| Diameter & Flat: 4-Inch (100.0 ± 0.3 mm) Primary Flat 32.5 mm <110> |
Substrate & Dopant: CZ N-Type / Antimony (Sb) <100>•0.005–0.02 Ω·cm |
Thickness: 525 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: SSP (Ra < 0.5 nm) Polished Front / Fine-Ground Back |
1. Scientific Overview & Substrate Electrical Properties
4-Inch (100 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Antimony-doped to a verified resistivity of 0.005–0.02 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 100.0 ± 0.3 mm diameter and 525 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.
Heavily Antimony (Sb)-doped to 0.005–0.02 Ω·cm (N+) (~1.5×1018–1.2×1019 cm-3 donor concentration), Antimony exhibits very low solid-state diffusivity and exceptionally low vapor-phase out-diffusion (“autodoping”) during elevated-temperature LPCVD and epitaxial processes. It serves as an industry-standard low-resistance base for abrupt silicon epitaxy, trench power MOSFETs, discrete Schottky barriers, and buried-layer R&D.
Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.
4-Inch (100 mm) Thickness & Process Compatibility Note: The industry-standard 525 ± 25 μm mechanical thickness offers high flexural rigidity across full-wafer photolithography steppers, PECVD/LPCVD cassettes, epitaxial susceptors, and automated handling chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.
|
SEMI M1 4-Inch Dimensional PrecisionStandardized 100.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | N-Type / Antimony (Sb) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 0.005–0.02 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <100> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 100.0 ± 0.3 mm (4-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 525 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Orientation Flat | Location: <110> ± 1°•Length: 32.5 ± 2.5 mm | SEMI M1 (100 mm) |
| Secondary Flat | 18.0 ± 2.0 mm secondary flat located 180° ± 5° from primary flat (SEMI M1 100 mm N<100>) | SEMI M1 (100 mm N<100>) |
| Surface Polish & Roughness | Single-Side Polished (SSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Total Thickness Variation (TTV) & Bow/Warp | TTV < 5 μm•Bow / Warp < 30 μm | Non-Contact Optical Flatness |
| Surface Particle Inspection | ≤ 10 particles / wafer (Cleanroom Audit) | Bright-Light & Laser Surface Scan |
| Available Pack Sizes | 10 pcs, 25 pcs cleanroom protective cassettes | Cleanroom Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- Thin-Film Deposition & Epitaxial Growth: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures clean, defect-free nucleation for Si/SiGe/III-V epitaxy, ALD, PVD sputtering, and high-resolution photolithography;
- Power Devices, Epitaxy & Anisotropic MEMS: Standard <100> crystal plane supports abrupt epitaxial layer growth, vertical discrete power diodes/MOSFETs, and KOH/DRIE micromachining;
- Semiconductor Device & Epitaxial Prototyping: Controlled Antimony-doped (0.005–0.02 Ω·cm) base for ohmic contacts, power/RF devices, epitaxial growth, and C-V metrology;
- In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 4-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters, dopants, and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 4-Inch (100 mm), N-Type Antimony (100), 0.005-0.02 ohm-cm, 525 um, SSP (This Product) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, N-Type Antimony (0.005–0.02 Ω·cm) | SEMI M1 525 μm 100 mm wafer in 10 pcs / 25 pcs cassettes |
| 4-Inch N-Type Arsenic <100> Wafer (0.001–0.005 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, N++ As <100> | Low-strain, low-diffusivity As-doped epi & MOSFET substrate |
| 4-Inch N-Type <110> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, N-Type <110> | Vertical-sidewall KOH MEMS & <110> lattice transport wafer |
| 4-Inch N-Type <111> High-Res Wafer (100–1000 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, High-Res N <111> | High-resistivity hexagonal <111> wafer for RF & III-nitride epi |
| 4-Inch N-Type <100> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, N-Type <100> | Standard SEMI M1 525 μm 100 mm N-type lithography substrate |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 4-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade virgin monocrystalline silicon substrates require cleanroom-compatible storage and edge-only manipulation to preserve CMP surface quality. Environmental exposure to particulate contamination, corrosive vapors, and ambient moisture must be minimized prior to downstream processing.
- Cleanroom Cassette Storage: Store unused wafers sealed inside the original cleanroom polypropylene cassette within a dry nitrogen cabinet or desiccator to limit airborne organic contamination.
- Edge-Only Manipulation: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid contacting the polished front surface.
- Native Oxide Awareness: Bare prime silicon forms an ambient native silicon dioxide film of approximately 1 to 2 nm in air, which must be removed by wet processing before metallization or epitaxy where an ohmic interface is required.
