Sintered Titanium and Porous Titanium Foam Sheet, 30 µm Filtration Rating, 100 × 100 × 5 mm, 30 PPI, 1 Piece
Research-grade laboratory product
|
|||||||||||||||||||||||||||||||||||||||||||||||
|
|||||||||||||||||||||||||||||||||||||||||||||||
|
LABORATORY PROCUREMENT SUPPORT
For filtration accuracy, dimensional confirmation, material compatibility or custom configuration review, contact our technical sales team.
E-MAIL: inquiry@atomfair.com
|
|||||||||||||||||||||||||||||||||||||||||||||||
|
Manufacturer: Atomfair LLC
Brand: ATOMFAIR®
|
This sintered porous titanium sheet requires review of media compatibility and operating limits before installation. Handling must preserve the porous structure, and cleaning must be matched to the process medium.
- Media Compatibility Review: Confirm that the titanium or titanium-alloy structure is compatible with the process medium before installation.
- Operating Temperature Limit: Do not exceed the recommended 300°C service temperature without reviewing material grade and media compatibility.
- Porous Surface Protection: Protect the porous surface from crushing and contamination during handling, cutting, welding, or machining.
- Cleaning Method Selection: Select backflushing, steam, ultrasonic, or chemical cleaning according to the process medium and operating procedure.
- Installation Parameter Review: Review operating pressure, temperature, target flow, and dimensional tolerance before installation.
Prepare the sintered titanium sheet by confirming operating conditions and protecting the porous structure. Use process-appropriate handling and cleaning methods to maintain filtration performance.
- Confirm Operating Requirements
Confirm the filtration rating, PPI, sheet dimensions, material grade, target flow, operating pressure, temperature, and media compatibility before installation. - Protect Porous Surface
Protect the porous surface from crushing and contamination during handling and assembly integration. - Select Cleaning Procedure
Select backflushing, steam, ultrasonic, or chemical cleaning according to the process medium and operating procedure after use.
How does the 30 µm filtration rating interact with the 30 PPI cellular structure to influence flow resistance and particle retention in this sintered titanium foam sheet?
The 30 µm rating defines the particle size cutoff, while the 30 PPI structure provides an approximate cell spacing of 0.85 mm and 35–45% porosity, with a relative air permeability of 5×10⁻⁴ L/(cm²·min·Pa). Together, they balance filtration precision and open flow paths. The manufacturer explicitly advises reviewing both values together to match the sheet to the target assembly.
What is the maximum service temperature for this sintered titanium foam sheet, and which cleaning methods are compatible with its porous structure?
The recommended service temperature is ≤300°C. The titanium-based porous structure supports cleaning by backflushing, steam, ultrasonic, and compatible chemical procedures. However, the porous surface must be protected from crushing and contamination during handling and cleaning.
Can this 100×100×5 mm sintered titanium sheet be cut or welded for integration into existing assemblies, and what procurement checks are critical before installation?
Yes, the metallic construction supports cutting, welding, and basic machining for assembly integration. Before quotation or installation, users must confirm filtration rating, PPI, sheet dimensions, material grade, target flow, operating pressure, temperature, and media compatibility. The sheet’s 35–45% porosity and interconnected pathways must be preserved during any modification.
This 100 × 100 × 5 mm sintered porous titanium foam sheet combines a 30 µm filtration rating with a 30 PPI cellular structure, 35–45% porosity, and approximately 0.85 mm cell spacing for interconnected liquid and gas flow paths. Its high-vacuum sintered titanium framework offers corrosion resistance, thermal tolerance up to 300°C, and cleanability, making it suitable for laboratory filtration trials and engineered separation assemblies once media compatibility and operating conditions are confirmed.
Positive
- Interconnected porous flow paths: The 35–45% porosity range with approximately 0.85 mm cell spacing and through-pore structure supports solid-liquid, gas-solid, and gas-liquid separation while providing a relative air permeability of 5 × 10^-4 L/(cm²·min·Pa).
- Cleanable sintered titanium media: The metallic porous structure tolerates backflushing, steam, ultrasonic, and compatible chemical cleaning, and is rated for recommended service up to 300°C, enabling reuse in compatible process conditions.
Trade-offs
- Surface damage and contamination sensitivity: The porous surface must be protected from crushing and contamination, and cleaning methods must be selected according to the process medium and operating procedure to preserve the 30 µm filtration structure.
- Media and operating condition validation required: Media compatibility, operating pressure, temperature, target flow, and dimensional tolerance must be reviewed before quotation or installation; both PPI and micron rating must be considered together when matching the sheet to an assembly.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).