4-Inch N-Type Silicon Wafer 0.001-0.005 Ω·cm DSP ATOMFAIR®

Price range: $229.00 through $499.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Prime CZ N-Type silicon wafer, 100 mm, 500 ± 15 μm, 0.001–0.005 Ω·cm, DSP Ra < 0.5 nm. SEMI M1 flats. In stock.

Diameter & Flat:
4-Inch (100.0 ± 0.3 mm)
Primary Flat 32.5 mm <110>
Substrate & Dopant:
CZ N-Type / Phosphorus (P)
<100>•0.001–0.005 Ω·cm
Thickness:
500 ± 15 μm
Prime-Grade Virgin Wafer
Surface Polish:
DSP (Ra < 0.5 nm)
Dual-Side Mirror-Polished (CMP)

4-Inch (100 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Phosphorus-doped to a verified resistivity of 0.001–0.005 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 100.0 ± 0.3 mm diameter and 500 ± 15 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).

Degenerately Phosphorus-doped to 0.001–0.005 Ω·cm (N++) (~1019–1020 cm-3 electron density), the wafer delivers metallic-like bulk conductivity for low-resistance backside ohmic contacts, conductive bottom gates, III-V/GaN buffer heteroepitaxy, and high-current device testing.

Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.

4-Inch (100 mm) Thickness & Process Compatibility Note: The 500 ± 15 μm tight-tolerance thickness suits precision MEMS micromachining, double-side alignment lithography, DRIE through-etching, and reproducible capacitive cavity fabrication. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Double-Side Polished (DSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)

SEMI M1 4-Inch Dimensional Precision

Standardized 100.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.

  • Diameter: 100.0 ± 0.3 mm (4.0 Inch)
  • Primary Flat: 32.5 ± 2.5 mm along <110> ± 1°
  • Secondary Flat: 18.0 ± 2.0 mm secondary flat located 180° ± 5° from primary flat (SEMI M1 100 mm N<100>)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant N-Type / Phosphorus (P) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 0.001–0.005 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <100> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 100.0 ± 0.3 mm (4-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 500 ± 15 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 32.5 ± 2.5 mm SEMI M1 (100 mm)
Secondary Flat 18.0 ± 2.0 mm secondary flat located 180° ± 5° from primary flat (SEMI M1 100 mm N<100>) SEMI M1 (100 mm N<100>)
Surface Polish & Roughness Double-Side Polished (DSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Total Thickness Variation (TTV) & Bow/Warp TTV < 3 μm•Bow / Warp < 25 μm Non-Contact Optical Flatness
Surface Particle Inspection ≤ 10 particles / wafer (Cleanroom Audit) Bright-Light & Laser Surface Scan
Available Pack Sizes 10 pcs, 25 pcs cleanroom protective cassettes Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications

  • Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm) supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding;
  • MEMS & Anisotropic Silicon Micromachining: Cleanroom <100> crystal plane supports KOH / TMAH wet anisotropic etching and Bosch deep reactive ion etching (DRIE);
  • Semiconductor Device & Electrode Prototyping: Controlled Phosphorus-doped (0.001–0.005 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.

Packaging, Storage & Handling Protocol

Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 4-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters, thicknesses, and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 4-Inch (100 mm), N-Type (100), 0.001-0.005 ohm-cm, 500 um, DSP (This Product) 4-Inch (100 mm) / DSP 500 ± 15 μm, N-Type (0.001–0.005 Ω·cm) SEMI M1 500 μm 100 mm wafer in 10 pcs / 25 pcs cassettes
4-Inch N-Type <100> Wafer (1–10 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, N-Type <100> Standard SEMI M1 525 μm 100 mm N-type lithography substrate
4-Inch N-Type <100> Wafer (1–10 Ω·cm, 525 μm DSP) 4-Inch (100 mm) / DSP 525 ± 25 μm, N-Type <100> Double-side CMP polished N-type wafer for IR optics & wafer bonding
4-Inch N-Type <111> Wafer (1–10 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, N-Type <111> Hexagonal <111> N-type substrate for III-nitride epitaxy & UHV growth
4-Inch P-Type <110> Wafer (1–10 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, P-Type <110> Vertical-sidewall KOH MEMS & high hole-mobility <110> lattice

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 4-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Prime-grade monocrystalline silicon wafers require cleanroom handling to prevent particulate contamination and surface damage. Storage must be in a dry nitrogen cabinet or desiccator to minimize native oxide growth and airborne organic contamination.

  • Cleanroom Handling Requirement: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface contact and contamination.
  • Storage Environment: Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.
  • Native Oxide Sensitivity: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air, requiring controlled wet processing for removal before metallization or epitaxy.
  • Wet Processing Safety: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols.

Proper handling and pre-cleaning procedures preserve mirror-polished CMP cleanliness and ensure reproducible thin-film interfaces. Sequential solvent cleaning followed by plasma descum prepares wafers for photoresist spin coating or PVD/ALD.

