Prime CZ N-Type silicon wafer, 50.8 mm, 275 μm, 0.01–0.1 Ω·cm, SSP Ra < 0.5 nm. SEMI M1 flats, 25 pcs cassette. In stock.

Diameter & Flat:
2-Inch (50.8 ± 0.2 mm)
Primary Flat 15.88 mm <110>
Substrate & Dopant:
CZ N-Type / Phosphorus (P)
<111>•0.01–0.1 Ω·cm
Thickness:
275 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
SSP (Ra < 0.5 nm)
Polished Front / Fine-Ground Back

1. Scientific Overview & Substrate Electrical Properties

2-Inch (50.8 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Phosphorus-doped to a verified resistivity of 0.01–0.1 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 50.8 ± 0.2 mm diameter and 275 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.

Phosphorus-doped to a low-resistivity range of 0.01–0.1 Ω·cm (N+), the wafer combines low substrate contact resistance with lower free-carrier optical loss than degenerately doped N++ wafers, supporting vertical diode fabrication, anodic glass bonding, and electrochemical electrodes.

Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D.

2-Inch Chamber Compatibility & Surface State Note: The compact 2-inch (50.8 mm) footprint fits research-scale tube furnaces, compact ALD/PECVD chambers, R&D spin coaters, and 2-inch sputtering sample holders without dicing waste. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Single-Side Polished (SSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)
SEMI M1 2-Inch Dimensional Precision

Standardized 50.8 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.

  • Diameter: 50.8 ± 0.2 mm (2.0 Inch)
  • Primary Flat: 15.88 ± 1.65 mm along <110> ± 1°
  • Secondary Flat: Located 45° ± 5° clockwise from primary flat (SEMI M1 50.8 mm N<111>)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant N-Type / Phosphorus (P) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 0.01–0.1 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <111> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 50.8 ± 0.2 mm (2-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 275 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 15.88 ± 1.65 mm SEMI M1 (50.8 mm)
Secondary Flat Located 45° ± 5° clockwise from primary flat (SEMI M1 50.8 mm N<111>) SEMI M1 (50.8 mm N<111>)
Surface Polish & Roughness Single-Side Polished (SSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Pack Size (MOQ) 25 pcs (1 × 25-wafer cleanroom cassette, 25BX) Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications
  • Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for PVD sputtering, ALD, e-beam evaporation, and high-resolution photoresist spin coating;
  • Hexagonal Epitaxy & UHV Surface Physics: Dense three-fold <111> crystal lattice supports lattice-matched GaN/AlN/SiC heteroepitaxy, graphene/TMDC template growth, and discrete bipolar/power prototyping;
  • Semiconductor Device & Electrode Prototyping: Controlled Phosphorus-doped (0.01–0.1 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol

Wafers are supplied in a standard 25-wafer protective cleanroom cassette (25 pcs pack, 25BX) engineered to immobilize 2-inch wafer edges and prevent surface contact during transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 2-Inch (50.8 mm), N-Type (111), 0.01-0.1 ohm-cm, 275 um, SSP (This Product) 2-Inch (50.8 mm) / SSP 275 ± 25 μm, N-Type (0.01–0.1 Ω·cm) SEMI M1 275 μm thickness, 25 pcs cassette for 2-inch R&D chambers
2-Inch P-Type <100> Wafer (1–10 Ω·cm SSP) 2-Inch (50.8 mm) / SSP 275 ± 25 μm, P-Type <100> Standard 50.8 mm P<100> bare lithography substrate
2-Inch P-Type <100> Wafer (1–10 Ω·cm DSP) 2-Inch (50.8 mm) / DSP 275 ± 25 μm, P-Type <100> Double-side CMP polished for IR optics & bonding
2-Inch N-Type <100> Wafer (1–10 Ω·cm SSP) 2-Inch (50.8 mm) / SSP 275 ± 25 μm, N-Type <100> Phosphorus-doped N<100> wafer for Schottky & diode R&D
2-Inch P-Type <111> Wafer (1–10 Ω·cm SSP) 2-Inch (50.8 mm) / SSP 275 ± 25 μm, P-Type <111> Hexagonal <111> lattice for III-nitride & UHV growth

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 2-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original 25-wafer polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Prime-grade monocrystalline silicon wafers require cleanroom-compatible storage and handling to preserve surface quality. Environmental exposure to particulates, corrosive vapors, and uncontrolled humidity must be minimized.

  • Cleanroom Storage Environment: Store wafers sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.
  • Edge-Only Handling: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface contact.
  • Native Oxide Awareness: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air that must be removed before metallization or epitaxy if an oxide-free interface is required.
  • Wet Processing Safety: Perform all wet-chemical or cleanroom processing strictly inside an exhaust fume hood or wet bench following institutional EHS and SDS safety protocols.

Proper handling and pre-cleaning of prime silicon wafers preserves the CMP mirror finish and ensures reproducible thin-film interfaces. Sequential solvent cleaning followed by plasma descum removes organic contamination prior to deposition or lithography.

