| Diameter & Flat: 4-Inch (100.0 ± 0.3 mm) Primary Flat 32.5 mm <110> |
Substrate & Dopant: CZ P-Type / Boron (B) <100>•20–50 Ω·cm |
Thickness: 525 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: DSP (Ra < 0.5 nm) Dual-Side Mirror-Polished (CMP) |
1. Scientific Overview & Substrate Electrical Properties
4-Inch (100 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 20–50 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 100.0 ± 0.3 mm diameter and 525 ± 25 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).
Boron-doped to 20–50 Ω·cm (~3×1014–7×1014 cm-3 hole concentration), this low-doping substrate widens depletion layers and lowers junction capacitance for optical/particle photodetectors, PIN photodiodes, and low-noise analog test structures.
Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.
4-Inch (100 mm) Thickness & Process Compatibility Note: The industry-standard 525 ± 25 μm mechanical thickness offers high flexural rigidity across full-wafer photolithography steppers, PECVD/LPCVD cassettes, tube oxidation boats, and automated handling chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.
|
SEMI M1 4-Inch Dimensional PrecisionStandardized 100.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | P-Type / Boron (B) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 20–50 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <100> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 100.0 ± 0.3 mm (4-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 525 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Orientation Flat | Location: <110> ± 1°•Length: 32.5 ± 2.5 mm | SEMI M1 (100 mm) |
| Secondary Flat | 18.0 ± 2.0 mm secondary flat located 90° ± 5° clockwise from primary flat (SEMI M1 100 mm P<100>) | SEMI M1 (100 mm P<100>) |
| Surface Polish & Roughness | Double-Side Polished (DSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Total Thickness Variation (TTV) & Bow/Warp | TTV < 3 μm•Bow / Warp < 25 μm | Non-Contact Optical Flatness |
| Surface Particle Inspection | ≤ 10 particles / wafer (Cleanroom Audit) | Bright-Light & Laser Surface Scan |
| Available Pack Sizes | 10 pcs, 25 pcs cleanroom protective cassettes | Cleanroom Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm) supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding;
- MEMS & Anisotropic Silicon Micromachining: Cleanroom <100> crystal plane supports KOH / TMAH wet anisotropic etching and Bosch deep reactive ion etching (DRIE);
- Semiconductor Device & Electrode Prototyping: Controlled Boron-doped (20–50 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
- In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 4-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters, thicknesses, and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 4-Inch (100 mm), P-Type (100), 20-50 ohm-cm, 525 um, DSP (This Product) | 4-Inch (100 mm) / DSP | 525 ± 25 μm, P-Type (20–50 Ω·cm) | SEMI M1 525 μm 100 mm wafer in 10 pcs / 25 pcs cassettes |
| 4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, P-Type <100> | Standard SEMI M1 525 μm 100 mm lithography substrate |
| 4-Inch P-Type <100> Wafer (1–10 Ω·cm, 500 μm SSP) | 4-Inch (100 mm) / SSP | 500 ± 15 μm, P-Type <100> | 500 ± 15 μm precision thickness for MEMS & DRIE etching |
| 4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm DSP) | 4-Inch (100 mm) / DSP | 525 ± 25 μm, P-Type <100> | Double-side CMP polished for IR optics & fusion bonding |
| 4-Inch P-Type <111> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, P-Type <111> | Hexagonal <111> lattice for III-nitride epitaxy & UHV growth |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 4-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade monocrystalline silicon wafers require cleanroom handling to preserve sub-nanometer surface quality and prevent particulate contamination. Storage must be in dry nitrogen or desiccator environments to minimize native oxide growth and airborne organic contamination.
- Surface Contamination Sensitivity: Mirror-polished CMP surfaces with Ra < 0.5 nm are highly susceptible to particulate and organic contamination, requiring cleanroom vacuum wands or PTFE/PEEK tweezers for edge-only handling.
- Native Oxide Formation: Bare prime silicon forms a 1–2 nm native SiO2 film in ambient air, which must be removed via RCA clean or wet processing before metallization or epitaxy if an oxide-free interface is required.
