| Diameter & Flat: 4-Inch (100.0 ± 0.3 mm) Primary Flat 32.5 mm <110> |
Substrate & Dopant: CZ P-Type / Boron (B) <100>•1–10 Ω·cm |
Thickness: 500 ± 15 μm Prime-Grade Virgin Wafer |
Surface Polish: SSP (Ra < 0.5 nm) Polished Front / Fine-Ground Back |
1. Scientific Overview & Substrate Electrical Properties
4-Inch (100 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 1–10 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 100.0 ± 0.3 mm diameter and 500 ± 15 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.
Doped with Boron to an industry-standard 1–10 Ω·cm semiconducting resistivity range, the wafer provides a well-characterized majority-hole carrier profile for MOSFET/CMOS device prototyping, Schottky barrier testing, PECVD/ALD dielectric C-V metrology, and general thin-film deposition.
Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.
4-Inch (100 mm) Thickness & Process Compatibility Note: The 500 ± 15 μm tight-tolerance thickness suits precision MEMS micromachining, double-side alignment lithography, DRIE through-etching, and reproducible capacitive cavity fabrication. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.
|
SEMI M1 4-Inch Dimensional PrecisionStandardized 100.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | P-Type / Boron (B) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 1–10 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <100> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 100.0 ± 0.3 mm (4-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 500 ± 15 μm | SEMI M1 / Capacitance Gauge |
| Primary Orientation Flat | Location: <110> ± 1°•Length: 32.5 ± 2.5 mm | SEMI M1 (100 mm) |
| Secondary Flat | 18.0 ± 2.0 mm secondary flat located 90° ± 5° clockwise from primary flat (SEMI M1 100 mm P<100>) | SEMI M1 (100 mm P<100>) |
| Surface Polish & Roughness | Single-Side Polished (SSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Total Thickness Variation (TTV) & Bow/Warp | TTV < 5 μm•Bow / Warp < 30 μm | Non-Contact Optical Flatness |
| Surface Particle Inspection | ≤ 10 particles / wafer (Cleanroom Audit) | Bright-Light & Laser Surface Scan |
| Available Pack Sizes | 10 pcs, 25 pcs cleanroom protective cassettes | Cleanroom Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for PVD sputtering, ALD, e-beam evaporation, and high-resolution photoresist spin coating;
- MEMS & Anisotropic Silicon Micromachining: Cleanroom <100> crystal plane supports KOH / TMAH wet anisotropic etching and Bosch deep reactive ion etching (DRIE);
- Semiconductor Device & Electrode Prototyping: Controlled Boron-doped (1–10 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
- In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 4-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters, thicknesses, and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 4-Inch (100 mm), P-Type (100), 1-10 ohm-cm, 500 um, SSP (This Product) | 4-Inch (100 mm) / SSP | 500 ± 15 μm, P-Type (1–10 Ω·cm) | SEMI M1 500 μm 100 mm wafer in 10 pcs / 25 pcs cassettes |
| 4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, P-Type <100> | Standard SEMI M1 525 μm 100 mm lithography substrate |
| 4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm DSP) | 4-Inch (100 mm) / DSP | 525 ± 25 μm, P-Type <100> | Double-side CMP polished for IR optics & fusion bonding |
| 4-Inch P-Type <111> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, P-Type <111> | Hexagonal <111> lattice for III-nitride epitaxy & UHV growth |
| 3-Inch P-Type <100> Wafer (1–10 Ω·cm, 380 μm SSP) | 3-Inch (76.2 mm) / SSP | 380 ± 25 μm, P-Type <100> | Intermediate 76.2 mm wafer for compact research chambers |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 4-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Bare prime silicon wafers carry a thin ambient native oxide and are sensitive to particulate, organic, and metallic contamination. Storage and handling must preserve the CMP-polished surface and prevent crystal damage or surface contamination.
- Native Oxide Formation: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, requiring controlled removal before metallization or epitaxy.
