4-Inch N-Type Silicon Wafer 1-10 Ω·cm ATOMFAIR®

Price range: $179.00 through $379.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Prime-grade 4-inch (100 mm) CZ N-type silicon wafer, orientation, 1–10 Ω·cm, 525 ± 25 μm, SSP Ra < 0.5 nm. SEMI M1 flats. In stock.

Diameter & Flat:
4-Inch (100.0 ± 0.3 mm)
Primary Flat 32.5 mm
Substrate & Dopant:
CZ N-Type / Phosphorus (P)
<110>•1–10 Ω·cm
Thickness:
525 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
SSP (Ra < 0.5 nm)
Polished Front / Fine-Ground Back

4-Inch (100 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Phosphorus-doped to a verified resistivity of 1–10 Ω·cm along the <110> (± 0.5°) crystal orientation. Manufactured to a 100.0 ± 0.3 mm diameter and 525 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.

Doped with Phosphorus to an industry-standard 1–10 Ω·cm n-type semiconducting range (~4.5×1014–5×1015 cm-3 donor density), the wafer provides uniform majority-electron transport for MOSFET/CMOS device R&D, Schottky rectifiers, PECVD/ALD C-V profiling, and thin-film metrology.

Sliced along the high-symmetry <110> (± 0.5°) crystal plane, the substrate exposes two sets of {111} etch-stop planes intersecting perpendicular to the wafer surface (at 70.5° / 109.5° in-plane angles), enabling anisotropic KOH/TMAH wet etching of atomically smooth, near-vertical (∼90°) high-aspect-ratio trench sidewalls as well as crystal-axis carrier mobility studies.

4-Inch (100 mm) Thickness & Process Compatibility Note: The industry-standard 525 ± 25 μm mechanical thickness offers high flexural rigidity across full-wafer photolithography steppers, PECVD/LPCVD cassettes, epitaxial susceptors, and automated handling chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Single-Side Polished (SSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)

SEMI M1 4-Inch Dimensional Precision

Standardized 100.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.

  • Diameter: 100.0 ± 0.3 mm (4.0 Inch)
  • Primary Flat: 32.5 ± 2.5 mm precision orientation flat (<111> / <110> verified per lot CoA)
  • Secondary Flat: Single-flat 100 mm <110> research wafer configuration (flat & crystal axes verified per lot CoA)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant N-Type / Phosphorus (P) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 1–10 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <110> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 100.0 ± 0.3 mm (4-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 525 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Length: 32.5 ± 2.5 mm•Axis: <111> / <110> flat (lot CoA verified) SEMI M1 (100 mm)
Secondary Flat Single-flat 100 mm <110> research wafer configuration (flat & crystal axes verified per lot CoA) SEMI M1 (100 mm <110>)
Surface Polish & Roughness Single-Side Polished (SSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Total Thickness Variation (TTV) & Bow/Warp TTV < 5 μm•Bow / Warp < 30 μm Non-Contact Optical Flatness
Surface Particle Inspection ≤ 10 particles / wafer (Cleanroom Audit) Bright-Light & Laser Surface Scan
Available Pack Sizes 10 pcs, 25 pcs cleanroom protective cassettes Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications

  • Thin-Film Deposition & Epitaxial Growth: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures clean, defect-free nucleation for Si/SiGe/III-V epitaxy, ALD, PVD sputtering, and high-resolution photolithography;
  • Vertical-Sidewall MEMS & Directional Transport Devices: Perpendicular {111} etch-stop planes in <110> silicon enable vertical high-aspect-ratio KOH/TMAH microchannels, microfluidic trenches, and axis-dependent FET studies;
  • Semiconductor Device & Epitaxial Prototyping: Controlled Phosphorus-doped (1–10 Ω·cm) base for ohmic contacts, power/RF devices, epitaxial growth, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.

Packaging, Storage & Handling Protocol

Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 4-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters, dopants, and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 4-Inch (100 mm), N-Type (110), 1-10 ohm-cm, 525 um, SSP (This Product) 4-Inch (100 mm) / SSP 525 ± 25 μm, N-Type Phosphorus (1–10 Ω·cm) SEMI M1 525 μm 100 mm wafer in 10 pcs / 25 pcs cassettes
4-Inch N-Type Arsenic <100> Wafer (0.001–0.005 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, N++ As <100> Low-strain, low-diffusivity As-doped epi & MOSFET substrate
4-Inch N-Type Antimony <100> Wafer (0.005–0.02 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, N+ Sb <100> Minimal autodoping Sb-doped wafer for sharp high-T epitaxy
4-Inch N-Type <111> High-Res Wafer (100–1000 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, High-Res N <111> High-resistivity hexagonal <111> wafer for RF & III-nitride epi
4-Inch N-Type <100> Wafer (1–10 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, N-Type <100> Standard SEMI M1 525 μm 100 mm N-type lithography substrate

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 4-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Prime-grade virgin silicon substrates require cleanroom-compatible handling to preserve sub-nanometer surface quality and prevent particulate or metallic contamination. Environmental exposure must be minimized because ambient air forms a native oxide and airborne organics degrade the polished front surface.

  • Cleanroom Handling Requirement: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid scratching or contaminating the polished surface.
  • Storage Atmosphere Control: Store unused wafers sealed inside the original cleanroom cassette within a dry nitrogen cabinet or desiccator to minimize native oxide growth and airborne organic contamination.
  • Wet Processing Safety: Perform all wet-chemical cleaning, native oxide removal, or RCA standard cleans strictly inside an exhaust fume hood or wet bench following institutional EHS and SDS protocols.
  • Thermal Budget Constraint: Account for the 525 ± 25 μm thickness and prime-grade surface when designing thermal oxidation or epitaxial processes, as excessive thermal stress can induce slip or warp beyond the specified < 30 μm limit.

