Zirconia Ceramic Plate, 100 mm x 100 mm x 0.5 mm, Pack of 10, WhiteProduct Type: Zirconia ceramic plate
Research-grade laboratory product
|
|||||||||||||||||||||||||||||||||||||||||||||||||
|
|||||||||||||||||||||||||||||||||||||||||||||||||
|
LABORATORY PROCUREMENT SUPPORT
For model selection, accessory matching, platform compatibility or configuration confirmation, contact our technical sales team.
E-MAIL: inquiry@atomfair.com
|
|||||||||||||||||||||||||||||||||||||||||||||||||
|
Manufacturer: Atomfair LLC
Brand: ATOMFAIR?
|
The zirconia ceramic plate must not exceed a maximum service temperature of 1600°C to maintain structural integrity. Thermal shock resistance is limited to 350°C, requiring controlled heating and cooling rates to avoid fracture.
- Maximum Service Temperature: Operate below 1600°C to prevent degradation of the ceramic structure.
- Thermal Shock Resistance: Limit temperature change rates to within 350°C to avoid thermal cracking.
- Water Absorption: The plate's zero water absorption makes it suitable for humid environments without dimensional change.
- Thermal Conductivity: Account for a thermal conductivity of 3 W/(m·K) when designing heat dissipation pathways.
What is the maximum service temperature of the Atomfair Zirconia Ceramic Plate and how does its thermal shock resistance compare?
The maximum service temperature is 1600 °C, while the thermal shock resistance is 350 °C. This means the plate can withstand a sudden temperature change of up to 350 °C without cracking, which is a critical trade-off for applications involving rapid heating or cooling cycles.
What are the dielectric properties of this zirconia ceramic plate for high-frequency insulation applications?
The plate has a dielectric constant of 12.5 at 1 MHz, a dielectric breakdown strength of 15 KT/m, and a volume resistivity greater than 1 × 10^12 Ω·cm. These properties make it suitable for electrical insulation in high-temperature environments where stable dielectric performance is required.
How should the 0.5 mm thick zirconia ceramic plate be handled to avoid damage during installation?
The plate is only 0.5 mm thick with high hardness (1400 HV) and compressive strength (25,000 kgf/cm²), but as a dense ceramic it requires careful handling to avoid edge chipping or cracking from impact or bending. Proper support during mounting and avoidance of point loads are recommended.
This 100 mm x 100 mm x 0.5 mm zirconia ceramic plate (ZrO2 ≥94%, density 5.9 g/cm³) provides high hardness (1400 HV), compressive strength (25,000 kgf/cm²), electrical insulation (volume resistivity >1×10¹² Ω·cm), and thermal stability up to 1600 °C, making it suitable for high-temperature jigs, insulators, and wear-resistant substrates. The 0.5 mm thickness and zero water absorption trade off mechanical robustness for thermal shock resistance (350 °C) and low thermal conductivity (3 W/(m·K)), requiring careful handling during clamping or thermal cycling.
Positive
- High-temperature electrical insulation: Volume resistivity >1×10¹² Ω·cm and dielectric breakdown strength 15 kV/mm at 1 MHz enable reliable electrical isolation in furnaces, sputtering targets, or plasma chambers up to 1600 °C, with negligible ionic conductivity in the ZrO2 lattice at elevated temperatures per the specification.
- Wear and corrosion resistance: Hardness of 1400 HV, compressive strength of 25,000 kgf/cm², and zero water absorption provide exceptional resistance to abrasive wear, chemical attack from acids/alkalis, and thermal cycling fatigue, reducing replacement frequency in high-throughput laboratory environments.
Trade-offs
- Brittleness at thin section: At 0.5 mm thickness and high hardness, the plate lacks ductility and may fracture under point loading or uneven clamping forces; mechanical support and uniform pressure distribution are required during handling and mounting to avoid catastrophic failure.
- Thermal shock limitation: Thermal shock resistance of 350 °C constrains rapid temperature changes; abrupt quenching or heating above this gradient can induce microcracking in the ZrO2 matrix, limiting use in processes with fast thermal cycles without preheating or ramping protocols.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).