| Diameter & Flat: 4-Inch (100.0 ± 0.3 mm) Primary Flat 32.5 mm <110> |
Substrate & Dopant: CZ P-Type / Boron (B) <100>•10–20 Ω·cm |
Thickness: 525 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: SSP (Ra < 0.5 nm) Polished Front / Fine-Ground Back |
1. Scientific Overview & Substrate Electrical Properties
4-Inch (100 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 10–20 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 100.0 ± 0.3 mm diameter and 525 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.
Boron-doped to 10–20 Ω·cm (~1015 cm-3 dopant density), this moderate-resistivity substrate minimizes impurity scattering and junction capacitance compared with heavily doped wafers, supporting MOS C-V gate characterization, minority-carrier diffusion studies, and photodiode test structures.
Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.
4-Inch (100 mm) Thickness & Process Compatibility Note: The industry-standard 525 ± 25 μm mechanical thickness offers high flexural rigidity across full-wafer photolithography steppers, PECVD/LPCVD cassettes, tube oxidation boats, and automated handling chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.
|
SEMI M1 4-Inch Dimensional PrecisionStandardized 100.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | P-Type / Boron (B) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 10–20 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <100> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 100.0 ± 0.3 mm (4-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 525 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Orientation Flat | Location: <110> ± 1°•Length: 32.5 ± 2.5 mm | SEMI M1 (100 mm) |
| Secondary Flat | 18.0 ± 2.0 mm secondary flat located 90° ± 5° clockwise from primary flat (SEMI M1 100 mm P<100>) | SEMI M1 (100 mm P<100>) |
| Surface Polish & Roughness | Single-Side Polished (SSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Total Thickness Variation (TTV) & Bow/Warp | TTV < 5 μm•Bow / Warp < 30 μm | Non-Contact Optical Flatness |
| Surface Particle Inspection | ≤ 10 particles / wafer (Cleanroom Audit) | Bright-Light & Laser Surface Scan |
| Available Pack Sizes | 10 pcs, 25 pcs cleanroom protective cassettes | Cleanroom Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for PVD sputtering, ALD, e-beam evaporation, and high-resolution photoresist spin coating;
- MEMS & Anisotropic Silicon Micromachining: Cleanroom <100> crystal plane supports KOH / TMAH wet anisotropic etching and Bosch deep reactive ion etching (DRIE);
- Semiconductor Device & Electrode Prototyping: Controlled Boron-doped (10–20 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
- In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 4-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters, thicknesses, and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 4-Inch (100 mm), P-Type (100), 10-20 ohm-cm, 525 um, SSP (This Product) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, P-Type (10–20 Ω·cm) | SEMI M1 525 μm 100 mm wafer in 10 pcs / 25 pcs cassettes |
| 4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, P-Type <100> | Standard SEMI M1 525 μm 100 mm lithography substrate |
| 4-Inch P-Type <100> Wafer (1–10 Ω·cm, 500 μm SSP) | 4-Inch (100 mm) / SSP | 500 ± 15 μm, P-Type <100> | 500 ± 15 μm precision thickness for MEMS & DRIE etching |
| 4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm DSP) | 4-Inch (100 mm) / DSP | 525 ± 25 μm, P-Type <100> | Double-side CMP polished for IR optics & fusion bonding |
| 4-Inch P-Type <111> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, P-Type <111> | Hexagonal <111> lattice for III-nitride epitaxy & UHV growth |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 4-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade virgin silicon wafers require cleanroom handling to prevent particulate contamination and surface damage. Storage in a dry nitrogen cabinet or desiccator is necessary to minimize native oxide growth and airborne organic contamination.
- Particulate and Surface Contamination Control: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid scratching the polished surface or introducing particles.
- Native Oxide Formation: Bare prime silicon forms an ambient native silicon dioxide layer of approximately 1–2 nm in air, which must be removed prior to processes requiring an oxide-free interface.
- Storage Environment: Store unused wafers sealed inside the original cleanroom cassette within a dry nitrogen cabinet or desiccator away from particulate dust and corrosive vapors.
- Thermal and Mechanical Stress Limits: The 525 ± 25 μm thickness provides flexural rigidity for automated handling, but rapid thermal cycling or mechanical shock can induce slip or fracture.
