| Diameter & Flat: 4-Inch (100.0 ± 0.3 mm) Primary Flat 32.5 mm <110> |
Substrate & Dopant: CZ P-Type / Boron (B) <100>•0.1–1.0 Ω·cm |
Thickness: 525 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: DSP (Ra < 0.5 nm) Dual-Side Mirror-Polished (CMP) |
1. Scientific Overview & Substrate Electrical Properties
4-Inch (100 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 0.1–1.0 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 100.0 ± 0.3 mm diameter and 525 ± 25 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).
Boron-doped to 0.1–1.0 Ω·cm (~2×1016–2×1017 cm-3 acceptor concentration), this moderately low-resistivity substrate bridges heavily doped electrode wafers and standard CMOS grades, supporting epitaxial growth templates, bipolar power structures, and low-resistance MOS back gates.
Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.
4-Inch (100 mm) Thickness & Process Compatibility Note: The industry-standard 525 ± 25 μm mechanical thickness offers high flexural rigidity across full-wafer photolithography steppers, PECVD/LPCVD cassettes, tube oxidation boats, and automated handling chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.
|
SEMI M1 4-Inch Dimensional PrecisionStandardized 100.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | P-Type / Boron (B) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 0.1–1.0 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <100> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 100.0 ± 0.3 mm (4-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 525 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Orientation Flat | Location: <110> ± 1°•Length: 32.5 ± 2.5 mm | SEMI M1 (100 mm) |
| Secondary Flat | 18.0 ± 2.0 mm secondary flat located 90° ± 5° clockwise from primary flat (SEMI M1 100 mm P<100>) | SEMI M1 (100 mm P<100>) |
| Surface Polish & Roughness | Double-Side Polished (DSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Total Thickness Variation (TTV) & Bow/Warp | TTV < 3 μm•Bow / Warp < 25 μm | Non-Contact Optical Flatness |
| Surface Particle Inspection | ≤ 10 particles / wafer (Cleanroom Audit) | Bright-Light & Laser Surface Scan |
| Available Pack Sizes | 10 pcs, 25 pcs cleanroom protective cassettes | Cleanroom Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm) supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding;
- MEMS & Anisotropic Silicon Micromachining: Cleanroom <100> crystal plane supports KOH / TMAH wet anisotropic etching and Bosch deep reactive ion etching (DRIE);
- Semiconductor Device & Electrode Prototyping: Controlled Boron-doped (0.1–1.0 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
- In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 4-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters, thicknesses, and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 4-Inch (100 mm), P-Type (100), 0.1-1.0 ohm-cm, 525 um, DSP (This Product) | 4-Inch (100 mm) / DSP | 525 ± 25 μm, P-Type (0.1–1.0 Ω·cm) | SEMI M1 525 μm 100 mm wafer in 10 pcs / 25 pcs cassettes |
| 4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, P-Type <100> | Standard SEMI M1 525 μm 100 mm lithography substrate |
| 4-Inch P-Type <100> Wafer (1–10 Ω·cm, 500 μm SSP) | 4-Inch (100 mm) / SSP | 500 ± 15 μm, P-Type <100> | 500 ± 15 μm precision thickness for MEMS & DRIE etching |
| 4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm DSP) | 4-Inch (100 mm) / DSP | 525 ± 25 μm, P-Type <100> | Double-side CMP polished for IR optics & fusion bonding |
| 4-Inch P-Type <111> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, P-Type <111> | Hexagonal <111> lattice for III-nitride epitaxy & UHV growth |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 4-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade monocrystalline silicon wafers require cleanroom-compatible handling to preserve CMP surface quality and prevent particulate contamination. Storage must be maintained in a dry nitrogen cabinet or cleanroom desiccator to avoid native oxide growth and airborne organic contamination.
- Surface Contamination Control: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to prevent surface contact and particle transfer.
- Native Oxide Sensitivity: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, requiring wet processing inside an exhaust fume hood or wet bench when native oxide removal is necessary.
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
- Thermal Processing Compatibility: The 525 ± 25 μm thickness provides high flexural rigidity for full-wafer photolithography steppers, PECVD/LPCVD cassettes, tube oxidation boats, and automated handling chucks.
Proper handling and pre-cleaning procedures preserve the CMP mirror finish and ensure reproducible thin-film interfaces. Sequential solvent cleaning followed by plasma descum removes organic contaminants prior to photoresist spin coating or PVD/ALD deposition.
