NVP Electrode Sheet 20 mg/cm2 Dry Process ATOMFAIR®

$109.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Research grade NVP electrode sheet with 20 mg/cm2 single-side dry coating, 120 × 90 mm active area, 5 sheets/pack; ISO 9001 processed. Order now.

Quantity Price
1 – 4 $109.00
5+ $99.00
SKU: AF-BM-S-CNVP-AS20-5P00
Category:
Brands:

ATOMFAIR® NVP-S03 SODIUM VANADIUM PHOSPHATE (NVP) ELECTRODE SHEET

RESEARCH GRADE MATERIAL

Product Overview

Atomfair NVP-S03 Sodium Vanadium Phosphate (NVP) Electrode Sheet is single-side coated with 20 mg/cm² via a precise dry process. Ideal for sodium-ion battery R&D, this specialized cathode architecture delivers exceptional reliability for electrochemical performance analysis, ensuring cell-to-cell consistency, baseline testing control, variable elimination, and electrolyte validation platform benefits while nesting target sodium vanadium phosphate electrode sheet price structures to optimize laboratory validation integrity.

Technical Specifications

PARAMETER DETAILS
1. Core Device & Electrochemical Design
Product Code S03
Capacity 110 mAh/g
Coating Process Dry Process
2. Cathode Parameters
Coating Material NVP (Sodium Vanadium Phosphate)
Active Material Ratio 94.50%
Coating Density 20 mg/cm2
Coating Area 120 × 90 mm
Coating Type Single-sided
Compaction Density 1.5 g/cm3
3. Substrate & Foil Parameters
Substrate Material Carbon-coated aluminum foil matrix crystals
Current Collector Density 4.2 mg/cm2
Substrate Thickness 12 + 0.5 + 0.5 μm
Substrate Size 90 × 140 mm
4. Compliance & Support
Pack Size 5 sheets/pack
Manufacturing Rules Processed under strict ISO 9001 compliance conditions
Alternative Options Explore our related catalog or custom dimensions. For urgent technical custom requests or bulk inquiries, please contact our support team.

Key Features & Advantages

  • Homogeneous Material Purity: Features an optimized active material ratio of 94.50% to deliver a robust, highly uniform NVP distribution across half-cell foils testing matrices.
  • Enhanced Operational Efficiency: Built on advanced carbon-coated aluminum foil substrates to maximize electrical contact, optimize boundary interfacial dynamics, and promote material evaluation accuracy.
  • Advanced Dry Process technology: Precise dry process single-sided coating coordinates an exceptionally uniform 20 mg/cm² loading profile across the 120 × 90 mm active area, securing reliable high-fidelity data outputs.
  • Tailored Solutions: Full customization options available for coating thickness, localized width, and current collector structural profiles to meet exact experimental specifications.

APPLICATION SCOPE: Sodium-ion battery Research and Development (R&D), laboratory testing, material evaluation, and reliable electrochemical performance analysis.
PACKAGING: 5 electrode sheets per pack (Substrate size: 90 × 140 mm), packaged meticulously to ensure consistent quality during laboratory baseline evaluations.
IMPORTANT NOTICE: This product is sold exclusively for laboratory research. Recommended baking protocol: Maintain strictly for 12 hours under vacuum at 100°C to prevent ambient phase contamination or structural degradation before thermal validation.

TAILORED SOLUTIONS FOR RESEARCH
Contact our engineering team for technical support or official institutional quotations.
EMAIL: inquiry@atomfair.com
Manufacturer: ATOMFAIR LLC
Brand: ATOMFAIR®

This electrode sheet requires vacuum baking at 100°C for 12 hours before use to prevent ambient phase contamination and structural degradation. The sheet is intended for research use only and should be used in a controlled environment.

  • Baking Protocol: Vacuum bake the sheet at 100°C for 12 hours prior to use.

The electrode sheet must be vacuum baked at 100°C for 12 hours to remove ambient contamination. Use a vacuum oven capable of maintaining 100°C and vacuum levels.

Required Equipment: Vacuum oven

  1. Place sheets in oven
    Place the NVP electrode sheets into a vacuum oven, ensuring they are not overlapping.
  2. Set temperature
    Set the oven temperature to 100°C and allow it to stabilize.
  3. Evacuate chamber
    Evacuate the oven chamber to achieve vacuum conditions suitable for the sheets.
  4. Bake for 12 hours
    Maintain the vacuum and temperature for 12 hours to ensure complete removal of contaminants.

What vacuum baking protocol is recommended for the NVP-S03 sodium vanadium phosphate electrode sheet before use?

The NVP-S03 electrode sheet should be baked for 12 hours under vacuum at 100°C to prevent ambient phase contamination or structural degradation before thermal validation.

What substrate material is used in the NVP-S03 electrode sheet and how does it improve electrical performance?

The substrate is a carbon-coated aluminum foil matrix crystals that maximizes electrical contact and optimizes boundary interfacial dynamics, thereby enhancing material evaluation accuracy.

What are the active material ratio and coating density of the NVP-S03 electrode sheet?

The active material ratio is 94.50% and the coating density is 20 mg/cm², providing a highly uniform NVP distribution across the 120 × 90 mm active area for reliable electrochemical performance analysis.

Atomfair NVP-S03 sodium vanadium phosphate electrode sheet provides a single-side coated cathode with 20 mg/cm² loading on carbon-coated aluminum foil, featuring a 94.5% active material ratio and dry process uniformity for reliable sodium-ion battery R&D. Requires strict vacuum baking at 100°C for 12 hours prior to use.

Positive

  • High active material ratio for uniformity: Optimized active material ratio of 94.50% ensures homogeneous NVP distribution across the electrode, promoting consistent electrochemical performance in half-cell testing.
  • Uniform dry process coating: Precise dry process single-sided coating delivers a highly uniform 20 mg/cm² loading over a 120 × 90 mm active area, securing reliable high-fidelity data outputs for baseline testing and electrolyte validation.

Trade-offs

  • Strict pre-use baking protocol required: Electrode sheets must be vacuum-baked at 100°C for 12 hours before thermal validation to prevent ambient phase contamination or structural degradation, demanding laboratory vacuum oven infrastructure and process control.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).