- Wet-Chemical Processing Controls: Perform solvent cleaning, RCA standard clean, or native oxide removal strictly inside an exhaust fume hood or wet bench using facility-approved protocols and institutional EHS and SDS safety procedures.
- Corrosive Vapor Exclusion: Keep wafers away from particulate dust and corrosive vapors during storage to prevent surface degradation of the CMP finish.
Preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs. Follow sequential solvent cleaning, plasma descum, and controlled storage to maintain prime-grade surface quality.
Required Equipment: Cleanroom vacuum wand, PTFE or PEEK tweezers, Cleanroom polypropylene cassette, Dry nitrogen cabinet or cleanroom desiccator
- Inspect Cassette and Wafer Edges
Inspect the cleanroom cassette and wafer edges for particulate contamination or physical damage before removing any substrate. - Transfer by Perimeter Edge
Transfer the wafer using a cleanroom vacuum wand or PTFE/PEEK tweezers applied only to the perimeter edge. - Degrease in Solvent Sequence
Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and deionized water. - Dry and Plasma Descum
Dry the wafer with nitrogen blow-drying followed by a mild oxygen plasma descum prior to photoresist spin coating or PVD/ALD deposition. - Remove Native Oxide Where Required
Perform native oxide removal or RCA standard clean inside an exhaust fume hood or wet bench using facility-approved protocols when an ohmic interface is required before metallization or epitaxy. - Return Unused Wafers to Sealed Storage
Return unused wafers to the original cleanroom polypropylene cassette box and store within a dry nitrogen cabinet to minimize airborne organic contamination.
Why choose antimony-doped silicon wafers over arsenic or phosphorus for epitaxial power device fabrication?
Antimony (Sb) doping is selected for its exceptionally low solid-state diffusivity and minimal vapor-phase out-diffusion (autodoping) during high-temperature LPCVD and epitaxial processes, which preserves abrupt doping profiles at the substrate-epi interface. This 4-inch wafer is doped to 0.005–0.02 Ω·cm (N+), corresponding to roughly 1.5×10^18–1.2×10^19 cm^-3 donor concentration, making it an industry-standard low-resistance base for trench power MOSFETs, discrete Schottky barriers, and buried-layer R&D. Compared to arsenic or phosphorus, antimony's low diffusivity reduces dopant migration into the growing epitaxial layer, enabling sharper junctions and more predictable device characteristics.
Can this 4-inch N-type antimony wafer be used for KOH anisotropic wet etching and MEMS micromachining?
Yes. The <100> (± 0.5°) crystal orientation supports predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions, with clean perpendicular cleaving along <110> planes. The cubic surface exhibits four-fold rotational symmetry and low Si/SiO2 interface state density, which are advantageous for MEMS and vertical device structures. The primary flat is oriented along <110> ± 1° per SEMI M1, ensuring accurate mask alignment for anisotropic etch processes.
What cleanroom handling and storage procedures are required to maintain the surface quality of these prime SSP wafers?
These wafers feature a single-side polished (SSP) front surface with Ra < 0.5 nm and ≤ 10 particles per wafer, so they must be handled strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface contact. Store unused wafers sealed inside the original cleanroom polypropylene cassette within a dry nitrogen cabinet or cleanroom desiccator, away from particulate dust and corrosive vapors. Bare prime silicon forms a ~1–2 nm native SiO2 film in air; if native oxide removal or RCA cleaning is required before metallization or epitaxy, perform wet processing in an exhaust fume hood or wet bench following institutional EHS and SDS protocols.
The 4-inch prime CZ silicon wafer with antimony doping (0.005–0.02 Ω·cm) and <100> orientation offers a low-diffusivity, low-autodoping substrate ideal for epitaxial and power device prototyping, while its 525 μm thickness and SEMI M1 flats ensure compatibility with standard cleanroom handling. However, its bare surface requires stringent cleanroom protocols to prevent contamination and native oxide growth.
Positive
- Low Autodoping Antimony Dopant: Antimony's low solid-state diffusivity and vapor-phase out-diffusion minimize autodoping during high-temperature LPCVD and epitaxial processes, enabling abrupt doping profiles for power devices and buried-layer R&D.
- SEMI M1 Dimensional Precision: Standardized 100.0 mm diameter and crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes, reducing handling errors in automated lithography.
Trade-offs
- Bare Surface Contamination Risk: The absence of a protective coating necessitates strict cleanroom handling and storage in dry nitrogen cabinets to prevent particulate and organic contamination, which can degrade thin-film nucleation.
- Native Oxide Formation: Ambient exposure forms a 1–2 nm native SiO2 layer that must be removed via wet etching or RCA clean before metallization or epitaxy, requiring exhaust fume hoods and facility-approved protocols.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).