4-Inch Antimony-Doped Silicon Wafer 525μm SSP ATOMFAIR®

Price range: $189.00 through $399.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Prime CZ N-type Sb wafer, 0.005–0.02 Ω·cm, 525 ± 25 μm, SSP Ra < 0.5 nm. SEMI M1 flats, 10/25 pcs cassettes. Order now.

Diameter & Flat:
4-Inch (100.0 ± 0.3 mm)
Primary Flat 32.5 mm <110>
Substrate & Dopant:
CZ N-Type / Antimony (Sb)
<100>•0.005–0.02 Ω·cm
Thickness:
525 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
SSP (Ra < 0.5 nm)
Polished Front / Fine-Ground Back

4-Inch (100 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Antimony-doped to a verified resistivity of 0.005–0.02 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 100.0 ± 0.3 mm diameter and 525 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.

Heavily Antimony (Sb)-doped to 0.005–0.02 Ω·cm (N+) (~1.5×1018–1.2×1019 cm-3 donor concentration), Antimony exhibits very low solid-state diffusivity and exceptionally low vapor-phase out-diffusion (“autodoping”) during elevated-temperature LPCVD and epitaxial processes. It serves as an industry-standard low-resistance base for abrupt silicon epitaxy, trench power MOSFETs, discrete Schottky barriers, and buried-layer R&D.

Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.

4-Inch (100 mm) Thickness & Process Compatibility Note: The industry-standard 525 ± 25 μm mechanical thickness offers high flexural rigidity across full-wafer photolithography steppers, PECVD/LPCVD cassettes, epitaxial susceptors, and automated handling chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Single-Side Polished (SSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)

SEMI M1 4-Inch Dimensional Precision

Standardized 100.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.

  • Diameter: 100.0 ± 0.3 mm (4.0 Inch)
  • Primary Flat: 32.5 ± 2.5 mm along <110> ± 1°
  • Secondary Flat: 18.0 ± 2.0 mm secondary flat located 180° ± 5° from primary flat (SEMI M1 100 mm N<100>)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant N-Type / Antimony (Sb) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 0.005–0.02 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <100> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 100.0 ± 0.3 mm (4-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 525 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 32.5 ± 2.5 mm SEMI M1 (100 mm)
Secondary Flat 18.0 ± 2.0 mm secondary flat located 180° ± 5° from primary flat (SEMI M1 100 mm N<100>) SEMI M1 (100 mm N<100>)
Surface Polish & Roughness Single-Side Polished (SSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Total Thickness Variation (TTV) & Bow/Warp TTV < 5 μm•Bow / Warp < 30 μm Non-Contact Optical Flatness
Surface Particle Inspection ≤ 10 particles / wafer (Cleanroom Audit) Bright-Light & Laser Surface Scan
Available Pack Sizes 10 pcs, 25 pcs cleanroom protective cassettes Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications

  • Thin-Film Deposition & Epitaxial Growth: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures clean, defect-free nucleation for Si/SiGe/III-V epitaxy, ALD, PVD sputtering, and high-resolution photolithography;
  • Power Devices, Epitaxy & Anisotropic MEMS: Standard <100> crystal plane supports abrupt epitaxial layer growth, vertical discrete power diodes/MOSFETs, and KOH/DRIE micromachining;
  • Semiconductor Device & Epitaxial Prototyping: Controlled Antimony-doped (0.005–0.02 Ω·cm) base for ohmic contacts, power/RF devices, epitaxial growth, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.

Packaging, Storage & Handling Protocol

Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 4-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters, dopants, and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 4-Inch (100 mm), N-Type Antimony (100), 0.005-0.02 ohm-cm, 525 um, SSP (This Product) 4-Inch (100 mm) / SSP 525 ± 25 μm, N-Type Antimony (0.005–0.02 Ω·cm) SEMI M1 525 μm 100 mm wafer in 10 pcs / 25 pcs cassettes
4-Inch N-Type Arsenic <100> Wafer (0.001–0.005 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, N++ As <100> Low-strain, low-diffusivity As-doped epi & MOSFET substrate
4-Inch N-Type <110> Wafer (1–10 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, N-Type <110> Vertical-sidewall KOH MEMS & <110> lattice transport wafer
4-Inch N-Type <111> High-Res Wafer (100–1000 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, High-Res N <111> High-resistivity hexagonal <111> wafer for RF & III-nitride epi
4-Inch N-Type <100> Wafer (1–10 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, N-Type <100> Standard SEMI M1 525 μm 100 mm N-type lithography substrate

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 4-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Prime-grade virgin monocrystalline silicon substrates require cleanroom-compatible storage and edge-only manipulation to preserve CMP surface quality. Environmental exposure to particulate contamination, corrosive vapors, and ambient moisture must be minimized prior to downstream processing.

