| Diameter & Flat: 4-Inch (100.0 ± 0.3 mm) Primary Flat 32.5 mm <110> |
Substrate & Dopant: CZ P-Type / Boron (B) <111>•10–20 Ω·cm |
Thickness: 525 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: DSP (Ra < 0.5 nm) Dual-Side Mirror-Polished (CMP) |
1. Scientific Overview & Substrate Electrical Properties
4-Inch (100 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 10–20 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 100.0 ± 0.3 mm diameter and 525 ± 25 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).
Boron-doped to 10–20 Ω·cm (~1015 cm-3 dopant density), this moderate-resistivity substrate minimizes impurity scattering and junction capacitance compared with heavily doped wafers, supporting MOS C-V gate characterization, minority-carrier diffusion studies, and photodiode test structures.
Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D.
4-Inch (100 mm) Thickness & Process Compatibility Note: The industry-standard 525 ± 25 μm mechanical thickness offers high flexural rigidity across full-wafer photolithography steppers, PECVD/LPCVD cassettes, tube oxidation boats, and automated handling chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.
|
SEMI M1 4-Inch Dimensional PrecisionStandardized 100.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | P-Type / Boron (B) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 10–20 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <111> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 100.0 ± 0.3 mm (4-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 525 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Orientation Flat | Location: <110> ± 1°•Length: 32.5 ± 2.5 mm | SEMI M1 (100 mm) |
| Secondary Flat | None (SEMI M1 standard for 100 mm P-type <111>) | SEMI M1 (100 mm P<111>) |
| Surface Polish & Roughness | Double-Side Polished (DSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Total Thickness Variation (TTV) & Bow/Warp | TTV < 3 μm•Bow / Warp < 25 μm | Non-Contact Optical Flatness |
| Surface Particle Inspection | ≤ 10 particles / wafer (Cleanroom Audit) | Bright-Light & Laser Surface Scan |
| Available Pack Sizes | 10 pcs, 25 pcs cleanroom protective cassettes | Cleanroom Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm) supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding;
- Hexagonal Epitaxy & UHV Surface Physics: Dense three-fold <111> crystal lattice supports lattice-matched GaN/AlN/SiC heteroepitaxy, graphene/TMDC template growth, and discrete bipolar/power prototyping;
- Semiconductor Device & Electrode Prototyping: Controlled Boron-doped (10–20 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
- In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 4-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters, thicknesses, and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 4-Inch (100 mm), P-Type (111), 10-20 ohm-cm, 525 um, DSP (This Product) | 4-Inch (100 mm) / DSP | 525 ± 25 μm, P-Type (10–20 Ω·cm) | SEMI M1 525 μm 100 mm wafer in 10 pcs / 25 pcs cassettes |
| 4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, P-Type <100> | Standard SEMI M1 525 μm 100 mm lithography substrate |
| 4-Inch P-Type <100> Wafer (1–10 Ω·cm, 500 μm SSP) | 4-Inch (100 mm) / SSP | 500 ± 15 μm, P-Type <100> | 500 ± 15 μm precision thickness for MEMS & DRIE etching |
| 4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm DSP) | 4-Inch (100 mm) / DSP | 525 ± 25 μm, P-Type <100> | Double-side CMP polished for IR optics & fusion bonding |
| 4-Inch P-Type <111> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, P-Type <111> | Hexagonal <111> lattice for III-nitride epitaxy & UHV growth |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 4-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade virgin silicon wafers require cleanroom-compatible storage and edge-only handling to preserve sub-nanometer CMP surface quality. Bare silicon surfaces form a native oxide in ambient air and are sensitive to particulate, organic, and metallic contamination.
- Atmospheric Storage: Store sealed wafers inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.
- Native Oxide Formation: Bare prime silicon develops an ambient native SiO2 film of approximately 1–2 nm in air, which must be removed prior to metallization or epitaxy when an oxide-free interface is required.
