Description
Product Overview
Core Specifications & Performance Parameters
|
Specification Item
|
Specific Parameters
|
|---|---|
|
Chemical Composition
|
Li1.5Al0.5Ge1.5P3O12 (LAGP)
|
|
Melting Point
|
1350℃
|
|
Shape & Size
|
Circular: d19mm/d25mm; Square: 2in*2in; Customization supported (compatible with various split test batteries)
|
|
Thickness
|
300um (0.30mm)
|
|
Density
|
>95% theoretical density
|
|
Grain Size
|
~25um
|
|
Ionic Conductivity (25℃, Room Temperature)
|
4.5×10⁻⁴ S/cm
|
|
Physical Stability
|
Stable in air and aqueous environments
|
|
Sales Model
|
Small-batch sales
|
|
Target Application
|
New materials R&D, lithium-ion metal-air battery research
|
Core Functional Advantages
Dual Performance of Isolation & Ion Conduction
Superior Chemical & Environmental Stability
Flexible Compatibility & Customization
Application Scenarios
-
Lithium-ion Metal-air Battery Assembly & Testing: Serves as the core solid electrolyte and isolation layer for experimental battery cells, supporting performance verification of new battery systems.
-
Solid Electrolyte Material R&D: Provides a standard LAGP-based test sample for researching ceramic electrolyte modification, performance optimization, and material compatibility.
-
Split-type Battery Experimentation: Matches various disassembled test battery platforms, facilitating in-depth analysis of battery electrochemical performance and failure mechanisms.
Quality Compliance
-
The LAGP ceramic material is manufactured in accordance with ISO 9001 quality management standards, ensuring batch consistency and purity control.
-
Dimensional accuracy meets ASTM C200 ceramic component precision specifications, matching the assembly requirements of laboratory test batteries.
-
Ionic conductivity testing adheres to IEC 62638 electrochemical performance test protocols for solid electrolytes, guaranteeing the reliability of performance data.