GH4099 is a Ni-based precipitation-hardened superalloy, suitable for long-term service below 900°C and short-term use up to 1000°C. It exhibits excellent thermal strength and good hot/cold work formability, making it ideal for high-temperature welded structural components like aero-engine combustion chambers and afterburners. Compatible with the SLM process.

SKU: AFMSWRFL719
Category:
Brands:
Chemical Composition (wt.%)
Ni Balance
Cr 17.0-20.0
Co 5.0-8.0
Mo 5.0-7.0
Al 3.5-4.5
Ti 1.7-2.4
C ≤0.08
Mg ≤0.01
Ce ≤0.02
B ≤0.005
Fe ≤2.0
P ≤0.015
S ≤0.015
Mn ≤0.4
Si ≤0.5
O ≤0.02
N ≤0.02
Physical Properties
Particle Size (μm) D10≥15, D50:30-40, D90≤58
Sphericity ≥0.9
Apparent Density (g/cm³) ≥4.4
Tapped Density (g/cm³) ≥5.0
Flowability (s/50g) ≤18
Mechanical Properties (Heat Treated)
Condition Tensile Strength (MPa) Yield Strength (MPa) Elongation (%)
Room Temp ≥1000 ≥600 ≥35.0
900°C ≥400 ≥350 ≥15.0

Precipitation-hardened nickel-based superalloy for long-term service below 900°C (short-term up to 1000°C). Excellent thermal strength and formability. Typical applications include aero-engine combustion chambers and afterburner components.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).