- Edge-Only Contact: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid scratching the mirror-polished CMP surfaces.
- Cassette Containment: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box to minimize airborne organic contamination.
- Wet-Chemistry Containment: Perform all wet-chemical processing such as RCA cleans or native oxide removal strictly inside an exhaust fume hood or wet bench under facility-approved EHS and SDS protocols.
Preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs. Follow sequential solvent cleaning, plasma descum, and controlled storage to maintain surface integrity.
Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Cleanroom polypropylene cassette, Dry nitrogen cabinet or cleanroom desiccator, Exhaust fume hood or wet bench
- Inspect cassette and wafer edges
Inspect the cleanroom cassette and wafer perimeter for particulate or edge damage before removing any substrate. - Transfer wafer by edge only
Transfer the wafer using a cleanroom vacuum wand or PTFE/PEEK tweezers contacting only the perimeter edge. - Degrease in solvent sequence
Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and DI water. - Dry and descum
Blow-dry the wafer with N2 and apply a mild O2 plasma descum prior to photoresist spin coating or PVD/ALD deposition. - Remove native oxide under containment
Perform native oxide removal or RCA standard clean inside an exhaust fume hood or wet bench using facility-approved protocols when an oxide-free interface is required. - Return unused wafers to storage
Return unused wafers to the original cleanroom polypropylene cassette box and store inside a dry nitrogen cabinet.
Why choose a <111> orientation P-type silicon wafer over <100> for epitaxy or device prototyping?
The <111> orientation provides a densely packed crystal plane with hexagonal three-fold surface symmetry, a higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon. These properties make it preferable for III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D. In contrast, <100> wafers are typically chosen for standard lithography and MEMS DRIE processes where faster etch rates and different surface chemistry are advantageous.
What resistivity range does this 4-inch P-type <111> silicon wafer have and how does it affect device performance?
This wafer is Boron-doped to a verified resistivity of 10–20 Ω·cm, corresponding to a dopant density of approximately 10^15 cm^-3. This moderate resistivity minimizes impurity scattering and junction capacitance compared with heavily doped wafers, making it suitable for MOS C-V gate characterization, minority-carrier diffusion studies, and photodiode test structures. The resistivity is measured by four-point probe (4PP) and documented on the Certificate of Analysis.
How should 4-inch prime silicon wafers be stored and handled to maintain surface quality?
Store wafers sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid contaminating the dual-side mirror-polished surfaces (Ra < 0.5 nm). The wafers are supplied in cleanroom protective cassettes (10 pcs or 25 pcs options) that immobilize edges and prevent surface contact during transit.
The 4-inch prime CZ P-type <111> silicon wafer with 10–20 Ω·cm resistivity and dual-side CMP finish (Ra < 0.5 nm) is a well-characterized substrate for hexagonal epitaxy, double-side lithography, and UHV surface studies. Its SEMI M1 geometry and 525 μm thickness ensure compatibility with standard cleanroom handling, though the <111> orientation and moderate resistivity impose specific process constraints.
Positive
- Dual-side CMP for bonding and IR: Double-side mirror polish (Ra < 0.5 nm) enables direct fusion/anodic bonding and through-wafer infrared transmission without additional surface preparation.
- <111> lattice for hexagonal epitaxy: The densely packed <111> plane provides three-fold surface symmetry and slower alkaline etch kinetics, supporting lattice-matched GaN/AlN/SiC growth and UHV reconstruction studies.
Trade-offs
- Native oxide requires removal: Bare prime silicon forms a 1–2 nm ambient native SiO2 layer; wet-chemical removal or RCA clean must be performed in an exhaust fume hood or wet bench following institutional EHS protocols.
- <111> orientation limits standard processes: The <111> crystal orientation is not compatible with standard <100>-optimized processes such as KOH anisotropic etching or certain gate oxide growth recipes, requiring process redevelopment.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).