- Storage Atmosphere Requirements: Unused wafers must remain sealed in original cleanroom cassettes within a dry nitrogen cabinet or desiccator to prevent moisture-driven oxidation and organic contamination.
- Wet Processing Safety: All wet-chemical processing including RCA clean, KOH/TMAH etching, and solvent degreasing must be performed in an exhaust fume hood or wet bench following institutional EHS and SDS protocols.
Proper handling preserves the CMP mirror finish and prevents contamination that degrades lithography and thin-film interfaces. Sequential solvent cleaning followed by plasma descum prepares the surface for photoresist or deposition.
Required Equipment: Cleanroom vacuum wand, PTFE or PEEK tweezers, Cleanroom cassette, Dry nitrogen cabinet
- Inspect wafer cassette
Verify the cleanroom cassette is intact and wafers are properly seated without edge contact before opening in a controlled environment. - Transfer wafer by edge
Handle the wafer strictly by its perimeter edge using a cleanroom vacuum wand or PTFE/PEEK tweezers to avoid surface contact. - Degrease in solvent sequence
Immerse the wafer sequentially in acetone, electronic-grade isopropanol, and DI water to remove organic contaminants. - Dry with nitrogen
Blow-dry the wafer surface with filtered N2 gas to remove residual solvent and water droplets. - Perform plasma descum
Apply a mild O2 plasma descum to remove trace organics prior to photoresist spin coating or PVD/ALD deposition. - Store unused wafers
Return unused wafers to the original cleanroom cassette and store sealed inside a dry nitrogen cabinet or desiccator.
What is the resistivity range of this 4-inch P-type <100> silicon wafer and how does it affect device performance?
This wafer is Boron-doped to a verified resistivity of 20–50 Ω·cm, corresponding to a hole concentration of approximately 3×10¹⁴–7×10¹⁴ cm⁻³. This low doping level widens depletion layers and lowers junction capacitance, making the substrate suitable for optical/particle photodetectors, PIN photodiodes, and low-noise analog test structures. The resistivity is verified per batch by four-point probe (4PP) and documented on the Certificate of Analysis.
Can this double-side polished 4-inch silicon wafer be used for KOH anisotropic etching and wafer bonding?
Yes. The <100> crystal orientation (± 0.5°) supports predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions and Bosch deep reactive ion etching (DRIE). The dual-side CMP mirror finish (DSP, Ra < 0.5 nm) enables direct fusion and anodic bonding as well as double-sided MEMS patterning. The 525 ± 25 μm thickness provides high flexural rigidity for handling in standard cleanroom cassettes and lithography steppers.
How should these prime-grade silicon wafers be stored and handled to maintain surface quality?
Store wafers sealed inside the original cleanroom polypropylene cassette within a dry nitrogen cabinet or cleanroom desiccator, away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface contact. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), so any wet-chemical processing must follow institutional EHS and SDS safety protocols.
The 4-inch prime CZ P-type <100> silicon wafer with 20–50 Ω·cm resistivity and dual-side CMP finish (Ra < 0.5 nm) is a versatile substrate for double-side lithography, MEMS micromachining, and low-noise photodetector prototyping. Its SEMI M1 geometry and 525 μm thickness ensure compatibility with standard cleanroom handling, though the low doping level and bare surface demand careful oxide control and cleanroom discipline.
Positive
- Low-doping enables wide depletion: Boron-doped to 20–50 Ω·cm (~3×10^14–7×10^14 cm^-3), this substrate widens depletion layers and lowers junction capacitance, benefiting optical/particle photodetectors, PIN photodiodes, and low-noise analog test structures.
- Dual-side CMP for bonding and IR: Double-side mirror-polished surfaces (Ra < 0.5 nm) support double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding without additional surface preparation.
Trade-offs
- Native oxide requires removal: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air; where native oxide removal or RCA clean is required before metallization or epitaxy, wet processing must be performed in an exhaust fume hood or wet bench using facility-approved protocols.
- Cleanroom storage mandatory: Wafers must be stored sealed inside the original cleanroom cassette within a dry nitrogen cabinet to minimize airborne organic contamination; handling requires cleanroom vacuum wands or PTFE/PEEK tweezers by the perimeter edge.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).