| Diameter & Flat: 4-Inch (100.0 ± 0.3 mm) Primary Flat 32.5 mm <110> |
Substrate & Dopant: CZ N-Type / Phosphorus (P) <100>•0.001–0.005 Ω·cm |
Thickness: 525 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: DSP (Ra < 0.5 nm) Dual-Side Mirror-Polished (CMP) |
1. Scientific Overview & Substrate Electrical Properties
4-Inch (100 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Phosphorus-doped to a verified resistivity of 0.001–0.005 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 100.0 ± 0.3 mm diameter and 525 ± 25 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).
Degenerately Phosphorus-doped to 0.001–0.005 Ω·cm (N++) (~1019–1020 cm-3 electron density), the wafer delivers metallic-like bulk conductivity for low-resistance backside ohmic contacts, conductive bottom gates, III-V/GaN buffer heteroepitaxy, and high-current device testing.
Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.
4-Inch (100 mm) Thickness & Process Compatibility Note: The industry-standard 525 ± 25 μm mechanical thickness offers high flexural rigidity across full-wafer photolithography steppers, PECVD/LPCVD cassettes, tube oxidation boats, and automated handling chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.
|
SEMI M1 4-Inch Dimensional PrecisionStandardized 100.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | N-Type / Phosphorus (P) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 0.001–0.005 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <100> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 100.0 ± 0.3 mm (4-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 525 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Orientation Flat | Location: <110> ± 1°•Length: 32.5 ± 2.5 mm | SEMI M1 (100 mm) |
| Secondary Flat | 18.0 ± 2.0 mm secondary flat located 180° ± 5° from primary flat (SEMI M1 100 mm N<100>) | SEMI M1 (100 mm N<100>) |
| Surface Polish & Roughness | Double-Side Polished (DSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Total Thickness Variation (TTV) & Bow/Warp | TTV < 3 μm•Bow / Warp < 25 μm | Non-Contact Optical Flatness |
| Surface Particle Inspection | ≤ 10 particles / wafer (Cleanroom Audit) | Bright-Light & Laser Surface Scan |
| Available Pack Sizes | 10 pcs, 25 pcs cleanroom protective cassettes | Cleanroom Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm) supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding;
- MEMS & Anisotropic Silicon Micromachining: Cleanroom <100> crystal plane supports KOH / TMAH wet anisotropic etching and Bosch deep reactive ion etching (DRIE);
- Semiconductor Device & Electrode Prototyping: Controlled Phosphorus-doped (0.001–0.005 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
- In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 4-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters, thicknesses, and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 4-Inch (100 mm), N-Type (100), 0.001-0.005 ohm-cm, 525 um, DSP (This Product) | 4-Inch (100 mm) / DSP | 525 ± 25 μm, N-Type (0.001–0.005 Ω·cm) | SEMI M1 525 μm 100 mm wafer in 10 pcs / 25 pcs cassettes |
| 4-Inch N-Type <100> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, N-Type <100> | Standard SEMI M1 525 μm 100 mm N-type lithography substrate |
| 4-Inch N-Type <100> Wafer (1–10 Ω·cm, 525 μm DSP) | 4-Inch (100 mm) / DSP | 525 ± 25 μm, N-Type <100> | Double-side CMP polished N-type wafer for IR optics & wafer bonding |
| 4-Inch N-Type <111> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, N-Type <111> | Hexagonal <111> N-type substrate for III-nitride epitaxy & UHV growth |
| 4-Inch P-Type <110> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, P-Type <110> | Vertical-sidewall KOH MEMS & high hole-mobility <110> lattice |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 4-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade monocrystalline silicon wafers require cleanroom handling to prevent particulate contamination and surface damage. Storage must occur in a dry nitrogen cabinet or desiccator to minimize native oxide growth and airborne organic contamination.
- Cleanroom Handling Requirement: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface contact and particle transfer.
- Storage Atmosphere Control: Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.
- Native Oxide Sensitivity: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, requiring controlled wet processing for removal before metallization or epitaxy.
- Wet Processing Safety: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols.
Proper handling and pre-cleaning procedures preserve mirror-polished CMP cleanliness and ensure reproducible thin-film interfaces. These steps must be performed in a cleanroom environment following institutional safety protocols.
