4-Inch N-Type Arsenic Silicon Wafer 525μm DSP ATOMFAIR®

Price range: $249.00 through $549.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Prime CZ N-Type Arsenic silicon wafer, 100 mm, 525 μm, 0.001–0.005 Ω·cm, DSP Ra < 0.5 nm. SEMI M1 flats. In stock.

Diameter & Flat:
4-Inch (100.0 ± 0.3 mm)
Primary Flat 32.5 mm <110>
Substrate & Dopant:
CZ N-Type / Arsenic (As)
<100>•0.001–0.005 Ω·cm
Thickness:
525 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
DSP (Ra < 0.5 nm)
Dual-Side Mirror-Polished (CMP)

4-Inch (100 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Arsenic-doped to a verified resistivity of 0.001–0.005 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 100.0 ± 0.3 mm diameter and 525 ± 25 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).

Degenerately Arsenic (As)-doped to 0.001–0.005 Ω·cm (N++) (~1019–7×1019 cm-3 donor density), Arsenic matches the covalent atomic radius of silicon closely to minimize lattice strain and misfit dislocations at ultra-high doping while diffusing roughly an order of magnitude slower than Phosphorus. This makes heavily As-doped wafers the preferred prime substrate for Si/SiGe epitaxy, power MOSFETs, IGBTs, and low-series-resistance vertical ohmic contacts.

Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.

4-Inch (100 mm) Thickness & Process Compatibility Note: The industry-standard 525 ± 25 μm mechanical thickness offers high flexural rigidity across full-wafer photolithography steppers, PECVD/LPCVD cassettes, epitaxial susceptors, and automated handling chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Double-Side Polished (DSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)

SEMI M1 4-Inch Dimensional Precision

Standardized 100.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.

  • Diameter: 100.0 ± 0.3 mm (4.0 Inch)
  • Primary Flat: 32.5 ± 2.5 mm along <110> ± 1°
  • Secondary Flat: 18.0 ± 2.0 mm secondary flat located 180° ± 5° from primary flat (SEMI M1 100 mm N<100>)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant N-Type / Arsenic (As) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 0.001–0.005 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <100> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 100.0 ± 0.3 mm (4-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 525 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 32.5 ± 2.5 mm SEMI M1 (100 mm)
Secondary Flat 18.0 ± 2.0 mm secondary flat located 180° ± 5° from primary flat (SEMI M1 100 mm N<100>) SEMI M1 (100 mm N<100>)
Surface Polish & Roughness Double-Side Polished (DSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Total Thickness Variation (TTV) & Bow/Warp TTV < 3 μm•Bow / Warp < 25 μm Non-Contact Optical Flatness
Surface Particle Inspection ≤ 10 particles / wafer (Cleanroom Audit) Bright-Light & Laser Surface Scan
Available Pack Sizes 10 pcs, 25 pcs cleanroom protective cassettes Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications

  • Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm) supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding;
  • Power Devices, Epitaxy & Anisotropic MEMS: Standard <100> crystal plane supports abrupt epitaxial layer growth, vertical discrete power diodes/MOSFETs, and KOH/DRIE micromachining;
  • Semiconductor Device & Epitaxial Prototyping: Controlled Arsenic-doped (0.001–0.005 Ω·cm) base for ohmic contacts, power/RF devices, epitaxial growth, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.

Packaging, Storage & Handling Protocol

Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 4-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters, dopants, and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 4-Inch (100 mm), N-Type Arsenic (100), 0.001-0.005 ohm-cm, 525 um, DSP (This Product) 4-Inch (100 mm) / DSP 525 ± 25 μm, N-Type Arsenic (0.001–0.005 Ω·cm) SEMI M1 525 μm 100 mm wafer in 10 pcs / 25 pcs cassettes
4-Inch N-Type Arsenic <100> Wafer (0.001–0.005 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, N++ As <100> Low-strain, low-diffusivity As-doped epi & MOSFET substrate
4-Inch N-Type Antimony <100> Wafer (0.005–0.02 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, N+ Sb <100> Minimal autodoping Sb-doped wafer for sharp high-T epitaxy
4-Inch N-Type <110> Wafer (1–10 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, N-Type <110> Vertical-sidewall KOH MEMS & <110> lattice transport wafer
4-Inch N-Type <111> High-Res Wafer (100–1000 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, High-Res N <111> High-resistivity hexagonal <111> wafer for RF & III-nitride epi

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 4-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Prime-grade monocrystalline silicon wafers require cleanroom-compatible storage and edge-only handling to preserve CMP surface quality. Environmental exposure to particulates, corrosive vapors, and uncontrolled humidity must be avoided to prevent surface contamination and native oxide variability.