Required Equipment: Cleanroom vacuum wand, PTFE/PEEK tweezers, O2 plasma descum system, Dry nitrogen cabinet

  1. Inspect wafer cassette
    Inspect the sealed 25-wafer cleanroom cassette for any signs of damage or contamination before opening.
  2. Transfer wafer by edge
    Transfer the wafer from the cassette using a cleanroom vacuum wand or PTFE/PEEK tweezers, contacting only the perimeter edge.
  3. Degrease sequentially
    Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and DI water.
  4. Dry with nitrogen
    Dry the wafer with a nitrogen blow-dry immediately after the final DI water rinse.
  5. Perform plasma descum
    Perform a mild O2 plasma descum to remove residual organic contamination prior to photoresist spin coating or PVD/ALD.
  6. Remove native oxide if required
    Remove the native oxide via wet processing inside an exhaust fume hood or wet bench using facility-approved protocols if an oxide-free interface is required.
  7. Store unused wafers
    Store unused wafers sealed inside the original polypropylene cassette within a dry nitrogen cabinet to minimize airborne organic contamination.

Why choose a 0.01–0.1 Ω·cm N-type <111> silicon wafer instead of a degenerately doped N++ substrate for vertical diode or electrochemical electrode fabrication?

The 0.01–0.1 Ω·cm phosphorus-doped N+ range balances low substrate contact resistance with lower free-carrier optical loss than degenerately doped N++ wafers, which is advantageous for vertical diode fabrication, anodic glass bonding, and electrochemical electrodes. The <111> orientation further provides hexagonal three-fold surface symmetry and a higher in-plane elastic modulus along key cleavage directions, supporting discrete power and bipolar R&D. If your process requires minimum series resistance at the expense of optical loss, an N++ substrate may be preferable; otherwise this N+ specification is the more versatile starting point.

Can this 2-inch N-type <111> prime silicon wafer be used directly for GaN, AlN, or SiC epitaxy without an intermediate buffer layer?

The wafer is supplied as bare prime silicon with only a thin ambient native oxide (~1–2 nm) and no deposited coating, so it is intended as a starting substrate for in-house epitaxial or thin-film growth rather than a ready-to-use template. Its densely packed <111> (± 0.5°) crystal plane supports III-nitride and hexagonal epitaxy (GaN, AlN, SiC) as well as UHV surface reconstruction studies, but lattice mismatch still requires an appropriate nucleation or buffer strategy. For lattice-matched growth, the <111> surface symmetry is advantageous; for direct high-quality III-nitride deposition, standard buffer-layer engineering remains necessary.

What cleanroom handling and storage conditions are required to preserve the Ra < 0.5 nm CMP surface of this SSP silicon wafer before thermal oxidation or photolithography?

Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers, and keep unused wafers sealed in the original 25-wafer polypropylene cassette inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Before photoresist spin coating or PVD/ALD, degrease sequentially in acetone, electronic-grade IPA, and DI water, followed by N2 blow-drying and a mild O2 plasma descum. Note that bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air; if native oxide removal or RCA cleaning is required before metallization or epitaxy, perform wet processing strictly in an exhaust fume hood or wet bench under facility-approved EHS and SDS protocols.

The 2-inch N-type <111> prime silicon wafer with 0.01–0.1 Ω·cm phosphorus doping and SSP finish (Ra < 0.5 nm) is engineered for hexagonal epitaxy, vertical diode prototyping, and in-house oxidation, but its bare surface, <111> orientation, and 275 µm thickness impose specific pre-clean, handling, and thermal budget constraints.

Positive

  • Low-resistivity N+ doping: Phosphorus-doped to 0.01–0.1 Ω·cm, the substrate provides low contact resistance for vertical diodes and electrochemical electrodes while maintaining lower free-carrier optical loss than degenerately doped N++ wafers.
  • <111> lattice for hexagonal epitaxy: The <111> (± 0.5°) orientation offers three-fold surface symmetry and slower wet alkaline etch kinetics, supporting lattice-matched GaN/AlN/SiC heteroepitaxy and UHV surface reconstruction studies.

Trade-offs

  • Native oxide requires removal: Bare prime silicon forms a ~1–2 nm ambient native SiO2 film in air; wet-chemical removal or RCA clean must be performed in an exhaust fume hood or wet bench under institutional EHS protocols before metallization or epitaxy.
  • Thin wafer handling risk: At 275 ± 25 µm thickness, the wafer is fragile and must be handled strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid breakage and surface contamination.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

25 pcs

Diameter

2-Inch (50.8 ± 0.2 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

N-Type / Phosphorus (P)

Orientation

± 0.5°

Resistivity

0.01-0.1 Ω·cm

Thickness

275 ± 25 μm

Surface Finish

Single-Side Polished (SSP, Ra < 0.5 nm)