Proper handling and cleaning of prime silicon wafers are critical to preserve surface quality and ensure reproducible thin-film deposition or lithography. The following steps outline standard cleanroom procedures for preparing wafers for processing.
Required Equipment: Cleanroom vacuum wand, PTFE/PEEK tweezers, Cleanroom cassette, Dry nitrogen cabinet
- Inspect wafer cassette
Verify that the cleanroom cassette is intact and free of particulate contamination before opening. - Handle wafer by edge
Use a cleanroom vacuum wand or PTFE/PEEK tweezers to grip the wafer strictly by its perimeter edge. - Perform solvent pre-cleaning
Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and deionized water, then blow-dry with nitrogen. - Remove native oxide if required
Perform wet-chemical native oxide removal or RCA standard clean inside an exhaust fume hood or wet bench using facility-approved protocols. - Store unused wafers properly
Return unused wafers to the original cleanroom cassette and store in a dry nitrogen cabinet or desiccator.
What is the resistivity of this 4-inch P-type silicon wafer and how does it affect MOS C-V characterization?
This wafer is Boron-doped to a verified resistivity of 10–20 Ω·cm, corresponding to a dopant density of approximately 10^15 cm⁻³. This moderate resistivity minimizes impurity scattering and junction capacitance compared with heavily doped wafers, making it well-suited for MOS C-V gate characterization, minority-carrier diffusion studies, and photodiode test structures. The resistivity is measured by four-point probe (4PP) and documented on the Certificate of Analysis.
Can this SSP wafer be used for KOH anisotropic etching and DRIE MEMS processing?
Yes. The <100> crystal orientation (± 0.5°) supports predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions and is compatible with Bosch deep reactive ion etching (DRIE). The primary flat is aligned along <110> ± 1° per SEMI M1, ensuring accurate mask registration. The single-side polished front surface (Ra < 0.5 nm) provides uniform nucleation for subsequent thin-film deposition or photoresist spin coating.
How should these prime silicon wafers be stored and handled to maintain surface quality?
Store wafers sealed inside the original cleanroom protective cassette within a dry nitrogen cabinet or cleanroom desiccator, away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers. The wafers are supplied in 10 pcs or 25 pcs cassettes engineered to immobilize edges and prevent surface contact during transit.
This 4-inch prime CZ P-type <100> silicon wafer at 10–20 Ω·cm and 525 μm SSP delivers a moderate-resistivity, SEMI M1-compliant substrate suited to MOS C-V characterization, anisotropic KOH/TMAH micromachining, and thin-film nucleation. Its bare, virgin surface and tight TTV/bow tolerances support in-house oxidation and lithography, but deployment requires cleanroom handling, dry nitrogen storage, and wet-bench infrastructure for native-oxide removal.
Positive
- Moderate resistivity reduces junction capacitance: Boron doping at 10–20 Ω·cm (~10^15 cm⁻³) minimizes impurity scattering and junction capacitance versus heavily doped wafers, supporting MOS C-V gate characterization, minority-carrier diffusion studies, and photodiode test structures.
- <100> plane enables anisotropic micromachining: The <100> (± 0.5°) orientation provides four-fold rotational symmetry, clean <110> cleaving, low Si/SiO2 interface state density, and predictable V-groove formation in KOH/TMAH, with compatibility for Bosch DRIE.
- CMP mirror surface for thin-film nucleation: Single-side polished front with Ra < 0.5 nm supports uniform nucleation for PVD sputtering, ALD, e-beam evaporation, and high-resolution photoresist spin coating.
- SEMI M1 geometry ensures tool registration: 100.0 ± 0.3 mm diameter with SEMI M1 flats (32.5 mm primary <110>, 18.0 mm secondary) and TTV < 5 μm / bow-warp < 30 μm enable accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.
Trade-offs
- Native oxide requires wet-bench removal: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air; removal or RCA standard clean before metallization or epitaxy must be performed in an exhaust fume hood or wet bench under facility-approved EHS and SDS protocols.
- Cleanroom storage and edge handling required: Wafers must be stored sealed in a dry nitrogen cabinet or cleanroom desiccator away from particulates and corrosive vapors, and handled strictly by the perimeter edge using vacuum wands or PTFE/PEEK tweezers to preserve the CMP surface.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).