Lithium niobate evaporation material requires specific evaporation source hardware and liner materials for optimal deposition. The Z-ratio of 0.463 must be used for accurate thickness monitoring during e-beam evaporation.
- Evaporation Source Preference: E-beam evaporation is preferred for this material, while thermal evaporation requires RFQ and is limited to compatible liner materials.
- Liner Material Compatibility: Use graphite, alumina, or boron nitride liners for e-beam evaporation, or tungsten, molybdenum, or tantalum boats for thermal evaporation.
- Material Form and Sizing: Pieces sized 1–3 mm are selected to ensure consistent source loading and controlled evaporation behavior.
- Thickness Monitoring: The Z-ratio of 0.463 must be programmed into the deposition controller for accurate film thickness measurement.
What is the Z-ratio of this LiNbO3 evaporation material and why is it critical for e-beam deposition?
The Z-ratio is 0.463. This value is required for accurate quartz crystal microbalance (QCM) thickness monitoring during e-beam evaporation; an incorrect Z-ratio leads to systematic film thickness errors. The Z-ratio must be programmed into the deposition controller to ensure correct tooling factor and final film thickness.
What evaporation source hardware is compatible with LiNbO3 pieces supplied in 1–3 mm size?
The material is compatible with e-beam evaporation using a hearth lined with graphite, Al2O3, or BN, or with W, Mo, or Ta boats. Thermal evaporation is possible by request for quotation (RFQ). The 1–3 mm piece size is suitable for direct loading into these sources without additional processing.
Lithium Niobate (LiNbO3) evaporation material in pieces (1-3 mm, 99.9% purity) is evaluated for vacuum thin-film deposition. The specified form and purity support controlled E-beam evaporation, while thermal evaporation requires RFQ and specific liner/boat hardware. The provided Z-ratio (0.463) aids process calibration.
Positive
- Defined Material Identity and Purity: Lithium Niobate (LiNbO3) at 99.9% purity ensures clear procurement and deposition-process matching for standard and high-purity film requirements.
- Specified Physical Form (1-3 mm Pieces): The pieces form with 1-3 mm dimensions supports consistent source loading and evaporation rate control in E-beam or thermal boats.
Trade-offs
- E-beam Preferred; Thermal by RFQ Only: Thermal evaporation requires RFQ and specific hardware (graphite/Al2O3/BN liner or W/Mo/Ta boat), limiting method flexibility without prior confirmation.
- Requires Pre-Order Compatibility Checks: Buyers must confirm model, purity, form, size range, pack size, and deposition-source compatibility before quotation to avoid procurement mismatches.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).