Required Equipment: Cleanroom vacuum wand, PTFE/PEEK tweezers, Exhaust fume hood or wet bench, Dry nitrogen cabinet
- Inspect wafer cassette
Verify that the cleanroom protective cassette is sealed and free from visible particulate contamination before opening. - Handle by perimeter edge
Transfer wafers using a cleanroom vacuum wand or PTFE/PEEK tweezers, contacting only the perimeter edge to avoid surface damage. - Degrease sequentially
Immerse wafers sequentially in acetone, electronic-grade isopropanol, and DI water to remove organic contaminants. - Dry with nitrogen
Blow-dry the wafer surface with filtered nitrogen gas until no visible liquid remains. - Perform plasma descum
Apply a mild oxygen plasma descum to remove residual organic layers prior to photoresist spin coating or PVD/ALD deposition. - Store in dry nitrogen cabinet
Return unused wafers to the original cleanroom polypropylene cassette and store inside a dry nitrogen cabinet or cleanroom desiccator.
What is the resistivity range and dopant type of this 4-inch prime silicon wafer?
This wafer is P-Type, Boron-doped with a verified electrical resistivity of 0.1–1.0 Ω·cm, corresponding to an acceptor concentration of approximately 2×10^16–2×10^17 cm^-3. The resistivity is measured by four-point probe (4PP) and documented on the lot-specific Certificate of Analysis. This moderately low-resistivity range bridges heavily doped electrode wafers and standard CMOS grades, making it suitable for epitaxial growth templates, bipolar power structures, and low-resistance MOS back gates.
Is this wafer compatible with double-side lithography and wafer bonding processes?
Yes. The wafer features a dual-side mirror-polished (DSP) CMP finish with Ra < 0.5 nm on both surfaces, which supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion or anodic bonding. The <100> crystal orientation with SEMI M1 flats ensures accurate registration on vacuum chucks and mask aligners. The 525 ± 25 μm thickness provides high flexural rigidity for handling in automated cassettes and tube oxidation boats.
How should these prime silicon wafers be stored and handled to maintain surface quality?
Wafers are supplied in cleanroom protective cassettes (10 pcs or 25 pcs options) that immobilize edges and prevent surface contact. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), so keep unused wafers in the original cassette to minimize airborne organic contamination.
This 4-inch prime CZ P-type <100> silicon wafer combines a moderately low 0.1–1.0 Ω·cm boron-doped bulk with dual-side CMP mirror polish (Ra < 0.5 nm) and SEMI M1 dimensional tolerances, making it a versatile substrate for double-side lithography, anisotropic KOH/TMAH micromachining, and in-house thermal oxidation. Its bare, virgin prime-grade surface demands strict cleanroom handling and dry nitrogen storage to preserve the sub-nanometer finish and native-oxide-controlled interfaces.
Positive
- Dual-Side CMP Mirror Finish: Double-side polished surfaces with Ra < 0.5 nm support double-sided MEMS patterning, through-wafer IR transmission, and direct fusion or anodic bonding without additional surface preparation.
- Moderate Boron-Doped Resistivity: The 0.1–1.0 Ω·cm P-type bulk (~2×10^16–2×10^17 cm^-3) bridges heavily doped electrode wafers and standard CMOS grades, enabling ohmic contacts, Schottky diodes, and low-resistance MOS back gates.
- <100> Plane Etch Predictability: The <100> ± 0.5° orientation provides four-fold symmetry, clean <110> cleaving, and predictable anisotropic V-groove formation in KOH/TMAH, with low Si/SiO2 interface state density.
- SEMI M1 Dimensional Consistency: 100.0 ± 0.3 mm diameter, 525 ± 25 μm thickness, TTV < 3 μm, and bow/warp < 25 μm ensure reliable registration on vacuum chucks, mask aligners, and automated handling cassettes.
Trade-offs
- Bare Surface Contamination Sensitivity: The uncoated prime silicon carries only a ~1–2 nm ambient native oxide and must be stored sealed in a dry nitrogen cabinet or desiccator; exposure to particulate dust or corrosive vapors degrades the CMP finish and interface reproducibility.
- Strict Cleanroom Handling Required: Wafers must be handled only by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers; wet-chemical processing requires an exhaust fume hood or wet bench under institutional EHS and SDS protocols.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).