4-Inch Prime CZ Silicon Wafer P-Type 300μm DSP ATOMFAIR®

Price range: $239.00 through $519.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Prime-grade 4-inch (100 mm) CZ silicon wafer, P-type boron-doped, 1–10 Ω·cm, , 300 ± 20 μm, DSP Ra < 0.5 nm. SEMI M1 flats. In stock.

Diameter & Flat:
4-Inch (100.0 ± 0.3 mm)
Primary Flat 32.5 mm <110>
Substrate & Dopant:
CZ P-Type / Boron (B)
<100>•1–10 Ω·cm
Thickness:
300 ± 20 μm
Prime-Grade Virgin Wafer
Surface Polish:
DSP (Ra < 0.5 nm)
Dual-Side Mirror-Polished (CMP)

4-Inch (100 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 1–10 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 100.0 ± 0.3 mm diameter and 300 ± 20 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).

Doped with Boron to an industry-standard 1–10 Ω·cm semiconducting resistivity range, the wafer provides a well-characterized majority-hole carrier profile for MOSFET/CMOS device prototyping, Schottky barrier testing, PECVD/ALD dielectric C-V metrology, and general thin-film deposition.

Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.

4-Inch (100 mm) Thickness & Process Compatibility Note: The ultra-responsive 300 ± 20 μm substrate profile enables rapid through-wafer MEMS membrane etching, thinner optical/X-ray paths, and compliant bonded device stacks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Double-Side Polished (DSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)

SEMI M1 4-Inch Dimensional Precision

Standardized 100.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.

  • Diameter: 100.0 ± 0.3 mm (4.0 Inch)
  • Primary Flat: 32.5 ± 2.5 mm along <110> ± 1°
  • Secondary Flat: 18.0 ± 2.0 mm secondary flat located 90° ± 5° clockwise from primary flat (SEMI M1 100 mm P<100>)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant P-Type / Boron (B) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 1–10 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <100> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 100.0 ± 0.3 mm (4-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 300 ± 20 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 32.5 ± 2.5 mm SEMI M1 (100 mm)
Secondary Flat 18.0 ± 2.0 mm secondary flat located 90° ± 5° clockwise from primary flat (SEMI M1 100 mm P<100>) SEMI M1 (100 mm P<100>)
Surface Polish & Roughness Double-Side Polished (DSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Total Thickness Variation (TTV) & Bow/Warp TTV < 3 μm•Bow / Warp < 25 μm Non-Contact Optical Flatness
Surface Particle Inspection ≤ 10 particles / wafer (Cleanroom Audit) Bright-Light & Laser Surface Scan
Available Pack Sizes 10 pcs, 25 pcs cleanroom protective cassettes Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications

  • Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm) supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding;
  • MEMS & Anisotropic Silicon Micromachining: Cleanroom <100> crystal plane supports KOH / TMAH wet anisotropic etching and Bosch deep reactive ion etching (DRIE);
  • Semiconductor Device & Electrode Prototyping: Controlled Boron-doped (1–10 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.

Packaging, Storage & Handling Protocol

Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 4-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters, thicknesses, and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 4-Inch (100 mm), P-Type (100), 1-10 ohm-cm, 300 um, DSP (This Product) 4-Inch (100 mm) / DSP 300 ± 20 μm, P-Type (1–10 Ω·cm) SEMI M1 300 μm 100 mm wafer in 10 pcs / 25 pcs cassettes
4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, P-Type <100> Standard SEMI M1 525 μm 100 mm lithography substrate
4-Inch P-Type <100> Wafer (1–10 Ω·cm, 500 μm SSP) 4-Inch (100 mm) / SSP 500 ± 15 μm, P-Type <100> 500 ± 15 μm precision thickness for MEMS & DRIE etching
4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm DSP) 4-Inch (100 mm) / DSP 525 ± 25 μm, P-Type <100> Double-side CMP polished for IR optics & fusion bonding
4-Inch P-Type <111> Wafer (1–10 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, P-Type <111> Hexagonal <111> lattice for III-nitride epitaxy & UHV growth

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 4-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Prime-grade virgin silicon wafers require particulate-controlled storage and edge-only manipulation to preserve sub-nanometer CMP surface quality. Ambient native oxide growth and anisotropic etch sensitivity impose defined pre-processing and compatibility limits.

  • Particulate and Atmospheric Storage Control: Store wafers sealed in the original cleanroom polypropylene cassette within a dry nitrogen cabinet or desiccator to limit airborne organic contamination and native oxide growth.
  • Edge-Only Manipulation Requirement: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid scratching or contaminating the mirror-polished CMP surfaces.
  • Native Oxide Formation: Bare prime silicon develops an ambient native SiO2 film of approximately 1–2 nm in air, which must be removed by RCA clean or wet processing before metallization or epitaxy.
  • Anisotropic Etch Compatibility: The <100> crystal plane supports KOH and TMAH anisotropic wet etching and Bosch DRIE, but wet-chemical processing must follow institutional EHS and SDS protocols inside an exhaust fume hood or wet bench.
  • Corrosive Vapor Exposure Limit: Avoid exposure to corrosive vapors and particulate dust, which degrade surface cleanliness and compromise lithographic registration and thin-film interface reproducibility.

