Atomfair GH4169 Nickel-Based Superalloy Material

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

GH4169 is a Ni-based precipitation-hardened superalloy, boasting excellent fatigue resistance, radiation resistance, oxidation resistance, and corrosion resistance. It also features good processability, weldability, and long-term microstructural stability. Ideal for disks, rings, blades, shafts, fasteners, elastic components, plate structures, and casings. Compatible with SLM and LSF processes.

SKU: AFMSKKME055
Category:
Brands:

High-performance precipitation-strengthened nickel alloy material.

Chemical Composition (wt.%)
C 0.02-0.06
Cr 17.0-21.0
Ni 50.0-55.0
Co ≤1.0
Mo 2.8-3.3
Fe Balance
Ti 0.65-1.15
Nb 5.0-5.5
Mn ≤0.35
P ≤0.015
S ≤0.015
B ≤0.006
Si ≤0.35
N ≤0.02
Mg ≤0.01
Cu ≤0.3
Physical Properties
D10 (μm) ≥15
D50 (μm) 30-40
D90 (μm) ≤58
Sphericity ≥0.9
Apparent Density (g/cm³) ≥4.4
Tapped Density (g/cm³) ≥5.0
Flowability (s/50g) ≤18
Mechanical Properties
Condition Tensile Strength (MPa) Yield Strength (MPa) Elongation (%)
Room Temperature ≥1300 ≥1100 ≥15.0
650°C ≥1000 ≥900 ≥12.0
650°C Stress Rupture: 690MPa, ≥100h

Applications: Disks, rings, blades, shafts, fasteners, elastic components, sheet structures, and casings.

Processing Methods: SLM, LSF.

Features: Excellent fatigue resistance, radiation resistance, oxidation resistance, corrosion resistance, along with good machinability, weldability, and long-term microstructure stability.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).