pores per inch) describes the cellular structure, while the 10 µm value specifies filtration precision. These are independent parameters; PPI governs the pore density and cell spacing (~0.23 mm), whereas the filtration rating indicates the particle size retained. Both need to be evaluated together when matching the sheet to an assembly.
What is the maximum service temperature for the Atomfair sintered titanium foam sheet?
The recommended maximum service temperature is 300°C. The sheet is made from titanium or titanium alloy via high-vacuum sintering, providing thermal stability and corrosion resistance within this limit.
What cleaning and machining methods are suitable for this porous titanium sheet?
The metallic construction supports cutting, welding, and basic machining for assembly integration. Cleaning options include backflushing, steam, ultrasonic, and compatible chemical procedures, as stated in the product handling guidelines.
This 100 × 100 × 3 mm sintered titanium foam sheet combines a 10 µm filtration rating with a 110 PPI open-cell structure, 35–45% interconnected porosity, and a ≤300°C service limit, suiting laboratory filtration, catalyst recovery, and porous-electrode studies.
Positive
- Interconnected porosity enables low-resistance 10 µm filtration: The sintered titanium network provides 35–45% open porosity with interconnected through-pores, delivering a 10 µm filtration rating while preserving flow pathways for solid-liquid, gas-solid, and gas-liquid separation.
- Titanium structure offers corrosion resistance and cleanability: The titanium/titanium-alloy sintered body is corrosion resistant and heat tolerant, and can be regenerated by backflushing, steam, ultrasonic, or compatible chemical cleaning for reuse.
Trade-offs
- Process compatibility must be confirmed before installation: Media compatibility, operating pressure, target flow, temperature, and dimensional tolerance must be reviewed against the assembly before quotation or installation because separation performance is process-dependent.
- Porous surface requires protection from crushing and contamination: The porous surface can be damaged by crushing or contamination, so handling and cleaning procedures must be selected according to the process medium and operating protocol.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).