Sequential solvent degreasing followed by plasma descum prepares DSP prime silicon for photoresist coating or vacuum deposition. Native oxide removal is performed under wet-bench conditions prior to metallization or epitaxial growth.

Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Exhaust fume hood or wet bench, O2 plasma descum system, Dry nitrogen cabinet or cleanroom desiccator

  1. Inspect Cassette and Wafer Edges
    Inspect the cleanroom cassette and wafer edges for particulate contamination or surface contact damage before removing any wafer.
  2. Transfer Wafer by Perimeter Edge
    Transfer the wafer from the cassette using a cleanroom vacuum wand or PTFE/PEEK tweezers applied only to the perimeter edge.
  3. Degrease in Solvent Sequence
    Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and DI water to remove organic residues.
  4. Dry Under Nitrogen
    Dry the wafer with a nitrogen blow-dry to eliminate residual solvent and water before further processing.
  5. Apply Mild O2 Plasma Descum
    Apply a mild O2 plasma descum to remove trace organics prior to photoresist spin coating or PVD/ALD deposition.
  6. Remove Native Oxide Under Wet Bench
    Remove the ambient native SiO2 film by RCA standard clean or wet processing strictly inside an exhaust fume hood or wet bench following facility-approved protocols.
  7. Return Unused Wafers to Nitrogen Storage
    Return unused wafers to the original cleanroom polypropylene cassette box and store sealed within a dry nitrogen cabinet.

What is the difference between DSP and SSP 4-inch silicon wafers for MEMS and bonding applications?

This wafer is double-side polished (DSP) with a CMP finish of Ra < 0.5 nm on both faces, enabling double-sided lithography, through-wafer IR transmission, and direct fusion or anodic bonding. Single-side polished (SSP) alternatives lack the backside mirror finish required for those processes. The DSP surface also supports reproducible thin-film growth and low-defect interfaces.

Can this 300 µm thick P-type <100> wafer be used for KOH anisotropic etching and DRIE?

Yes. The <100> crystal orientation (± 0.5°) supports predictable anisotropic wet-etch V-groove formation in KOH or TMAH solutions, and the 300 ± 20 µm thickness is suitable for through-wafer MEMS membrane etching and Bosch deep reactive ion etching (DRIE). The primary flat is aligned to <110> ± 1° for accurate mask registration.

How should 4-inch prime silicon wafers be stored and handled to maintain surface cleanliness?

Store wafers sealed in the original cleanroom cassette inside a dry nitrogen cabinet or desiccator, away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers. The supplied cleanroom protective cassettes (10 pcs or 25 pcs) immobilize wafer edges to prevent surface contact during transit.

The 4-inch prime CZ P-type <100> silicon wafer with 300 µm thickness and dual-side CMP finish (Ra < 0.5 nm) offers a well-characterized substrate for MEMS membrane etching, double-side lithography, and thin-film metrology, with batch-verified resistivity and flatness. Its thin profile and bare surface demand careful cleanroom handling and prompt native-oxide management to preserve interface quality.

Positive

  • Dual-Side CMP for Bonding and Lithography: Double-side mirror-polished surfaces (Ra < 0.5 nm) enable direct fusion/anodic bonding, double-sided MEMS patterning, and through-wafer IR transmission with minimal surface scattering.
  • Thin 300 µm Profile for Rapid Etching: The 300 ± 20 µm thickness supports faster through-wafer KOH/TMAH or DRIE membrane release and reduces optical/X-ray path length compared to standard 525 µm wafers.

Trade-offs

  • Native Oxide Requires Removal Before Metallization: Bare prime silicon forms a ~1–2 nm ambient native SiO2 film in air; wet-chemical removal (e.g., RCA clean or HF) must be performed in an exhaust fume hood or wet bench following institutional EHS protocols prior to epitaxy or ohmic contact formation.
  • Cleanroom Storage and Handling Mandatory: Wafers must be stored sealed in a dry nitrogen cabinet or cleanroom desiccator and handled only by the perimeter edge with vacuum wands or PTFE/PEEK tweezers to prevent particulate contamination and surface damage.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

10 pcs, 25 pcs

Diameter

4-Inch (100.0 ± 0.3 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

P-Type / Boron (B)

Orientation

± 0.5°

Resistivity

1-10 Ω·cm

Thickness

300 ± 20 μm

Surface Finish

Double-Side Polished (DSP, Ra < 0.5 nm)