4-Inch Prime CZ Silicon Wafer P-Type 525μm ATOMFAIR®

Price range: $169.00 through $339.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Prime CZ P-Type silicon wafer, 100mm, 525μm, 0.1–1.0 Ω·cm, SSP Ra<0.5nm. SEMI M1 flats, CoA included. In stock.

Diameter & Flat:
4-Inch (100.0 ± 0.3 mm)
Primary Flat 32.5 mm <110>
Substrate & Dopant:
CZ P-Type / Boron (B)
<100>•0.1–1.0 Ω·cm
Thickness:
525 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
SSP (Ra < 0.5 nm)
Polished Front / Fine-Ground Back

4-Inch (100 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 0.1–1.0 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 100.0 ± 0.3 mm diameter and 525 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.

Boron-doped to 0.1–1.0 Ω·cm (~2×1016–2×1017 cm-3 acceptor concentration), this moderately low-resistivity substrate bridges heavily doped electrode wafers and standard CMOS grades, supporting epitaxial growth templates, bipolar power structures, and low-resistance MOS back gates.

Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.

4-Inch (100 mm) Thickness & Process Compatibility Note: The industry-standard 525 ± 25 μm mechanical thickness offers high flexural rigidity across full-wafer photolithography steppers, PECVD/LPCVD cassettes, tube oxidation boats, and automated handling chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Single-Side Polished (SSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)

SEMI M1 4-Inch Dimensional Precision

Standardized 100.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.

  • Diameter: 100.0 ± 0.3 mm (4.0 Inch)
  • Primary Flat: 32.5 ± 2.5 mm along <110> ± 1°
  • Secondary Flat: 18.0 ± 2.0 mm secondary flat located 90° ± 5° clockwise from primary flat (SEMI M1 100 mm P<100>)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant P-Type / Boron (B) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 0.1–1.0 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <100> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 100.0 ± 0.3 mm (4-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 525 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 32.5 ± 2.5 mm SEMI M1 (100 mm)
Secondary Flat 18.0 ± 2.0 mm secondary flat located 90° ± 5° clockwise from primary flat (SEMI M1 100 mm P<100>) SEMI M1 (100 mm P<100>)
Surface Polish & Roughness Single-Side Polished (SSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Total Thickness Variation (TTV) & Bow/Warp TTV < 5 μm•Bow / Warp < 30 μm Non-Contact Optical Flatness
Surface Particle Inspection ≤ 10 particles / wafer (Cleanroom Audit) Bright-Light & Laser Surface Scan
Available Pack Sizes 10 pcs, 25 pcs cleanroom protective cassettes Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications

  • Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for PVD sputtering, ALD, e-beam evaporation, and high-resolution photoresist spin coating;
  • MEMS & Anisotropic Silicon Micromachining: Cleanroom <100> crystal plane supports KOH / TMAH wet anisotropic etching and Bosch deep reactive ion etching (DRIE);
  • Semiconductor Device & Electrode Prototyping: Controlled Boron-doped (0.1–1.0 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.

Packaging, Storage & Handling Protocol

Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 4-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters, thicknesses, and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 4-Inch (100 mm), P-Type (100), 0.1-1.0 ohm-cm, 525 um, SSP (This Product) 4-Inch (100 mm) / SSP 525 ± 25 μm, P-Type (0.1–1.0 Ω·cm) SEMI M1 525 μm 100 mm wafer in 10 pcs / 25 pcs cassettes
4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, P-Type <100> Standard SEMI M1 525 μm 100 mm lithography substrate
4-Inch P-Type <100> Wafer (1–10 Ω·cm, 500 μm SSP) 4-Inch (100 mm) / SSP 500 ± 15 μm, P-Type <100> 500 ± 15 μm precision thickness for MEMS & DRIE etching
4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm DSP) 4-Inch (100 mm) / DSP 525 ± 25 μm, P-Type <100> Double-side CMP polished for IR optics & fusion bonding
4-Inch P-Type <111> Wafer (1–10 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, P-Type <111> Hexagonal <111> lattice for III-nitride epitaxy & UHV growth

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 4-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Prime-grade monocrystalline silicon wafers require particulate-controlled storage and edge-only contact to preserve the CMP-polished surface. Ambient native oxide growth and contamination risks dictate sealed dry-nitrogen cabinet storage between processing steps.

  • Particulate and Organic Contamination Control: Store wafers sealed inside the original cleanroom polypropylene cassette within a dry nitrogen cabinet to minimize airborne organic contamination.
  • Edge-Only Contact Requirement: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface damage.
  • Native Oxide Formation: Bare prime silicon forms an ambient approximately 1–2 nm native SiO2 film in air, requiring controlled wet processing for removal before metallization or epitaxy.
  • Corrosive Vapor and Dust Exposure: Store wafers away from particulate dust and corrosive vapors to prevent surface degradation.

