4-Inch N-Type Silicon Wafer 525μm Prime Grade ATOMFAIR®

Price range: $159.00 through $329.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Prime CZ N-Type silicon wafer, 100mm, 525±25μm, 1–10 Ω·cm, SSP Ra<0.5nm. SEMI M1 flats. In stock.

Diameter & Flat:
4-Inch (100.0 ± 0.3 mm)
Primary Flat 32.5 mm <110>
Substrate & Dopant:
CZ N-Type / Phosphorus (P)
<100>•1–10 Ω·cm
Thickness:
525 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
SSP (Ra < 0.5 nm)
Polished Front / Fine-Ground Back

4-Inch (100 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Phosphorus-doped to a verified resistivity of 1–10 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 100.0 ± 0.3 mm diameter and 525 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.

Doped with Phosphorus to an industry-standard 1–10 Ω·cm n-type semiconducting range (~4.5×1014–5×1015 cm-3 donor density), the wafer provides uniform majority-electron transport for PMOS/CMOS device R&D, Schottky barrier rectifiers, PECVD/ALD dielectric C-V profiling, and cleanroom thin-film deposition.

Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.

4-Inch (100 mm) Thickness & Process Compatibility Note: The industry-standard 525 ± 25 μm mechanical thickness offers high flexural rigidity across full-wafer photolithography steppers, PECVD/LPCVD cassettes, tube oxidation boats, and automated handling chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Single-Side Polished (SSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)

SEMI M1 4-Inch Dimensional Precision

Standardized 100.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.

  • Diameter: 100.0 ± 0.3 mm (4.0 Inch)
  • Primary Flat: 32.5 ± 2.5 mm along <110> ± 1°
  • Secondary Flat: 18.0 ± 2.0 mm secondary flat located 180° ± 5° from primary flat (SEMI M1 100 mm N<100>)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant N-Type / Phosphorus (P) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 1–10 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <100> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 100.0 ± 0.3 mm (4-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 525 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 32.5 ± 2.5 mm SEMI M1 (100 mm)
Secondary Flat 18.0 ± 2.0 mm secondary flat located 180° ± 5° from primary flat (SEMI M1 100 mm N<100>) SEMI M1 (100 mm N<100>)
Surface Polish & Roughness Single-Side Polished (SSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Total Thickness Variation (TTV) & Bow/Warp TTV < 5 μm•Bow / Warp < 30 μm Non-Contact Optical Flatness
Surface Particle Inspection ≤ 10 particles / wafer (Cleanroom Audit) Bright-Light & Laser Surface Scan
Available Pack Sizes 10 pcs, 25 pcs cleanroom protective cassettes Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications

  • Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for PVD sputtering, ALD, e-beam evaporation, and high-resolution photoresist spin coating;
  • MEMS & Anisotropic Silicon Micromachining: Cleanroom <100> crystal plane supports KOH / TMAH wet anisotropic etching and Bosch deep reactive ion etching (DRIE);
  • Semiconductor Device & Electrode Prototyping: Controlled Phosphorus-doped (1–10 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.

Packaging, Storage & Handling Protocol

Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 4-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters, thicknesses, and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 4-Inch (100 mm), N-Type (100), 1-10 ohm-cm, 525 um, SSP (This Product) 4-Inch (100 mm) / SSP 525 ± 25 μm, N-Type (1–10 Ω·cm) SEMI M1 525 μm 100 mm wafer in 10 pcs / 25 pcs cassettes
4-Inch N-Type <100> Wafer (1–10 Ω·cm, 525 μm DSP) 4-Inch (100 mm) / DSP 525 ± 25 μm, N-Type <100> Double-side CMP polished N-type wafer for IR optics & wafer bonding
4-Inch N-Type <111> Wafer (1–10 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, N-Type <111> Hexagonal <111> N-type substrate for III-nitride epitaxy & UHV growth
4-Inch P-Type <110> Wafer (1–10 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, P-Type <110> Vertical-sidewall KOH MEMS & high hole-mobility <110> lattice
4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, P-Type <100> Complementary Boron-doped P-type <100> 100 mm reference substrate

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 4-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Prime-grade virgin silicon wafers require cleanroom-compatible storage and edge-only handling to preserve the CMP-polished surface. Environmental exposure to particulates, corrosive vapors, and ambient moisture must be minimized to prevent surface contamination and uncontrolled native oxide growth.

