| Diameter & Flat: 4-Inch (100.0 ± 0.3 mm) Primary Flat 32.5 mm <110> |
Substrate & Dopant: CZ N-Type / Phosphorus (P) <100>•1–10 Ω·cm |
Thickness: 300 ± 20 μm Prime-Grade Virgin Wafer |
Surface Polish: DSP (Ra < 0.5 nm) Dual-Side Mirror-Polished (CMP) |
1. Scientific Overview & Substrate Electrical Properties
4-Inch (100 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Phosphorus-doped to a verified resistivity of 1–10 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 100.0 ± 0.3 mm diameter and 300 ± 20 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).
Doped with Phosphorus to an industry-standard 1–10 Ω·cm n-type semiconducting range (~4.5×1014–5×1015 cm-3 donor density), the wafer provides uniform majority-electron transport for PMOS/CMOS device R&D, Schottky barrier rectifiers, PECVD/ALD dielectric C-V profiling, and cleanroom thin-film deposition.
Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.
4-Inch (100 mm) Thickness & Process Compatibility Note: The ultra-responsive 300 ± 20 μm substrate profile enables rapid through-wafer MEMS membrane etching, thinner optical/X-ray paths, and compliant bonded device stacks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.
|
SEMI M1 4-Inch Dimensional PrecisionStandardized 100.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | N-Type / Phosphorus (P) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 1–10 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <100> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 100.0 ± 0.3 mm (4-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 300 ± 20 μm | SEMI M1 / Capacitance Gauge |
| Primary Orientation Flat | Location: <110> ± 1°•Length: 32.5 ± 2.5 mm | SEMI M1 (100 mm) |
| Secondary Flat | 18.0 ± 2.0 mm secondary flat located 180° ± 5° from primary flat (SEMI M1 100 mm N<100>) | SEMI M1 (100 mm N<100>) |
| Surface Polish & Roughness | Double-Side Polished (DSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Total Thickness Variation (TTV) & Bow/Warp | TTV < 3 μm•Bow / Warp < 25 μm | Non-Contact Optical Flatness |
| Surface Particle Inspection | ≤ 10 particles / wafer (Cleanroom Audit) | Bright-Light & Laser Surface Scan |
| Available Pack Sizes | 10 pcs, 25 pcs cleanroom protective cassettes | Cleanroom Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm) supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding;
- MEMS & Anisotropic Silicon Micromachining: Cleanroom <100> crystal plane supports KOH / TMAH wet anisotropic etching and Bosch deep reactive ion etching (DRIE);
- Semiconductor Device & Electrode Prototyping: Controlled Phosphorus-doped (1–10 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
- In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 4-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters, thicknesses, and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 4-Inch (100 mm), N-Type (100), 1-10 ohm-cm, 300 um, DSP (This Product) | 4-Inch (100 mm) / DSP | 300 ± 20 μm, N-Type (1–10 Ω·cm) | SEMI M1 300 μm 100 mm wafer in 10 pcs / 25 pcs cassettes |
| 4-Inch N-Type <100> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, N-Type <100> | Standard SEMI M1 525 μm 100 mm N-type lithography substrate |
| 4-Inch N-Type <100> Wafer (1–10 Ω·cm, 525 μm DSP) | 4-Inch (100 mm) / DSP | 525 ± 25 μm, N-Type <100> | Double-side CMP polished N-type wafer for IR optics & wafer bonding |
| 4-Inch N-Type <111> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, N-Type <111> | Hexagonal <111> N-type substrate for III-nitride epitaxy & UHV growth |
| 4-Inch P-Type <110> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, P-Type <110> | Vertical-sidewall KOH MEMS & high hole-mobility <110> lattice |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 4-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade monocrystalline silicon wafers require cleanroom handling to preserve sub-nanometer surface quality and prevent particulate contamination. Storage must be in a dry nitrogen cabinet or desiccator to avoid native oxide growth and airborne organic contamination.
- Surface Contamination Control: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface contact and particle transfer.
- Native Oxide Formation: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, requiring wet processing in an exhaust fume hood or wet bench when oxide removal is needed.
- Storage Atmosphere: Store unused wafers sealed inside the original cleanroom polypropylene cassette within a dry nitrogen cabinet to minimize airborne organic contamination.
- Cleanroom Compatibility: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols to prevent contamination and ensure operator safety.
Proper handling and pre-cleaning procedures are essential to preserve the CMP mirror finish and ensure reproducible thin-film interfaces. These steps outline the sequence for degreasing, drying, and descumming prior to photoresist spin coating or deposition.
