2-Inch N-Type Silicon Wafer 100-1000 Ω·cm ATOMFAIR®

$299.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Prime CZ N-Type silicon wafer, 50.8 mm, 275 μm, 100–1000 Ω·cm, SSP Ra < 0.5 nm. SEMI M1 flats, 25 pcs cassette. In stock.

Diameter & Flat:
2-Inch (50.8 ± 0.2 mm)
Primary Flat 15.88 mm <110>
Substrate & Dopant:
CZ N-Type / Phosphorus (P)
<111>•100–1000 Ω·cm
Thickness:
275 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
SSP (Ra < 0.5 nm)
Polished Front / Fine-Ground Back

1. Scientific Overview & Substrate Electrical Properties

2-Inch (50.8 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Phosphorus-doped to a verified resistivity of 100–1000 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 50.8 ± 0.2 mm diameter and 275 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.

Lightly Phosphorus-doped to 100–1000 Ω·cm, this high-resistivity n-type CZ substrate suppresses conductive substrate coupling and parasitic RF loss, serving RF/microwave planar circuits, IR/THz transmission windows, radiation/particle detector prototyping, and low-noise MEMS sensors.

Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D.

2-Inch Chamber Compatibility & Surface State Note: The compact 2-inch (50.8 mm) footprint fits research-scale tube furnaces, compact ALD/PECVD chambers, R&D spin coaters, and 2-inch sputtering sample holders without dicing waste. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Single-Side Polished (SSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)
SEMI M1 2-Inch Dimensional Precision

Standardized 50.8 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.

  • Diameter: 50.8 ± 0.2 mm (2.0 Inch)
  • Primary Flat: 15.88 ± 1.65 mm along <110> ± 1°
  • Secondary Flat: Located 45° ± 5° clockwise from primary flat (SEMI M1 50.8 mm N<111>)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant N-Type / Phosphorus (P) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 100–1000 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <111> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 50.8 ± 0.2 mm (2-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 275 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 15.88 ± 1.65 mm SEMI M1 (50.8 mm)
Secondary Flat Located 45° ± 5° clockwise from primary flat (SEMI M1 50.8 mm N<111>) SEMI M1 (50.8 mm N<111>)
Surface Polish & Roughness Single-Side Polished (SSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Pack Size (MOQ) 25 pcs (1 × 25-wafer cleanroom cassette, 25BX) Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications
  • Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for PVD sputtering, ALD, e-beam evaporation, and high-resolution photoresist spin coating;
  • Hexagonal Epitaxy & UHV Surface Physics: Dense three-fold <111> crystal lattice supports lattice-matched GaN/AlN/SiC heteroepitaxy, graphene/TMDC template growth, and discrete bipolar/power prototyping;
  • Semiconductor Device & Electrode Prototyping: Controlled Phosphorus-doped (100–1000 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol

Wafers are supplied in a standard 25-wafer protective cleanroom cassette (25 pcs pack, 25BX) engineered to immobilize 2-inch wafer edges and prevent surface contact during transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 2-Inch (50.8 mm), N-Type (111), 100-1000 ohm-cm, 275 um, SSP (This Product) 2-Inch (50.8 mm) / SSP 275 ± 25 μm, N-Type (100–1000 Ω·cm) SEMI M1 275 μm thickness, 25 pcs cassette for 2-inch R&D chambers
2-Inch P-Type <100> Wafer (1–10 Ω·cm SSP) 2-Inch (50.8 mm) / SSP 275 ± 25 μm, P-Type <100> Standard 50.8 mm P<100> bare lithography substrate
2-Inch P-Type <100> Wafer (1–10 Ω·cm DSP) 2-Inch (50.8 mm) / DSP 275 ± 25 μm, P-Type <100> Double-side CMP polished for IR optics & bonding
2-Inch N-Type <100> Wafer (1–10 Ω·cm SSP) 2-Inch (50.8 mm) / SSP 275 ± 25 μm, N-Type <100> Phosphorus-doped N<100> wafer for Schottky & diode R&D
2-Inch P-Type <111> Wafer (1–10 Ω·cm SSP) 2-Inch (50.8 mm) / SSP 275 ± 25 μm, P-Type <111> Hexagonal <111> lattice for III-nitride & UHV growth

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 2-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original 25-wafer polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Prime-grade virgin silicon wafers require particulate-controlled storage and edge-only handling to preserve the CMP mirror finish. Ambient native oxide growth and surface contamination must be managed before critical thin-film or epitaxy processes.

  • Cleanroom Storage Atmosphere: Store wafers sealed in the original 25-wafer polypropylene cassette inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.
  • Edge-Only Handling: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid contacting the polished front surface.
  • Native Oxide Control: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, which must be removed by RCA clean or wet processing before metallization or epitaxy if an oxide-free interface is required.
  • Wet-Chemical Safety Compliance: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols.

