4-Inch Prime CZ Silicon Wafer P-Type 525μm DSP ATOMFAIR®

Price range: $219.00 through $479.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Prime-grade 4-inch (100 mm) CZ P-Type/Boron silicon wafer, 0.01–0.1 Ω·cm, 525 ± 25 μm, DSP Ra < 0.5 nm. SEMI M1 flats. In stock.

Diameter & Flat:
4-Inch (100.0 ± 0.3 mm)
Primary Flat 32.5 mm <110>
Substrate & Dopant:
CZ P-Type / Boron (B)
<100>•0.01–0.1 Ω·cm
Thickness:
525 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
DSP (Ra < 0.5 nm)
Dual-Side Mirror-Polished (CMP)

4-Inch (100 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 0.01–0.1 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 100.0 ± 0.3 mm diameter and 525 ± 25 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).

Boron-doped to a low-resistivity range of 0.01–0.1 Ω·cm (P+), the wafer provides low bulk series resistance for vertical current conduction, anodic glass bonding, and electrochemical working electrodes while reducing free-carrier infrared absorption compared with degenerately doped P++ substrates.

Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.

4-Inch (100 mm) Thickness & Process Compatibility Note: The industry-standard 525 ± 25 μm mechanical thickness offers high flexural rigidity across full-wafer photolithography steppers, PECVD/LPCVD cassettes, tube oxidation boats, and automated handling chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Double-Side Polished (DSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)

SEMI M1 4-Inch Dimensional Precision

Standardized 100.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.

  • Diameter: 100.0 ± 0.3 mm (4.0 Inch)
  • Primary Flat: 32.5 ± 2.5 mm along <110> ± 1°
  • Secondary Flat: 18.0 ± 2.0 mm secondary flat located 90° ± 5° clockwise from primary flat (SEMI M1 100 mm P<100>)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant P-Type / Boron (B) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 0.01–0.1 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <100> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 100.0 ± 0.3 mm (4-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 525 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 32.5 ± 2.5 mm SEMI M1 (100 mm)
Secondary Flat 18.0 ± 2.0 mm secondary flat located 90° ± 5° clockwise from primary flat (SEMI M1 100 mm P<100>) SEMI M1 (100 mm P<100>)
Surface Polish & Roughness Double-Side Polished (DSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Total Thickness Variation (TTV) & Bow/Warp TTV < 3 μm•Bow / Warp < 25 μm Non-Contact Optical Flatness
Surface Particle Inspection ≤ 10 particles / wafer (Cleanroom Audit) Bright-Light & Laser Surface Scan
Available Pack Sizes 10 pcs, 25 pcs cleanroom protective cassettes Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications

  • Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm) supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding;
  • MEMS & Anisotropic Silicon Micromachining: Cleanroom <100> crystal plane supports KOH / TMAH wet anisotropic etching and Bosch deep reactive ion etching (DRIE);
  • Semiconductor Device & Electrode Prototyping: Controlled Boron-doped (0.01–0.1 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.

Packaging, Storage & Handling Protocol

Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 4-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters, thicknesses, and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 4-Inch (100 mm), P-Type (100), 0.01-0.1 ohm-cm, 525 um, DSP (This Product) 4-Inch (100 mm) / DSP 525 ± 25 μm, P-Type (0.01–0.1 Ω·cm) SEMI M1 525 μm 100 mm wafer in 10 pcs / 25 pcs cassettes
4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, P-Type <100> Standard SEMI M1 525 μm 100 mm lithography substrate
4-Inch P-Type <100> Wafer (1–10 Ω·cm, 500 μm SSP) 4-Inch (100 mm) / SSP 500 ± 15 μm, P-Type <100> 500 ± 15 μm precision thickness for MEMS & DRIE etching
4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm DSP) 4-Inch (100 mm) / DSP 525 ± 25 μm, P-Type <100> Double-side CMP polished for IR optics & fusion bonding
4-Inch P-Type <111> Wafer (1–10 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, P-Type <111> Hexagonal <111> lattice for III-nitride epitaxy & UHV growth

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 4-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Prime-grade monocrystalline silicon wafers require cleanroom handling to preserve sub-nanometer surface quality and prevent particulate contamination. Storage must occur in dry nitrogen or desiccator environments to minimize native oxide growth and organic contamination.

  • Particulate and Surface Contamination Control: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface contact and particle deposition.
  • Native Oxide Formation: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, requiring wet processing inside an exhaust fume hood or wet bench for removal before metallization or epitaxy.
  • Storage Atmosphere Requirements: Store unused wafers sealed inside the original cleanroom polypropylene cassette within a dry nitrogen cabinet to minimize airborne organic contamination.
  • Thermal Processing Compatibility: The 525 ± 25 μm thickness provides flexural rigidity for full-wafer photolithography steppers, PECVD/LPCVD cassettes, tube oxidation boats, and automated handling chucks.

Proper handling and pre-cleaning procedures preserve the dual-side mirror-polished CMP surface and ensure reproducible thin-film interfaces. Sequential solvent cleaning followed by plasma descum removes organic contaminants prior to photoresist spin coating or deposition.