Required Equipment: Cleanroom vacuum wand, PTFE/PEEK tweezers, Exhaust fume hood or wet bench, O2 plasma descum system
- Inspect wafer cassette
Inspect the cleanroom protective cassette for damage and verify that wafers are immobilized without surface contact. - Transfer wafer
Transfer the wafer from the cassette using a cleanroom vacuum wand or PTFE/PEEK tweezers, handling only by the perimeter edge. - Degrease wafer
Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and DI water to remove organic contaminants. - Dry wafer
Dry the wafer with a nitrogen blow-dry to remove residual solvent and water. - Perform plasma descum
Perform a mild O2 plasma descum to remove trace organics prior to photoresist spin coating or PVD/ALD deposition. - Store unused wafers
Store unused wafers sealed inside the original cleanroom polypropylene cassette within a dry nitrogen cabinet.
What is the difference between this 300 µm DSP 4-inch N-type wafer and the 525 µm SSP version for MEMS membrane etching?
The 300 ± 20 µm thickness of this DSP wafer enables significantly faster through-wafer MEMS membrane etching than the 525 ± 25 µm SSP alternative, because the etch depth is reduced by roughly 225 µm. Additionally, the dual-side mirror-polished (DSP) surfaces with Ra < 0.5 nm support double-sided lithography and direct fusion or anodic bonding, which are not possible with single-side polished (SSP) wafers. For processes requiring rapid release of thin membranes or bonded stacks, the thinner DSP substrate is the appropriate choice.
Can this 4-inch N-type <100> prime silicon wafer be used directly for thermal oxidation without an RCA clean?
Yes, the wafer is a bare prime silicon substrate with only a thin ambient native oxide (~1–2 nm) and no added film or coating, so it can be loaded into a tube furnace for dry/wet thermal SiO2 growth after standard solvent pre-cleaning (acetone, IPA, DI water, N2 dry, optional O2 plasma descum). However, if you require removal of the native oxide or an RCA standard clean before oxidation or metallization, that wet processing must be performed in an exhaust fume hood or wet bench following your institutional EHS and SDS protocols. The wafer itself is not pre-cleaned or pre-oxidized; surface preparation is the user's responsibility.
What flat configuration does this SEMI M1 100 mm N-type <100> wafer have, and how does it affect cassette loading?
This wafer conforms to SEMI M1 for 100 mm N<100> and features a primary flat of 32.5 ± 2.5 mm along <110> ± 1° and a secondary flat of 18.0 ± 2.0 mm located 180° ± 5° from the primary flat. The primary flat provides crystal orientation reference for mask alignment and cleaving along <110> planes, while the secondary flat identifies the n-type <100> specification. Both flats are compatible with standard cleanroom cassettes and vacuum chucks designed for SEMI M1 100 mm wafers, ensuring proper registration during lithography and handling.
The 4-inch prime CZ N-type <100> silicon wafer with 300 µm thickness and dual-side CMP finish (Ra < 0.5 nm) offers a thin, low-defect substrate well-suited for through-wafer MEMS etching, double-side lithography, and direct bonding. Its 1–10 Ω·cm phosphorus doping and SEMI M1 flats ensure reproducible device prototyping, though the thin profile demands careful handling to avoid fracture and the bare surface requires immediate native-oxide management before critical deposition steps.
Positive
- Thin 300 µm profile enables rapid through-wafer processing: The 300 ± 20 µm thickness reduces etch times for MEMS membrane release and shortens optical/X-ray path lengths, while remaining compatible with standard cleanroom handling when using appropriate vacuum wands or tweezers.
- Dual-side CMP finish supports double-sided lithography and bonding: DSP with Ra < 0.5 nm on both faces allows double-sided MEMS patterning, through-wafer IR transmission, and direct fusion or anodic bonding without additional surface preparation.
Trade-offs
- Thin substrate requires careful handling to prevent fracture: At 300 µm, the wafer is more fragile than standard 525 µm substrates; strict edge-only handling with cleanroom vacuum wands or PTFE/PEEK tweezers is necessary to avoid breakage during cassette loading and processing.
- Bare silicon surface demands immediate native-oxide control: The absence of a protective coating means a ~1–2 nm native SiO2 layer forms in ambient air; wet-chemical removal or RCA cleaning must be performed in an exhaust fume hood or wet bench following institutional EHS protocols before metallization or epitaxy.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).