Required Equipment: Cleanroom vacuum wands or PTFE/PEEK tweezers, Cleanroom polypropylene cassette box, Dry nitrogen cabinet or cleanroom desiccator, Exhaust fume hood or wet bench

  1. Inspect wafer cassette
    Inspect the cleanroom protective cassette for integrity and verify that wafers are immobilized without surface contact.
  2. Handle by perimeter edge
    Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
  3. Degrease sequentially
    Degrease diced dies or whole 4-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water.
  4. Blow-dry with nitrogen
    Blow-dry the wafer surface with N2 to remove residual solvent and water.
  5. Perform plasma descum
    Perform a mild O2 plasma descum prior to photoresist spin coating or PVD/ALD deposition.
  6. Store unused wafers
    Store unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet.

Can a 0.001–0.005 Ω·cm N++ silicon wafer be used for standard MOS gate fabrication?

No. At 0.001–0.005 Ω·cm (N++, ~10^19–10^20 cm^-3 electron density), the bulk is degenerately doped and behaves nearly metallically, so it cannot provide the depletion region or threshold-voltage control required for a MOS gate channel. This wafer is intended instead for low-resistance backside ohmic contacts, conductive bottom gates, III-V/GaN buffer heteroepitaxy, and high-current device testing. For conventional MOS gate stacks, select a higher-resistivity substrate such as the 1–10 Ω·cm 4-inch N-type <100> wafers in the same catalog.

Does the 500 ± 15 μm thickness of this 4-inch N++ wafer affect DRIE through-etching or double-side alignment?

The 500 ± 15 μm tight-tolerance thickness is specifically suited to precision MEMS micromachining, double-side alignment lithography, DRIE through-etching, and reproducible capacitive cavity fabrication. The <100> (± 0.5°) orientation supports KOH/TMAH anisotropic wet etching and Bosch DRIE, while the dual-side CMP finish (DSP, Ra < 0.5 nm) enables double-sided patterning and direct fusion/anodic bonding. Note that this is a 500 μm wafer; if your process is qualified for the more common 525 ± 25 μm SEMI M1 thickness, verify your etch-depth and alignment budgets before substituting.

How should these bare prime silicon wafers be stored and handled to preserve the CMP surface before oxidation or epitaxy?

Keep unused wafers sealed inside the original cleanroom polypropylene cassette within a dry nitrogen cabinet or cleanroom desiccator, away from particulate dust and corrosive vapors, and handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), so if native oxide removal or an RCA standard clean is required before metallization or epitaxy, perform wet processing inside an exhaust fume hood or wet bench under facility-approved EHS and SDS protocols. Pre-clean diced dies or whole wafers sequentially in acetone, electronic-grade IPA, and DI water, then N2 blow-dry and apply a mild O2 plasma descum before photoresist spin coating or PVD/ALD.

This 4-inch prime CZ N-type <100> silicon wafer combines degenerate phosphorus doping (0.001–0.005 Ω·cm) with dual-side CMP polishing (Ra < 0.5 nm) and tight 500 ± 15 μm thickness control, making it well-suited for low-resistance ohmic contact prototyping, double-side MEMS lithography, and anisotropic KOH/TMAH micromachining. Its bare, uncoated surface and sub-nanometer finish demand strict cleanroom handling and prompt native-oxide management before downstream thermal or epitaxial processing.

Positive

  • Degenerate N++ Doping for Ohmic Contacts: Phosphorus-doped to 0.001–0.005 Ω·cm (~10^19–10^20 cm^-3), the wafer provides metallic-like bulk conductivity that supports low-resistance backside ohmic contacts, conductive bottom gates, and high-current device testing without additional epi doping steps.
  • Dual-Side CMP Finish for Bonding and Lithography: Double-side mirror polish (DSP, Ra < 0.5 nm) with TTV < 3 μm and bow/warp < 25 μm enables double-sided alignment lithography, direct fusion/anodic wafer bonding, and reproducible thin-film growth on either face.

Trade-offs

  • Native Oxide Requires Pre-Process Removal: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air; wet-chemical removal (e.g., RCA clean or HF-based protocols) inside an exhaust fume hood or wet bench is required before metallization or epitaxy to avoid interfacial resistance.
  • Cleanroom Storage and Handling Mandatory: Sub-nanometer CMP surfaces and ≤10 particles/wafer cleanliness require sealed dry-nitrogen cabinet storage and edge-only handling with vacuum wands or PTFE/PEEK tweezers; exposure to particulate dust or corrosive vapors degrades the polished surface.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

10 pcs, 25 pcs

Diameter

4-Inch (100.0 ± 0.3 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

N-Type / Phosphorus (P)

Orientation

± 0.5°

Resistivity

0.001-0.005 Ω·cm

Thickness

500 ± 15 μm

Surface Finish

Double-Side Polished (DSP, Ra < 0.5 nm)