Required Equipment: Cleanroom vacuum wand, PTFE/PEEK tweezers, Dry nitrogen cabinet or cleanroom desiccator, Exhaust fume hood or wet bench
- Inspect wafer cassette
Inspect the cleanroom protective cassette for integrity and verify that wafers are immobilized without surface contact. - Handle by perimeter edge
Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers. - Degrease wafer surfaces
Degrease diced dies or whole wafers sequentially in acetone, electronic-grade isopropanol, and DI water. - Dry and descum
Blow-dry with nitrogen and perform a mild O2 plasma descum prior to photoresist spin coating or PVD/ALD. - Remove native oxide if required
Perform wet processing for native oxide removal or RCA standard clean strictly inside an exhaust fume hood or wet bench using facility-approved protocols. - Store unused wafers
Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet.
Can a 0.001–0.005 Ω·cm N++ silicon wafer be used for epitaxial growth without a heavily doped buffer layer?
Yes. The degenerately phosphorus-doped bulk (N++, ~10^19–10^20 cm^-3) provides metallic-like conductivity that can serve directly as a conductive substrate for III-V/GaN buffer heteroepitaxy and low-resistance backside ohmic contacts, reducing or eliminating the need for an additional heavily doped epitaxial buffer. The <100> ± 0.5° orientation and DSP surface with Ra < 0.5 nm support reproducible thin-film nucleation. However, because the wafer is bare prime silicon with only a ~1–2 nm native oxide, any epitaxial or metallization step still requires an in-house native-oxide removal or RCA clean before growth.
What are the SEMI M1 flat specifications for this 4-inch N-type <100> wafer?
This 100 mm N-type <100> prime wafer follows SEMI M1 flat geometry: a primary flat of 32.5 ± 2.5 mm located along <110> ± 1°, and a secondary flat of 18.0 ± 2.0 mm positioned 180° ± 5° from the primary flat. These flats are critical for consistent crystallographic registration on mask aligners, vacuum chucks, and cleanroom cassettes. The wafer diameter is held to 100.0 ± 0.3 mm and thickness to 525 ± 25 μm, both verified per batch on the Certificate of Analysis.
How should these DSP prime silicon wafers be stored and handled to preserve the Ra < 0.5 nm CMP surface?
Store unused wafers sealed in the original cleanroom polypropylene cassette inside a dry nitrogen cabinet or cleanroom desiccator, away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers — never touch the mirror-polished face. The dual-side CMP finish (Ra < 0.5 nm) and ≤ 10 particles/wafer inspection limit are only maintained if the cassette remains closed between processing steps; bare prime silicon also forms a ~1–2 nm native oxide in air, so solvent/IPA/DI pre-cleaning and optional O2 plasma descum are recommended before photoresist or PVD/ALD.
The 4-inch prime CZ N-type silicon wafer with degenerate phosphorus doping (0.001–0.005 Ω·cm) and dual-side CMP finish (Ra < 0.5 nm) is engineered for low-resistance ohmic contacts, III-V/GaN heteroepitaxy, and double-side lithography. Its 525 μm thickness and SEMI M1 flats ensure compatibility with automated cleanroom handling, though the reactive bare surface and tight resistivity window demand strict environmental control and process discipline.
Positive
- Degenerate N++ Doping for Ohmic Contacts: Phosphorus doping at 0.001–0.005 Ω·cm (~10^19–10^20 cm^-3) provides metallic-like bulk conductivity, enabling low-resistance backside ohmic contacts and conductive bottom gates without additional implant steps.
- Dual-Side CMP for Bonding and Lithography: Double-side mirror polish (Ra < 0.5 nm) supports double-sided MEMS patterning, through-wafer IR transmission, and direct fusion or anodic bonding with minimal surface roughness-induced defects.
Trade-offs
- Reactive Bare Silicon Surface: The native ~1–2 nm SiO2 film grows in ambient air, requiring controlled pre-clean (e.g., RCA or plasma descum) before metallization or epitaxy to avoid interfacial contamination or contact resistance variability.
- Tight Resistivity Tolerance: The 0.001–0.005 Ω·cm window demands careful process control during high-temperature steps to prevent dopant out-diffusion or unintended compensation, which could shift device characteristics.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).