| Diameter & Flat: 4-Inch (100.0 ± 0.3 mm) Primary Flat 32.5 mm <110> |
Substrate & Dopant: CZ P-Type / Boron (B) <100>•1–10 Ω·cm |
Thickness: 380 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: DSP (Ra < 0.5 nm) Dual-Side Mirror-Polished (CMP) |
1. Scientific Overview & Substrate Electrical Properties
4-Inch (100 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 1–10 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 100.0 ± 0.3 mm diameter and 380 ± 25 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).
Doped with Boron to an industry-standard 1–10 Ω·cm semiconducting resistivity range, the wafer provides a well-characterized majority-hole carrier profile for MOSFET/CMOS device prototyping, Schottky barrier testing, PECVD/ALD dielectric C-V metrology, and general thin-film deposition.
Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.
4-Inch (100 mm) Thickness & Process Compatibility Note: The thinned 380 ± 25 μm profile accelerates through-wafer DRIE/wet etching, enhances thermal transfer during rapid thermal processing (RTP), and increases mid/far-infrared optical transmission. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.
|
SEMI M1 4-Inch Dimensional PrecisionStandardized 100.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | P-Type / Boron (B) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 1–10 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <100> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 100.0 ± 0.3 mm (4-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 380 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Orientation Flat | Location: <110> ± 1°•Length: 32.5 ± 2.5 mm | SEMI M1 (100 mm) |
| Secondary Flat | 18.0 ± 2.0 mm secondary flat located 90° ± 5° clockwise from primary flat (SEMI M1 100 mm P<100>) | SEMI M1 (100 mm P<100>) |
| Surface Polish & Roughness | Double-Side Polished (DSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Total Thickness Variation (TTV) & Bow/Warp | TTV < 3 μm•Bow / Warp < 25 μm | Non-Contact Optical Flatness |
| Surface Particle Inspection | ≤ 10 particles / wafer (Cleanroom Audit) | Bright-Light & Laser Surface Scan |
| Available Pack Sizes | 10 pcs, 25 pcs cleanroom protective cassettes | Cleanroom Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm) supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding;
- MEMS & Anisotropic Silicon Micromachining: Cleanroom <100> crystal plane supports KOH / TMAH wet anisotropic etching and Bosch deep reactive ion etching (DRIE);
- Semiconductor Device & Electrode Prototyping: Controlled Boron-doped (1–10 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
- In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 4-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters, thicknesses, and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 4-Inch (100 mm), P-Type (100), 1-10 ohm-cm, 380 um, DSP (This Product) | 4-Inch (100 mm) / DSP | 380 ± 25 μm, P-Type (1–10 Ω·cm) | SEMI M1 380 μm 100 mm wafer in 10 pcs / 25 pcs cassettes |
| 4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, P-Type <100> | Standard SEMI M1 525 μm 100 mm lithography substrate |
| 4-Inch P-Type <100> Wafer (1–10 Ω·cm, 500 μm SSP) | 4-Inch (100 mm) / SSP | 500 ± 15 μm, P-Type <100> | 500 ± 15 μm precision thickness for MEMS & DRIE etching |
| 4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm DSP) | 4-Inch (100 mm) / DSP | 525 ± 25 μm, P-Type <100> | Double-side CMP polished for IR optics & fusion bonding |
| 4-Inch P-Type <111> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, P-Type <111> | Hexagonal <111> lattice for III-nitride epitaxy & UHV growth |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 4-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade monocrystalline silicon wafers require particulate-controlled storage and edge-only manipulation to preserve CMP surface integrity. Ambient native oxide growth and ionic contamination must be managed prior to critical thin-film or metallization steps.
- Cleanroom Storage Atmosphere: Store wafers sealed in the original polypropylene cassette inside a dry nitrogen cabinet or cleanroom desiccator to minimize airborne organic contamination and native oxide growth.
- Edge-Only Manipulation: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid scratching or contaminating the mirror-polished surfaces.
- Native Oxide Control: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, which must be removed via RCA standard clean or wet processing inside an exhaust fume hood before metallization or epitaxy.