Preserve the CMP mirror finish and ensure reproducible thin-film interfaces by following sequential cleaning, drying, and storage steps. Each step must be performed in a controlled cleanroom environment with appropriate EHS oversight.

Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Exhaust fume hood or wet bench, Dry nitrogen cabinet or cleanroom desiccator

  1. Inspect Cassette and Wafer Edges
    Inspect the sealed 25-wafer cassette for integrity and verify that wafer edges are immobilized without surface contact before opening.
  2. Transfer Wafer by Edge
    Transfer the wafer using a cleanroom vacuum wand or PTFE/PEEK tweezers, gripping only the perimeter edge.
  3. Degrease in Solvent Sequence
    Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and DI water inside an exhaust fume hood or wet bench.
  4. Dry with Nitrogen
    Dry the wafer with a nitrogen blow-dry immediately after the final DI water rinse.
  5. Perform Optional Plasma Descum
    Apply a mild O2 plasma descum prior to photoresist spin coating or PVD/ALD if organic contamination is a concern.
  6. Remove Native Oxide if Required
    Perform RCA standard clean or wet processing inside an exhaust fume hood or wet bench when native oxide removal is required before metallization or epitaxy.
  7. Store Unused Wafers Sealed
    Return unused wafers to the original polypropylene cassette box and store sealed inside a dry nitrogen cabinet to minimize airborne organic contamination.

Why choose a high-resistivity 100–1000 Ω·cm N-type <111> silicon wafer instead of a standard 1–10 Ω·cm substrate?

The 100–1000 Ω·cm Phosphorus-doped bulk suppresses conductive substrate coupling and parasitic RF loss, which is why this wafer is specified for RF/microwave planar circuits, IR/THz transmission windows, radiation/particle detector prototyping, and low-noise MEMS sensors. Standard 1–10 Ω·cm wafers are optimized for conventional device fabrication but introduce higher substrate loss and coupling at high frequency. The trade-off is that the lightly doped high-resistivity bulk requires careful handling to avoid contamination that would shift the verified resistivity range.

Can this 2-inch N-type <111> wafer be used for GaN or AlN epitaxy, and how does the <111> orientation affect growth?

Yes. The <111> (± 0.5°) orientation presents a densely packed hexagonal three-fold surface symmetry that supports lattice-matched III-nitride/hexagonal epitaxy including GaN, AlN, and SiC, as well as graphene/TMDC template growth and UHV surface reconstruction studies. The <111> plane also exhibits higher in-plane elastic modulus along key cleavage directions and slower wet alkaline etch kinetics than <100> silicon. The mirror-polished SSP front surface (Ra < 0.5 nm) provides uniform nucleation for PVD, ALD, and e-beam evaporation.

What handling and storage requirements apply to this bare prime 2-inch silicon wafer to preserve its CMP surface?

Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers, and store unused wafers sealed inside the original 25-wafer polypropylene cassette within a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. The bare prime surface carries only a thin ambient native oxide (~1–2 nm), so any wet-chemical native oxide removal or RCA clean must be performed in an exhaust fume hood or wet bench following institutional EHS and SDS protocols. Solvent pre-cleaning should proceed sequentially in acetone, electronic-grade IPA, and DI water, followed by N2 blow-drying and mild O2 plasma descum before photoresist spin coating or PVD/ALD.

This 2-inch prime-grade CZ N-type <111> silicon wafer combines a high 100–1000 Ω·cm resistivity with sub-nanometer CMP surface finish, making it well-suited for RF/microwave planar circuits, III-nitride heteroepitaxy, and low-noise MEMS prototyping. Its 275 μm SEMI M1 geometry and 25-wafer cassette packaging support research-scale chambers, though users must account for native oxide growth and strict cleanroom handling.

Positive

  • High-Resistivity N-Type Substrate: Phosphorus-doped to 100–1000 Ω·cm, this high-resistivity n-type CZ silicon suppresses conductive substrate coupling and parasitic RF loss, supporting RF/microwave planar circuits, IR/THz transmission windows, and low-noise MEMS sensors.
  • <111> Lattice for Hexagonal Epitaxy: The densely packed <111> (± 0.5°) crystal plane provides hexagonal three-fold surface symmetry and slower wet alkaline etch kinetics than <100> silicon, enabling lattice-matched GaN/AlN/SiC heteroepitaxy and UHV surface reconstruction studies.

Trade-offs

  • Native Oxide Requires Removal: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air; where native oxide removal or RCA standard clean is required before metallization or epitaxy, wet processing must be performed strictly inside an exhaust fume hood or wet bench using facility-approved protocols.
  • Strict Cleanroom Handling Required: Wafers must be stored sealed in a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors, and handled strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to preserve the mirror-polished CMP surface.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

25 pcs

Diameter

2-Inch (50.8 ± 0.2 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

N-Type / Phosphorus (P)

Orientation

± 0.5°

Resistivity

100-1000 Ω·cm

Thickness

275 ± 25 μm

Surface Finish

Single-Side Polished (SSP, Ra < 0.5 nm)