  • Cleanroom Cassette Storage: Store unused wafers sealed inside the original cleanroom polypropylene cassette within a dry nitrogen cabinet or desiccator to limit airborne organic contamination.
  • Edge-Only Manipulation: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid contacting the polished front surface.
  • Native Oxide Awareness: Bare prime silicon forms an ambient native silicon dioxide film of approximately 1 to 2 nm in air, which must be removed by wet processing before metallization or epitaxy where an ohmic interface is required.
  • Wet-Chemical Processing Controls: Perform solvent cleaning, RCA standard clean, or native oxide removal strictly inside an exhaust fume hood or wet bench using facility-approved protocols and institutional EHS and SDS safety procedures.
  • Corrosive Vapor Exclusion: Keep wafers away from particulate dust and corrosive vapors during storage to prevent surface degradation of the CMP finish.

Preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs. Follow sequential solvent cleaning, plasma descum, and controlled storage to maintain prime-grade surface quality.

Required Equipment: Cleanroom vacuum wand, PTFE or PEEK tweezers, Cleanroom polypropylene cassette, Dry nitrogen cabinet or cleanroom desiccator

  1. Inspect Cassette and Wafer Edges
    Inspect the cleanroom cassette and wafer edges for particulate contamination or physical damage before removing any substrate.
  2. Transfer by Perimeter Edge
    Transfer the wafer using a cleanroom vacuum wand or PTFE/PEEK tweezers applied only to the perimeter edge.
  3. Degrease in Solvent Sequence
    Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and deionized water.
  4. Dry and Plasma Descum
    Dry the wafer with nitrogen blow-drying followed by a mild oxygen plasma descum prior to photoresist spin coating or PVD/ALD deposition.
  5. Remove Native Oxide Where Required
    Perform native oxide removal or RCA standard clean inside an exhaust fume hood or wet bench using facility-approved protocols when an ohmic interface is required before metallization or epitaxy.
  6. Return Unused Wafers to Sealed Storage
    Return unused wafers to the original cleanroom polypropylene cassette box and store within a dry nitrogen cabinet to minimize airborne organic contamination.

Why choose antimony-doped silicon wafers over arsenic or phosphorus for epitaxial power device fabrication?

Antimony (Sb) doping is selected for its exceptionally low solid-state diffusivity and minimal vapor-phase out-diffusion (autodoping) during high-temperature LPCVD and epitaxial processes, which preserves abrupt doping profiles at the substrate-epi interface. This 4-inch wafer is doped to 0.005–0.02 Ω·cm (N+), corresponding to roughly 1.5×10^18–1.2×10^19 cm^-3 donor concentration, making it an industry-standard low-resistance base for trench power MOSFETs, discrete Schottky barriers, and buried-layer R&D. Compared to arsenic or phosphorus, antimony's low diffusivity reduces dopant migration into the growing epitaxial layer, enabling sharper junctions and more predictable device characteristics.

Can this 4-inch N-type antimony wafer be used for KOH anisotropic wet etching and MEMS micromachining?

Yes. The <100> (± 0.5°) crystal orientation supports predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions, with clean perpendicular cleaving along <110> planes. The cubic surface exhibits four-fold rotational symmetry and low Si/SiO2 interface state density, which are advantageous for MEMS and vertical device structures. The primary flat is oriented along <110> ± 1° per SEMI M1, ensuring accurate mask alignment for anisotropic etch processes.

What cleanroom handling and storage procedures are required to maintain the surface quality of these prime SSP wafers?

These wafers feature a single-side polished (SSP) front surface with Ra < 0.5 nm and ≤ 10 particles per wafer, so they must be handled strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface contact. Store unused wafers sealed inside the original cleanroom polypropylene cassette within a dry nitrogen cabinet or cleanroom desiccator, away from particulate dust and corrosive vapors. Bare prime silicon forms a ~1–2 nm native SiO2 film in air; if native oxide removal or RCA cleaning is required before metallization or epitaxy, perform wet processing in an exhaust fume hood or wet bench following institutional EHS and SDS protocols.

The 4-inch prime CZ silicon wafer with antimony doping (0.005–0.02 Ω·cm) and <100> orientation offers a low-diffusivity, low-autodoping substrate ideal for epitaxial and power device prototyping, while its 525 μm thickness and SEMI M1 flats ensure compatibility with standard cleanroom handling. However, its bare surface requires stringent cleanroom protocols to prevent contamination and native oxide growth.

Positive

  • Low Autodoping Antimony Dopant: Antimony's low solid-state diffusivity and vapor-phase out-diffusion minimize autodoping during high-temperature LPCVD and epitaxial processes, enabling abrupt doping profiles for power devices and buried-layer R&D.
  • SEMI M1 Dimensional Precision: Standardized 100.0 mm diameter and crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes, reducing handling errors in automated lithography.

Trade-offs

  • Bare Surface Contamination Risk: The absence of a protective coating necessitates strict cleanroom handling and storage in dry nitrogen cabinets to prevent particulate and organic contamination, which can degrade thin-film nucleation.
  • Native Oxide Formation: Ambient exposure forms a 1–2 nm native SiO2 layer that must be removed via wet etching or RCA clean before metallization or epitaxy, requiring exhaust fume hoods and facility-approved protocols.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

10 pcs, 25 pcs

Diameter

4-Inch (100.0 ± 0.3 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

N-Type / Antimony (Sb)

Orientation

± 0.5°

Resistivity

0.005-0.02 Ω·cm

Thickness

525 ± 25 μm

Surface Finish

Single-Side Polished (SSP, Ra < 0.5 nm)