Required Equipment: Cleanroom vacuum wand, PTFE/PEEK tweezers, Exhaust fume hood or wet bench, Dry nitrogen cabinet

  1. Inspect wafer cassette
    Verify that the cleanroom protective cassette immobilizes wafer edges and shows no signs of particulate contamination before opening.
  2. Handle by perimeter edge
    Transfer wafers using a cleanroom vacuum wand or PTFE/PEEK tweezers, contacting only the perimeter edge to avoid surface damage.
  3. Degrease sequentially
    Immerse wafers sequentially in acetone, electronic-grade isopropanol, and DI water to remove organic contaminants.
  4. Dry with nitrogen
    Blow-dry the wafer surface with filtered N2 gas until all visible liquid is removed.
  5. Perform plasma descum
    Apply a mild O2 plasma descum to remove residual organic material prior to photoresist spin coating or PVD/ALD deposition.
  6. Store in dry nitrogen cabinet
    Return unused wafers to the original cleanroom polypropylene cassette and store sealed inside a dry nitrogen cabinet.

What is the resistivity range of this 4-inch P-type silicon wafer and how does it affect device performance?

This wafer is Boron-doped to a resistivity of 0.01–0.1 Ω·cm (P+), verified by four-point probe. This low-resistivity range provides low bulk series resistance for vertical current conduction, making it suitable for ohmic contacts, electrochemical working electrodes, and anodic bonding. Compared to degenerately doped P++ substrates, it reduces free-carrier infrared absorption while maintaining adequate conductivity for device prototyping.

Can this double-side polished silicon wafer be used for KOH anisotropic etching and what crystal orientation does it have?

Yes, the wafer is sliced along the <100> crystal plane (± 0.5°), which supports predictable anisotropic wet-etch V-groove formation in KOH or TMAH solutions. The primary flat is oriented along <110> ± 1° with a length of 32.5 ± 2.5 mm, and the secondary flat is 18.0 ± 2.0 mm located 90° ± 5° clockwise from the primary flat (SEMI M1 100 mm P<100>). The dual-side CMP finish (Ra < 0.5 nm) also enables double-sided lithography and MEMS micromachining.

How should these prime silicon wafers be stored and handled to maintain surface quality?

Store wafers sealed inside the original cleanroom protective cassette within a dry nitrogen cabinet or cleanroom desiccator, away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface contamination. The wafers are supplied in cleanroom cassettes (10 pcs or 25 pcs options) that immobilize edges during transit, and each shipment includes a Certificate of Analysis documenting resistivity, thickness, orientation, and particle inspection (≤ 10 particles per wafer).

This 4-inch prime CZ P-type <100> silicon wafer combines a low 0.01–0.1 Ω·cm boron-doped bulk with dual-side CMP polishing (Ra < 0.5 nm) and SEMI M1 dimensional tolerances, making it well suited to double-side lithography, anodic/fusion bonding, and electrochemical electrode prototyping. Its bare, uncoated surface and 525 μm thickness demand cleanroom handling and in-house oxidation or cleaning steps before most device processes.

Positive

  • Low-resistivity P+ bulk conduction: Boron doping at 0.01–0.1 Ω·cm provides low bulk series resistance for vertical current conduction, anodic glass bonding, and electrochemical working electrodes while reducing free-carrier IR absorption versus degenerately doped P++ substrates.
  • Dual-side CMP mirror finish: Double-side polished surfaces with Ra < 0.5 nm support double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion or anodic bonding with reproducible thin-film growth and lithography.
  • <100> orientation for anisotropic etch: The <100> (± 0.5°) plane with four-fold symmetry and clean <110> cleaving enables predictable KOH/TMAH V-groove formation and Bosch DRIE micromachining with low Si/SiO2 interface state density.
  • SEMI M1 dimensional precision: 100.0 ± 0.3 mm diameter, 525 ± 25 μm thickness, TTV < 3 μm, and bow/warp < 25 μm ensure accurate registration on vacuum chucks, mask aligners, and automated handling cassettes.

Trade-offs

  • Bare surface requires pre-processing: Wafers ship uncoated with only a ~1–2 nm ambient native oxide; users must perform in-house thermal oxidation, RCA clean, or wet-etch native-oxide removal before metallization or epitaxy, adding process steps and cleanroom infrastructure.
  • Strict cleanroom handling required: Mirror-polished CMP surfaces must be handled only by the perimeter edge with vacuum wands or PTFE/PEEK tweezers and stored in dry nitrogen cabinets or desiccators away from particulates and corrosive vapors to preserve the ≤ 10 particles/wafer specification.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

10 pcs, 25 pcs

Diameter

4-Inch (100.0 ± 0.3 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

P-Type / Boron (B)

Orientation

± 0.5°

Resistivity

0.01-0.1 Ω·cm

Thickness

525 ± 25 μm

Surface Finish

Double-Side Polished (DSP, Ra < 0.5 nm)