Graphite Single-Sided Anode Sheet, 27.4 mg/cm2

$89.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

single-sided Graphite anode sheet for lithium-ion battery research. Key specifications: 27.4 mg/cm2 areal loading, 96.00% active material, 1.31 g/cm3 compaction density, Carbon-Coated Copper Foil. Suitable for lithium-ion half-cell testing, full-cell assembly, electrolyte studies, and anode-cathode balancing.

Brands:

Graphite Single-Sided Anode Sheet, 27.4 mg/cm2

Graphite is a layered carbon anode material for lithium-ion batteries. This ready-to-use sheet is supplied for laboratory cell assembly and material evaluation in the listed Single-Sided, 27.4 mg/cm2 configuration.

Material Characteristics

  • Layered carbon structure
  • Established lithium-ion negative-electrode material
  • Coated sheet for half-cell and full-cell research

Typical Research Uses

Use for lithium-ion half-cell testing, full-cell assembly, electrolyte studies, and anode-cathode balancing.

How to Read This Configuration

Use the listed areal loading and side basis when matching graphite with a lithium-ion cathode sheet.

  • Areal loading: 27.4 mg/cm2. Use this value as the coating-mass basis when comparing electrode configurations.
  • Active material ratio: 96.00% is the listed active-material fraction of the coating formulation. The actual active mass still depends on the punched electrode mass.
  • Compaction density: 1.31 g/cm3 is a physical electrode parameter. Interpret it with loading, thickness, porosity, and the source measurement method.
  • Current collector: Carbon-Coated Copper Foil, listed as 1 um C / 6 um Cu / 1 um C. This identifies the foil supporting the coating.
Product Specification Value / Description
Product Type Single-Sided Anode Sheet
Active Material System Graphite
Battery System Lithium-Ion
Electrode Role Anode
Coating Side Single-Sided
Areal Loading 27.4 mg/cm2
Current Collector Carbon-Coated Copper Foil
Current Collector Structure 1 um C / 6 um Cu / 1 um C
Active Material Ratio 96.00%
Compaction Density 1.31 g/cm3
SKU AF-BM-S-AGR0-CS274-5P0

Drying and Handling

Before cell assembly, dry the electrode sheet at 90-100 C for 12-24 hours. Use a clean, dry handling environment after drying.

Avoid bending, scratching, or contaminating the coated surface during cutting, punching, transfer, and stacking.

Research Need Related Atomfair Category Best For
Full-cell electrode pairing Lithium-Ion Cathode Electrode Sheets Selecting a matched lithium-ion cathode sheet for cell assembly
Material selection Lithium-Ion Anode Materials Comparing anode material options before custom electrode preparation
Custom configuration Custom Battery Electrode Coating Service Alternative loading, dimensions, current collector, or coating configuration
Tailored Solutions for Research
Contact our engineering team for technical support or institutional quotation requests.

Email: inquiry@atomfair.com

Manufacturer: Atomfair LLC
Brand: ATOMFAIR®

This document outlines handling and storage constraints for the graphite anode electrode sheet. It specifies moisture sensitivity, mechanical integrity requirements, and mass calculation procedures.

  • Moisture Sensitivity: The electrode coating is sensitive to moisture and must be handled and stored in a dry environment or inert atmosphere to prevent degradation.
  • Mechanical Integrity: The coated surface must not be touched, bent, scratched, or contaminated to avoid compromising electrode performance.
  • Mass Calculation Requirement: Active material mass must be calculated from coating loading, active material ratio, and punched electrode area for accurate cell balancing.

This procedure describes the steps for handling and preparing the graphite anode electrode sheet before cell assembly. It ensures proper moisture control, surface integrity, and mass calculation.

Required Equipment: Glovebox

  1. Transfer to dry environment
    Transfer the electrode sheet to a dry environment or inert atmosphere before opening the package.
  2. Inspect coated surface
    Inspect the coated surface for any visible defects such as scratches or contamination.
  3. Calculate active material mass
    Calculate the active material mass using the coating loading, active material ratio, and punched electrode area.

How does the compaction density of 1.31 g/cm3 affect the electrochemical performance of this graphite anode?

The compaction density of 1.31 g/cm3 indicates the electrode's porosity and electronic connectivity, directly influencing rate capability and cycle life. Combined with a coating loading of 27.4 mg/cm2 and 96.00% active material ratio, this electrode is designed for balanced ionic and electronic transport in half-cell or full-cell experiments. The dry process coating further affects the electrode's mechanical integrity and electrolyte wetting behavior.

How should I calculate the active material mass for cell balancing when using this single-sided graphite anode?

Multiply the coating loading (27.4 mg/cm2) by the punched electrode area (in cm2) to obtain total coating mass, then multiply by the active material ratio (0.96) to get active graphite mass. This calculation is essential for setting the N/P ratio when matching with a cathode, as noted in the product's handling and research use case guidance.

What storage conditions are required to prevent moisture degradation of this dry-process graphite anode sheet?

Store opened sheets in a dry environment or inert atmosphere (e.g., argon or nitrogen glovebox) to minimize moisture exposure before use. The dry process coating and carbon-coated copper foil current collector are sensitive to ambient humidity, which can degrade electrode performance. A dry handling environment is also recommended during punching and cell assembly.

The 27.4 mg/cm² graphite anode sheet with 96% active material ratio and dry-process coating on carbon-coated copper foil provides a consistent baseline for electrolyte screening and cathode matching, but requires careful dry handling and mechanical protection of the coated surface.

Positive

  • High active material ratio: 96.00% active material ratio provides a well-defined electrode composition for repeatable half-cell or full-cell experiments.
  • Dry process coating for baseline studies: Dry-process coating enables direct comparison with wet-process electrodes and supports process variable studies.

Trade-offs

  • Moisture-sensitive handling required: Dry handling environment and inert atmosphere storage are recommended to prevent moisture exposure on the coated electrode surface.
  • Fragile coated surface requires careful handling: The coated surface must not be touched, bent, scratched, or contaminated during punching, transfer, and stacking to avoid compromising electrode integrity.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).