4-Inch Arsenic-Doped Silicon Wafer 525μm ATOMFAIR®

Price range: $259.00 through $569.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Prime-grade 4-inch CZ N-type arsenic-doped silicon wafer, ±0.5°, 0.001–0.005 Ω·cm, 525 ±25 μm, DSP Ra <0.5 nm. SEMI M1 flats. In stock.

Diameter & Flat:
4-Inch (100.0 ± 0.3 mm)
Primary Flat 32.5 mm <110>
Substrate & Dopant:
CZ N-Type / Arsenic (As)
<111>•0.001–0.005 Ω·cm
Thickness:
525 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
DSP (Ra < 0.5 nm)
Dual-Side Mirror-Polished (CMP)

4-Inch (100 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Arsenic-doped to a verified resistivity of 0.001–0.005 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 100.0 ± 0.3 mm diameter and 525 ± 25 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).

Degenerately Arsenic (As)-doped to 0.001–0.005 Ω·cm (N++) (~1019–7×1019 cm-3 donor density), Arsenic matches the covalent atomic radius of silicon closely to minimize lattice strain and misfit dislocations at ultra-high doping while diffusing roughly an order of magnitude slower than Phosphorus. This makes heavily As-doped wafers the preferred prime substrate for Si/SiGe epitaxy, power MOSFETs, IGBTs, and low-series-resistance vertical ohmic contacts.

Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D.

4-Inch (100 mm) Thickness & Process Compatibility Note: The industry-standard 525 ± 25 μm mechanical thickness offers high flexural rigidity across full-wafer photolithography steppers, PECVD/LPCVD cassettes, epitaxial susceptors, and automated handling chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Double-Side Polished (DSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)

SEMI M1 4-Inch Dimensional Precision

Standardized 100.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.

  • Diameter: 100.0 ± 0.3 mm (4.0 Inch)
  • Primary Flat: 32.5 ± 2.5 mm along <110> ± 1°
  • Secondary Flat: 18.0 ± 2.0 mm secondary flat located 45° ± 5° clockwise from primary flat (SEMI M1 100 mm N<111>)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant N-Type / Arsenic (As) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 0.001–0.005 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <111> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 100.0 ± 0.3 mm (4-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 525 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 32.5 ± 2.5 mm SEMI M1 (100 mm)
Secondary Flat 18.0 ± 2.0 mm secondary flat located 45° ± 5° clockwise from primary flat (SEMI M1 100 mm N<111>) SEMI M1 (100 mm N<111>)
Surface Polish & Roughness Double-Side Polished (DSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Total Thickness Variation (TTV) & Bow/Warp TTV < 3 μm•Bow / Warp < 25 μm Non-Contact Optical Flatness
Surface Particle Inspection ≤ 10 particles / wafer (Cleanroom Audit) Bright-Light & Laser Surface Scan
Available Pack Sizes 10 pcs, 25 pcs cleanroom protective cassettes Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications

  • Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm) supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding;
  • Hexagonal Epitaxy & UHV Surface Physics: Dense three-fold <111> crystal lattice supports lattice-matched GaN/AlN/SiC heteroepitaxy, graphene/TMDC template growth, and discrete power/bipolar prototyping;
  • Semiconductor Device & Epitaxial Prototyping: Controlled Arsenic-doped (0.001–0.005 Ω·cm) base for ohmic contacts, power/RF devices, epitaxial growth, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.

Packaging, Storage & Handling Protocol

Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 4-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters, dopants, and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 4-Inch (100 mm), N-Type Arsenic (111), 0.001-0.005 ohm-cm, 525 um, DSP (This Product) 4-Inch (100 mm) / DSP 525 ± 25 μm, N-Type Arsenic (0.001–0.005 Ω·cm) SEMI M1 525 μm 100 mm wafer in 10 pcs / 25 pcs cassettes
4-Inch N-Type Arsenic <100> Wafer (0.001–0.005 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, N++ As <100> Low-strain, low-diffusivity As-doped epi & MOSFET substrate
4-Inch N-Type Antimony <100> Wafer (0.005–0.02 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, N+ Sb <100> Minimal autodoping Sb-doped wafer for sharp high-T epitaxy
4-Inch N-Type <110> Wafer (1–10 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, N-Type <110> Vertical-sidewall KOH MEMS & <110> lattice transport wafer
4-Inch N-Type <111> High-Res Wafer (100–1000 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, High-Res N <111> High-resistivity hexagonal <111> wafer for RF & III-nitride epi

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 4-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Prime-grade arsenic-doped silicon substrates require particulate-controlled storage and edge-only manipulation to preserve CMP surface integrity. Ambient native oxide growth and atmospheric contaminant adsorption must be managed prior to any oxidation, epitaxy, or metallization step.