Proper handling and pre-cleaning procedures preserve the mirror-polished CMP surface and ensure reproducible thin-film interfaces. Sequential solvent cleaning followed by plasma descum removes organic contamination prior to deposition or lithography.

Required Equipment: Cleanroom vacuum wand, PTFE/PEEK tweezers, Cleanroom polypropylene cassette, Dry nitrogen cabinet

  1. Inspect wafer cassette
    Verify that the cleanroom protective cassette is sealed and free of visible particulate contamination before opening.
  2. Transfer wafer with edge-only contact
    Transfer the wafer using a cleanroom vacuum wand or PTFE/PEEK tweezers applied strictly to the perimeter edge.
  3. Degrease in solvent sequence
    Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and DI water.
  4. Dry with nitrogen
    Blow-dry the wafer with filtered nitrogen gas until all solvent residue is removed.
  5. Perform plasma descum
    Apply a mild oxygen plasma descum to remove residual organic contamination prior to photoresist spin coating or PVD/ALD.
  6. Store unused wafers
    Return unused wafers to the original cleanroom polypropylene cassette and store inside a dry nitrogen cabinet.

What is the resistivity range of this 4-inch P-type silicon wafer and how does it affect device fabrication?

This wafer is Boron-doped to a resistivity of 0.1–1.0 Ω·cm, corresponding to an acceptor concentration of approximately 2×10^16–2×10^17 cm^-3. This moderately low resistivity bridges heavily doped electrode wafers and standard CMOS grades, making it suitable for epitaxial growth templates, bipolar power structures, and low-resistance MOS back gates. The tight tolerance ensures predictable electrical behavior for ohmic contacts and Schottky diodes.

Can this 4-inch silicon wafer be used for KOH anisotropic etching and MEMS fabrication?

Yes, the <100> crystal orientation (± 0.5°) with a primary flat along <110> ± 1° is ideal for anisotropic wet etching in KOH or TMAH solutions, producing predictable V-groove geometries. The 525 ± 25 μm thickness provides sufficient mechanical rigidity for through-wafer etching and deep reactive ion etching (DRIE) processes. The fine-ground back surface and SSP front surface (Ra < 0.5 nm) support uniform masking and etch uniformity.

How should I store and handle these prime silicon wafers to maintain surface quality?

Store wafers sealed in the original cleanroom protective cassette inside a dry nitrogen cabinet or desiccator to prevent native oxide growth and particulate contamination. Handle only by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers; never touch the polished face. The wafers are shipped in cassettes of 10 or 25 pieces, and each lot includes a Certificate of Analysis verifying resistivity, thickness, orientation, and particle count (≤ 10 particles per wafer).

The 4-inch prime CZ P-type <100> silicon wafer at 0.1–1.0 Ω·cm and 525 μm SSP offers a moderately low-resistivity, SEMI M1-compliant substrate suited to epitaxial templates, MEMS anisotropic etching, and low-resistance MOS back gates. Its bare, single-side-polished surface with Ra < 0.5 nm supports direct in-house oxidation and thin-film growth, but requires cleanroom handling and dry storage to preserve surface integrity.

Positive

  • Moderate Boron Doping for Device Prototyping: Boron-doped to 0.1–1.0 Ω·cm (~2×10^16–2×10^17 cm^-3), this substrate bridges heavily doped electrode wafers and standard CMOS grades, supporting ohmic contacts, Schottky diodes, and low-resistance MOS back gates.
  • CMP Mirror Surface for Thin-Film Growth: Single-side polished front with Ra < 0.5 nm ensures uniform nucleation for PVD, ALD, e-beam evaporation, and high-resolution photoresist spin coating.

Trade-offs

  • Cleanroom Handling and Storage Required: Wafers must be handled strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers and stored sealed in a dry nitrogen cabinet or desiccator away from particulate dust and corrosive vapors.
  • Native Oxide Requires Wet Processing: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air; removal or RCA standard clean before metallization or epitaxy must be performed in an exhaust fume hood or wet bench following institutional EHS and SDS protocols.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

10 pcs, 25 pcs

Diameter

4-Inch (100.0 ± 0.3 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

P-Type / Boron (B)

Orientation

± 0.5°

Resistivity

0.1-1.0 Ω·cm

Thickness

525 ± 25 μm

Surface Finish

Single-Side Polished (SSP, Ra < 0.5 nm)