- Particulate and Organic Contamination Control: Unused wafers must remain sealed in the original cleanroom polypropylene cassette within a dry nitrogen cabinet to minimize airborne organic contamination.
- Edge-Only Handling Requirement: Wafers must be handled strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface contact.
- Corrosive Vapor and Dust Exposure: Storage away from particulate dust and corrosive vapors is required to prevent surface degradation and contamination.
- Wet-Chemical Processing Safety: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols.
Proper handling preserves the mirror-polished CMP surface and prevents contamination during thin-film deposition, lithography, or wet processing. Sequential solvent cleaning and controlled storage maintain reproducible interface quality.
Required Equipment: Cleanroom vacuum wand, PTFE/PEEK tweezers, Cleanroom polypropylene cassette, Dry nitrogen cabinet
- Inspect wafer cassette
Inspect the cleanroom protective cassette for edge immobilization and absence of surface contact before opening. - Handle by perimeter edge
Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers. - Degrease sequentially
Degrease diced dies or whole wafers sequentially in acetone, electronic-grade isopropanol, and DI water. - Blow-dry with nitrogen
Blow-dry the wafer surface with filtered N2 to remove residual solvent and moisture. - Perform plasma descum
Apply mild O2 plasma descum prior to photoresist spin coating or PVD/ALD deposition. - Remove native oxide if required
Perform wet processing for native oxide removal or RCA standard clean strictly inside an exhaust fume hood or wet bench using facility-approved protocols. - Store unused wafers sealed
Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet.
What is the difference between this 500 µm 4-inch silicon wafer and the standard 525 µm version?
This wafer is specified at 500 ± 15 µm thickness, whereas the standard SEMI M1 4-inch wafer is 525 ± 25 µm. The tighter 500 µm tolerance supports precision MEMS micromachining, double-side alignment lithography, DRIE through-etching, and reproducible capacitive cavity fabrication. Both wafers share the same P-type <100> orientation, 1–10 Ω·cm resistivity, and SSP finish with Ra < 0.5 nm.
Can this P-type <100> silicon wafer be used for KOH anisotropic wet etching and DRIE?
Yes. The <100> (± 0.5°) crystal orientation provides four-fold rotational symmetry with clean perpendicular cleaving along <110> planes and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions. The 500 ± 15 µm thickness and TTV < 5 µm / Bow-Warp < 30 µm support Bosch deep reactive ion etching (DRIE) for through-wafer features. The SSP front surface (Ra < 0.5 nm) ensures uniform mask adhesion for lithographic patterning.
How should these prime-grade silicon wafers be stored and handled to preserve surface quality?
Store wafers sealed inside the original cleanroom polypropylene cassette within a dry nitrogen cabinet or cleanroom desiccator, away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid contacting the Ra < 0.5 nm polished front surface. Bare prime silicon carries only a ~1–2 nm ambient native oxide; perform any wet-chemical cleaning or RCA standard clean strictly inside an exhaust fume hood or wet bench following institutional EHS and SDS protocols.
The 4-inch prime CZ P-type <100> silicon wafer with 500 µm thickness and SSP finish offers a well-characterized substrate for MEMS, thin-film, and device prototyping, but its bare surface and tight flatness tolerances demand strict cleanroom handling and native-oxide control.
Positive
- Sub-nanometer CMP surface: Ra < 0.5 nm on the polished front enables uniform nucleation for ALD, PVD, and high-resolution photoresist spin coating.
- Tight thickness and flatness: 500 ± 15 µm thickness with TTV < 5 µm and bow/warp < 30 µm supports double-side alignment lithography and reproducible capacitive cavity fabrication.
Trade-offs
- Native oxide requires removal: Bare prime silicon forms a 1–2 nm ambient SiO2 layer, necessitating RCA clean or wet etching before metallization or epitaxy.
- Cleanroom handling mandatory: Wafers must be stored in dry nitrogen cabinets and handled only by edge with vacuum wands or PTFE tweezers to prevent particulate contamination.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).