  • Storage Atmosphere: Store sealed wafers inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.
  • Handling Contact Restriction: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to prevent surface contact and particle transfer.
  • Native Oxide Sensitivity: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, requiring controlled wet processing before metallization or epitaxy.
  • Wet Processing Environment: Perform native oxide removal or RCA standard clean strictly inside an exhaust fume hood or wet bench using facility-approved protocols.
  • Cassette Storage Integrity: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Proper handling and pre-cleaning procedures preserve the dual-side CMP finish and ensure reproducible thin-film interfaces. Sequential solvent cleaning followed by plasma descum prepares the wafer surface for photoresist spin coating or PVD/ALD deposition.

Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Cleanroom polypropylene cassette, Exhaust fume hood or wet bench, O2 plasma descum system

  1. Inspect Cassette and Wafer Edges
    Inspect the cleanroom cassette and wafer edges for particulate contamination or physical damage before removal.
  2. Transfer Wafer by Perimeter Edge
    Transfer the wafer strictly by its perimeter edge using a cleanroom vacuum wand or PTFE/PEEK tweezers.
  3. Degrease in Solvent Sequence
    Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and DI water.
  4. Dry with Nitrogen
    Dry the wafer with a nitrogen blow-dry to remove residual solvent and water.
  5. Apply Mild O2 Plasma Descum
    Apply a mild O2 plasma descum prior to photoresist spin coating or PVD/ALD deposition.
  6. Perform Wet Processing in Approved Environment
    Perform native oxide removal or RCA standard clean strictly inside an exhaust fume hood or wet bench using facility-approved protocols.
  7. Return Unused Wafers to Sealed Storage
    Return unused wafers to the original cleanroom polypropylene cassette box within a dry nitrogen cabinet.

Why choose arsenic-doped silicon wafers over phosphorus-doped for N++ power device substrates?

Arsenic doping minimizes lattice strain and misfit dislocations at ultra-high doping levels because its covalent atomic radius closely matches that of silicon, and it diffuses roughly an order of magnitude slower than phosphorus. This product is degenerately doped to 0.001–0.005 Ω·cm (N++, ~10^19–7×10^19 cm⁻³ donor density), making it the preferred prime substrate for Si/SiGe epitaxy, power MOSFETs, IGBTs, and low-series-resistance vertical ohmic contacts where abrupt doping profiles and thermal stability are critical.

Can this 4-inch DSP wafer be used for double-sided lithography and wafer bonding?

Yes. The dual-side mirror-polished (DSP) surfaces with CMP finish (Ra < 0.5 nm) support double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion or anodic bonding. The 525 ± 25 μm thickness provides high flexural rigidity for handling in full-wafer photolithography steppers, PECVD/LPCVD cassettes, and epitaxial susceptors.

What are the storage and handling requirements to maintain the CMP surface quality of these prime silicon wafers?

Store wafers sealed inside the original cleanroom polypropylene cassette within a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to prevent surface contamination. The wafers are supplied in cleanroom protective cassettes (10 pcs or 25 pcs options) engineered to immobilize edges and prevent surface contact during transit.

The 4-inch prime CZ silicon wafer with arsenic doping at 0.001–0.005 Ω·cm and DSP finish (Ra < 0.5 nm) is a high-quality substrate for epitaxy, power devices, and MEMS, offering low lattice strain and slow dopant diffusion. However, its successful use requires cleanroom handling, native oxide management, and compatibility with standard 525 µm processing infrastructure.

Positive

  • Arsenic Doping Minimizes Lattice Strain: Arsenic's covalent radius closely matches silicon, reducing misfit dislocations at ultra-high doping levels (0.001–0.005 Ω·cm), which is critical for high-quality Si/SiGe epitaxy and low-resistance ohmic contacts.
  • Dual-Side Polish Enables Double-Side Processing: The DSP finish with Ra < 0.5 nm supports double-sided lithography, wafer bonding, and IR transmission applications, while also ensuring reproducible thin-film growth and lithography.

Trade-offs

  • Native Oxide Requires Removal: Bare prime silicon forms a 1–2 nm native oxide in ambient air, necessitating wet-chemical or plasma cleaning before metallization or epitaxy to ensure proper interface quality.
  • Cleanroom Handling Mandatory: To preserve surface cleanliness and prevent particulate contamination, wafers must be stored in dry nitrogen cabinets and handled with vacuum wands or PTFE tweezers in a cleanroom environment.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

10 pcs, 25 pcs

Diameter

4-Inch (100.0 ± 0.3 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

N-Type / Arsenic (As)

Orientation

± 0.5°

Resistivity

0.001-0.005 Ω·cm

Thickness

525 ± 25 μm

Surface Finish

Double-Side Polished (DSP, Ra < 0.5 nm)