  • Atmospheric Storage Environment: Store wafers sealed inside the original cleanroom cassette within a dry nitrogen cabinet or desiccator to limit airborne organic contamination and uncontrolled native oxide growth.
  • Edge-Only Manipulation: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid scratching or contaminating the mirror-polished faces.
  • Native Oxide Interfacial Control: Account for the ambient 1–2 nm native SiO2 layer when preparing ohmic contacts, epitaxial interfaces, or gate dielectrics, since it alters surface chemistry unless removed.
  • Wet-Chemical Containment: Perform all RCA cleans, oxide stripping, and wet etching inside an exhaust fume hood or wet bench under facility-approved EHS and SDS protocols.
  • Particulate and Vapor Exposure Limits: Avoid exposure to particulate dust and corrosive vapors, which degrade the sub-nanometer CMP finish and compromise lithographic registration.

This procedure covers cassette retrieval, edge-only transfer, solvent pre-cleaning, and native-oxide management for prime CZ arsenic-doped silicon substrates. Each step preserves the dual-side CMP finish and prepares the surface for lithography, epitaxy, or metallization.

Required Equipment: Cleanroom vacuum wand, PTFE or PEEK wafer tweezers, Cleanroom polypropylene cassette, Dry nitrogen cabinet or desiccator

  1. Retrieve wafer from sealed cassette
    Open the cleanroom polypropylene cassette inside a controlled environment and lift the wafer by its perimeter edge using a vacuum wand or PTFE/PEEK tweezers.
  2. Inspect surface for particulates
    Examine both polished faces under bright-light or laser surface scan to confirm particle counts remain within the ≤ 10 particles per wafer specification before processing.
  3. Degrease in solvent sequence
    Immerse the wafer sequentially in acetone, electronic-grade isopropanol, and DI water to remove organic residues from the CMP surface.
  4. Dry and descum
    Blow-dry the wafer with filtered N2 and apply a mild O2 plasma descum to eliminate residual organics prior to photoresist spin coating or PVD/ALD deposition.
  5. Remove native oxide if required
    Perform RCA standard clean or wet oxide stripping inside an exhaust fume hood under facility-approved EHS protocols when an oxide-free interface is needed for metallization or epitaxy.
  6. Return unused wafers to storage
    Seal any unused wafers back inside the original cleanroom cassette and place the cassette within a dry nitrogen cabinet to prevent recontamination.

Why choose arsenic-doped <111> silicon over phosphorus-doped <100> for epitaxial power device substrates?

Arsenic doping at 0.001–0.005 Ω·cm (N++) provides roughly an order of magnitude slower diffusion than phosphorus, which suppresses dopant out-diffusion and autodoping during high-temperature Si/SiGe epitaxy. The <111> orientation offers a densely packed three-fold surface symmetry with higher in-plane elastic modulus and slower wet alkaline etch kinetics than <100>, making it preferable for III-nitride heteroepitaxy and discrete power/bipolar R&D. Arsenic also closely matches the covalent atomic radius of silicon, minimizing lattice strain and misfit dislocations at ultra-high doping.

Can this 4-inch DSP arsenic-doped wafer be used for double-side lithography and wafer bonding?

Yes. The dual-side mirror-polished (DSP) CMP finish with Ra < 0.5 nm supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion or anodic bonding. The 525 ± 25 μm thickness provides high flexural rigidity for full-wafer photolithography steppers and automated handling chucks, while the SEMI M1 flats (32.5 mm primary, 18.0 mm secondary) ensure accurate registration on mask aligners and vacuum chucks.

What cleanroom handling and storage procedures are required to maintain the CMP surface quality of these prime silicon wafers?

Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers, and store unused wafers sealed inside the original cleanroom polypropylene cassette within a dry nitrogen cabinet or desiccator away from particulate dust and corrosive vapors. Bare prime silicon forms a ~1–2 nm native SiO2 film in air; if native oxide removal or RCA clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. All wet-chemical processing must follow institutional EHS and SDS safety protocols.

The 4-inch prime CZ silicon wafer with arsenic doping at 0.001–0.005 Ω·cm and <111> orientation offers a low-strain, low-diffusivity substrate ideal for Si/SiGe epitaxy and III-nitride growth, while its dual-side CMP finish (Ra < 0.5 nm) supports double-side lithography and wafer bonding. However, its high doping level and <111> orientation impose constraints on certain etch processes and require careful cleanroom handling to preserve surface quality.

Positive

  • Low lattice strain from arsenic doping: Arsenic's covalent radius closely matches silicon, minimizing misfit dislocations at ultra-high doping levels, which is critical for high-quality epitaxial layers.
  • Dual-side mirror polish for bonding: Double-side CMP with Ra < 0.5 nm enables direct fusion and anodic bonding, as well as double-sided MEMS patterning and through-wafer IR transmission.

Trade-offs

  • Slower wet etch kinetics on <111>: The <111> orientation exhibits slower alkaline etch rates compared to <100>, which may require adjusted etch times or alternative chemistries for certain MEMS or cleaning processes.
  • High doping limits high-resistivity applications: The 0.001–0.005 Ω·cm resistivity range is unsuitable for high-resistivity or RF applications where low loss and high isolation are required.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

10 pcs, 25 pcs

Diameter

4-Inch (100.0 ± 0.3 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

N-Type / Arsenic (As)

Orientation

± 0.5°

Resistivity

0.001-0.005 Ω·cm

Thickness

525 ± 25 μm

Surface Finish

Double-Side Polished (DSP, Ra < 0.5 nm)