- Wet-Chemical Safety Compliance: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols.
Proper pre-cleaning and handling procedures preserve the CMP mirror finish and ensure reproducible thin-film interfaces. Sequential solvent cleaning followed by plasma descum removes organic contamination prior to deposition or lithography.
Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Exhaust fume hood or wet bench, O2 plasma descum system, Dry nitrogen cabinet or cleanroom desiccator
- Inspect Cassette and Wafer Edges
Inspect the cleanroom cassette and wafer edges for particulate contamination or physical damage before opening. - Transfer Wafer by Perimeter Edge
Transfer the wafer using a cleanroom vacuum wand or PTFE/PEEK tweezers applied only to the perimeter edge. - Degrease in Solvent Sequence
Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and DI water inside an exhaust fume hood. - Dry with Nitrogen
Dry the wafer with a filtered N2 blow-dry until all solvent residue is removed. - Perform Plasma Descum
Perform a mild O2 plasma descum to remove residual organic contamination prior to photoresist spin coating or PVD/ALD. - Return Unused Wafers to Storage
Return unused wafers to the original polypropylene cassette and store sealed inside a dry nitrogen cabinet.
What is the difference between DSP and SSP silicon wafers for MEMS and bonding applications?
This 4-inch wafer is Double-Side Polished (DSP) with a CMP finish of Ra < 0.5 nm on both faces, whereas SSP (single-side polished) wafers have only one mirror surface. The dual-side CMP finish supports double-sided lithography, through-wafer infrared transmission, and direct fusion or anodic bonding, which require both surfaces to be planar and defect-free. For standard single-side lithography, an SSP wafer may be sufficient, but DSP is necessary when both faces are functionalized or optically accessed.
Can this 380 µm thick 4-inch silicon wafer be used for KOH anisotropic etching and DRIE?
Yes. The <100> crystal orientation (± 0.5°) with a primary flat along <110> ± 1° supports predictable anisotropic wet-etch V-groove formation in KOH or TMAH solutions, as well as Bosch deep reactive ion etching (DRIE). The 380 ± 25 µm thickness accelerates through-wafer etching compared to standard 525 µm wafers, reducing process time for membranes and vias. The low TTV (< 3 µm) and bow/warp (< 25 µm) help maintain uniform etch depth across the wafer.
How should prime-grade silicon wafers be stored and handled to preserve surface quality?
Store wafers sealed inside the original cleanroom protective cassette within a dry nitrogen cabinet or cleanroom desiccator, away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers; never touch the polished faces. The DSP surface has Ra < 0.5 nm and ≤ 10 particles per wafer, so any contact or airborne contamination can degrade lithography and thin-film adhesion.
The 4-inch prime CZ P-type <100> silicon wafer with 380 µm thickness and dual-side CMP polish (Ra < 0.5 nm) offers a well-characterized boron-doped substrate for MEMS, device prototyping, and thin-film calibration, with SEMI M1 flats and low TTV/bow ensuring lithographic registration. Its thin profile aids through-wafer etching and IR transmission, but requires careful edge handling and dry storage to preserve the native oxide and particle specification.
Positive
- Dual-side CMP for bonding and lithography: Double-side polished surfaces with Ra < 0.5 nm enable double-sided MEMS patterning, direct fusion/anodic bonding, and reproducible thin-film growth.
- Thin 380 µm profile aids etching and IR: The 380 ± 25 µm thickness accelerates through-wafer DRIE/wet etching, enhances thermal transfer during RTP, and increases mid/far-infrared optical transmission.
Trade-offs
- Native oxide requires controlled removal: Bare prime silicon forms a ~1–2 nm ambient native SiO2 film; wet processing for oxide removal or RCA clean must be performed in an exhaust fume hood or wet bench following institutional EHS and SDS protocols.
- Strict cleanroom handling and storage: Wafers must be handled by the perimeter edge with vacuum wands or PTFE/PEEK tweezers and stored sealed in a dry nitrogen cabinet or cleanroom desiccator to prevent particulate contamination and preserve the ≤10 particles/wafer specification.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).