  • Particulate and Organic Contamination Control: Store wafers sealed inside the original cleanroom polypropylene cassette within a dry nitrogen cabinet or desiccator to limit airborne organic and particulate contamination.
  • Native Oxide Formation: Bare prime silicon develops an ambient native SiO2 film of approximately 1–2 nm in air, which must be removed by wet processing or RCA clean before metallization or epitaxy if an oxide-free interface is required.
  • Edge-Only Mechanical Handling: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid scratching or contaminating the mirror-polished front surface.
  • Corrosive Vapor and Moisture Exposure: Keep wafers away from particulate dust and corrosive vapors, as these can degrade the polished surface and alter surface chemistry prior to deposition or lithography.
  • Wet-Chemical Processing Safety: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols, including the use of exhaust fume hoods or wet benches for RCA cleans and native oxide removal.

Proper handling and pre-cleaning of prime CZ silicon wafers preserves the CMP-polished surface and ensures reproducible thin-film interfaces. The following steps outline solvent degreasing, plasma descum, and cassette storage procedures for cleanroom processing.

Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Cleanroom polypropylene cassette, Dry nitrogen cabinet or cleanroom desiccator, O2 plasma descum system

  1. Inspect wafer cassette and packaging
    Inspect the cleanroom protective cassette for seal integrity and verify that wafers are immobilized without edge contact before opening.
  2. Transfer wafer by perimeter edge
    Transfer the wafer using a cleanroom vacuum wand or PTFE/PEEK tweezers applied only to the perimeter edge, avoiding contact with the polished front surface.
  3. Degrease in solvent sequence
    Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and DI water to remove organic residues prior to further processing.
  4. Dry and descum surface
    Blow-dry the wafer with N2 and apply a mild O2 plasma descum to remove residual organics before photoresist spin coating or PVD/ALD deposition.
  5. Remove native oxide if required
    Perform wet processing inside an exhaust fume hood or wet bench using facility-approved protocols when native oxide removal or RCA standard clean is required before metallization or epitaxy.
  6. Store unused wafers in nitrogen cabinet
    Return unused wafers to the original cleanroom polypropylene cassette and store sealed inside a dry nitrogen cabinet to minimize airborne organic contamination.

What is the difference between SSP and DSP 4-inch silicon wafers for thin-film deposition?

This wafer is single-side polished (SSP): the front surface is CMP-polished to Ra < 0.5 nm while the back is fine-ground. That front-side finish is sufficient for uniform PVD, ALD, e-beam evaporation, and photoresist spin coating. A double-side polished (DSP) wafer would only be necessary if you need a polished back surface for IR transmission or wafer bonding; for standard front-side lithography and deposition, SSP is the appropriate and more economical choice.

Can I use this N-type <100> wafer for KOH anisotropic wet etching of MEMS structures?

Yes. The <100> (± 0.5°) crystal orientation supports predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions, and the clean perpendicular cleaving along <110> planes aids die separation. The primary flat is oriented along <110> ± 1° (32.5 ± 2.5 mm), which provides the reference needed for mask alignment to the crystal axes. For through-wafer features, note the 525 ± 25 μm thickness when calculating etch times.

How should I store and handle these prime silicon wafers to avoid contamination before processing?

Keep unused wafers sealed in the original cleanroom polypropylene cassette inside a dry nitrogen cabinet or cleanroom desiccator, away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers; never touch the polished face. Bare prime silicon carries only a ~1–2 nm native oxide, so minimize ambient exposure before thermal oxidation or epitaxy, and perform any wet-chemical cleans in an exhaust fume hood or wet bench per institutional EHS and SDS protocols.

The 4-inch prime CZ N-type <100> SSP wafer with 1–10 Ω·cm resistivity and 525 µm thickness provides a verified, SEMI M1-compliant substrate for thin-film deposition, MEMS micromachining, and device prototyping. Its single-side CMP finish (Ra < 0.5 nm) and bare silicon surface enable direct in-house oxidation and epitaxy, though cleanroom handling and dry storage are mandatory to preserve surface quality.

Positive

  • CMP Mirror Surface for Thin-Film Growth: Single-side polished front with Ra < 0.5 nm ensures uniform nucleation for PVD, ALD, e-beam evaporation, and high-resolution photoresist spin coating.
  • SEMI M1 Dimensional Precision: Standardized 100.0 mm diameter and crystal alignment flats enable accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.

Trade-offs

  • Cleanroom Handling Required: Wafers must be handled strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface contamination and mechanical damage.
  • Dry Storage Needed: Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors to prevent native oxide growth and organic contamination.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

10 pcs, 25 pcs

Diameter

4-Inch (100.0 ± 0.3 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

N-Type / Phosphorus (P)

Orientation

± 0.5°

Resistivity

1-10 Ω·cm

Thickness

525 ± 25 μm

Surface Finish

Single-Side Polished (SSP, Ra < 0.5 nm)