Proper handling and pre-cleaning of prime silicon wafers preserves surface quality and ensures reproducible thin-film and lithography results. The following steps outline edge-only manipulation, solvent cleaning, native oxide control, and safe storage.

Required Equipment: Cleanroom vacuum wand, PTFE or PEEK tweezers, Exhaust fume hood or wet bench, Dry nitrogen cabinet or cleanroom desiccator

  1. Inspect Cassette and Wafer
    Inspect the cleanroom cassette and wafer edges for particulate contamination or physical damage before opening in a controlled environment.
  2. Handle by Perimeter Edge
    Transfer the wafer using a cleanroom vacuum wand or PTFE/PEEK tweezers applied only to the perimeter edge.
  3. Perform Solvent Pre-Cleaning
    Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and deionized water, then blow-dry with nitrogen.
  4. Remove Native Oxide if Required
    Perform wet-chemical native oxide removal or RCA standard clean inside an exhaust fume hood or wet bench using facility-approved protocols.
  5. Dry and Verify Surface
    Dry the wafer with filtered nitrogen and verify surface cleanliness under bright light before proceeding to deposition or lithography.
  6. Store Unused Wafers Properly
    Return unused wafers to the original cleanroom cassette and store sealed inside a dry nitrogen cabinet or desiccator.

Why choose a <110> oriented silicon wafer over standard <100> for MEMS or trench etching?

The <110> crystal orientation exposes two sets of {111} etch-stop planes that intersect perpendicular to the wafer surface, enabling anisotropic KOH or TMAH wet etching to produce near-vertical (~90°) high-aspect-ratio trench sidewalls. In contrast, standard <100> silicon yields sloped sidewalls defined by the 54.7° angle between {100} and {111} planes. This makes the <110> substrate specifically suited for vertical-sidewall MEMS, microfluidic trenches, and crystal-axis carrier mobility studies.

Can this 4-inch N-type <110> wafer be used directly for thermal oxidation or epitaxial growth without additional surface preparation?

Yes, the wafer is a bare prime silicon substrate with a single-side polished (SSP) front surface (Ra < 0.5 nm) and a fine-ground back, allowing direct in-house thermal oxidation, LPCVD, or epitaxial growth. However, it carries only a thin ambient native oxide (~1–2 nm), so for critical epitaxy or ohmic contact formation, an RCA standard clean or native oxide removal is recommended. All wet processing must follow institutional EHS and SDS protocols.

What are the storage and handling requirements to maintain the surface quality of this prime silicon wafer?

Store wafers sealed inside the original cleanroom protective cassette within a dry nitrogen cabinet or cleanroom desiccator to minimize airborne organic contamination and particle deposition. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers; never touch the polished face. The cassettes are engineered to immobilize 4-inch wafer edges and prevent surface contact during transit.

This 4-inch prime CZ N-type <110> silicon wafer (1–10 Ω·cm, 525 μm, SSP) is a well-characterized research substrate whose perpendicular {111} etch-stop planes and sub-nanometer CMP finish make it particularly suited to anisotropic KOH/TMAH micromachining and epitaxial nucleation studies. Its value depends on cleanroom discipline: bare prime silicon requires edge-only handling, dry nitrogen storage, and facility-approved wet-bench protocols to preserve the polished interface.

Positive

  • <110> Orientation Enables Vertical Etch Stops: The <110> (± 0.5°) crystal plane exposes two sets of {111} etch-stop planes intersecting perpendicular to the surface, enabling anisotropic KOH/TMAH wet etching of near-vertical (~90°) high-aspect-ratio trench sidewalls for MEMS and microfluidic structures.
  • Sub-Nanometer CMP Front Surface: Single-side polished front with Ra < 0.5 nm supports reproducible thin-film nucleation for Si/SiGe/III-V epitaxy, ALD, PVD sputtering, and high-resolution photolithography, while the fine-ground back aids handling.
  • Verified Prime-Grade Batch Traceability: Each lot ships with a Certificate of Analysis documenting four-point-probe resistivity (1–10 Ω·cm), XRD orientation, SEMI M1 thickness (525 ± 25 μm), and cleanroom particle inspection (≤ 10 particles/wafer), supporting reproducible process qualification.

Trade-offs

  • Bare Surface Requires Strict Cleanroom Handling: Uncoated prime silicon carries only a ~1–2 nm ambient native oxide and is vulnerable to particulate and organic contamination; wafers must be handled by the perimeter edge with vacuum wands or PTFE/PEEK tweezers and stored sealed in a dry nitrogen cabinet or desiccator.
  • Wet Processing Needs EHS-Approved Infrastructure: Native oxide removal, RCA cleans, and KOH/TMAH etching require an exhaust fume hood or wet bench operating under institutional EHS and SDS protocols; facilities without compliant wet-processing infrastructure cannot safely exploit the <110> anisotropic etch capability.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

10 pcs, 25 pcs

Diameter

4-Inch (100.0 ± 0.3 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

N-Type / Phosphorus (P)

Orientation

± 0.5°

Resistivity

1-10 Ω·cm

Thickness

525 ± 25 μm

Surface Finish

Single-Side Polished (SSP, Ra < 0.5 nm)