4-Inch Prime CZ Silicon Wafer P-Type 525μm ATOMFAIR®

Price range: $189.00 through $389.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Prime-grade 4-inch (100 mm) CZ P-Type/Boron silicon wafer, 100–1000 Ω·cm, 525 ± 25 μm, SSP Ra < 0.5 nm. SEMI M1 flats. In stock.

Diameter & Flat:
4-Inch (100.0 ± 0.3 mm)
Primary Flat 32.5 mm <110>
Substrate & Dopant:
CZ P-Type / Boron (B)
<111>•100–1000 Ω·cm
Thickness:
525 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
SSP (Ra < 0.5 nm)
Polished Front / Fine-Ground Back

4-Inch (100 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 100–1000 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 100.0 ± 0.3 mm diameter and 525 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.

Lightly Boron-doped to 100–1000 Ω·cm, this high-resistivity CZ substrate substantially suppresses free-carrier conductive loss and parasitic capacitance, making it well suited for RF/microwave coplanar waveguides, THz/IR optical windows (especially DSP), photodetectors, and MEMS sensor isolation.

Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D.

4-Inch (100 mm) Thickness & Process Compatibility Note: The industry-standard 525 ± 25 μm mechanical thickness offers high flexural rigidity across full-wafer photolithography steppers, PECVD/LPCVD cassettes, tube oxidation boats, and automated handling chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Single-Side Polished (SSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)

SEMI M1 4-Inch Dimensional Precision

Standardized 100.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.

  • Diameter: 100.0 ± 0.3 mm (4.0 Inch)
  • Primary Flat: 32.5 ± 2.5 mm along <110> ± 1°
  • Secondary Flat: None (SEMI M1 standard for 100 mm P-type <111>)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant P-Type / Boron (B) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 100–1000 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <111> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 100.0 ± 0.3 mm (4-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 525 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 32.5 ± 2.5 mm SEMI M1 (100 mm)
Secondary Flat None (SEMI M1 standard for 100 mm P-type <111>) SEMI M1 (100 mm P<111>)
Surface Polish & Roughness Single-Side Polished (SSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Total Thickness Variation (TTV) & Bow/Warp TTV < 5 μm•Bow / Warp < 30 μm Non-Contact Optical Flatness
Surface Particle Inspection ≤ 10 particles / wafer (Cleanroom Audit) Bright-Light & Laser Surface Scan
Available Pack Sizes 10 pcs, 25 pcs cleanroom protective cassettes Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications

  • Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for PVD sputtering, ALD, e-beam evaporation, and high-resolution photoresist spin coating;
  • Hexagonal Epitaxy & UHV Surface Physics: Dense three-fold <111> crystal lattice supports lattice-matched GaN/AlN/SiC heteroepitaxy, graphene/TMDC template growth, and discrete bipolar/power prototyping;
  • Semiconductor Device & Electrode Prototyping: Controlled Boron-doped (100–1000 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.

Packaging, Storage & Handling Protocol

Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 4-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters, thicknesses, and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 4-Inch (100 mm), P-Type (111), 100-1000 ohm-cm, 525 um, SSP (This Product) 4-Inch (100 mm) / SSP 525 ± 25 μm, P-Type (100–1000 Ω·cm) SEMI M1 525 μm 100 mm wafer in 10 pcs / 25 pcs cassettes
4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, P-Type <100> Standard SEMI M1 525 μm 100 mm lithography substrate
4-Inch P-Type <100> Wafer (1–10 Ω·cm, 500 μm SSP) 4-Inch (100 mm) / SSP 500 ± 15 μm, P-Type <100> 500 ± 15 μm precision thickness for MEMS & DRIE etching
4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm DSP) 4-Inch (100 mm) / DSP 525 ± 25 μm, P-Type <100> Double-side CMP polished for IR optics & fusion bonding
4-Inch P-Type <111> Wafer (1–10 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, P-Type <111> Hexagonal <111> lattice for III-nitride epitaxy & UHV growth

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 4-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Prime-grade virgin silicon wafers require cleanroom-compatible handling to preserve sub-nanometer surface quality and prevent particulate contamination. Storage must occur in dry nitrogen or desiccator environments away from corrosive vapors and airborne organics.

  • Surface Contamination Sensitivity: The CMP-polished front surface (Ra < 0.5 nm) is vulnerable to airborne organic and particulate contamination that degrades thin-film nucleation and lithographic reproducibility.
  • Native Oxide Formation: Bare prime silicon forms a 1–2 nm native SiO2 film in ambient air, requiring controlled wet processing before metallization or epitaxial growth.
  • Edge-Contact Restriction: Direct contact with the polished wafer face must be avoided; handling is restricted to the perimeter edge using vacuum wands or PTFE/PEEK tweezers.
  • Atmospheric Storage Requirement: Unused wafers must remain sealed in the original cleanroom cassette within a dry nitrogen cabinet or desiccator to minimize moisture and organic adsorption.

Proper handling preserves the CMP-polished surface and prevents contamination during semiconductor processing. Sequential solvent cleaning and controlled storage maintain reproducible thin-film interfaces.

Required Equipment: Cleanroom vacuum wand, PTFE/PEEK tweezers, Cleanroom polypropylene cassette, Dry nitrogen cabinet or desiccator

  1. Inspect cassette packaging
    Verify the cleanroom protective cassette is intact and the wafer edges are immobilized without surface contact before opening.
  2. Handle by perimeter edge
    Transfer wafers strictly by the perimeter edge using a cleanroom vacuum wand or PTFE/PEEK tweezers to avoid contacting the polished face.
  3. Perform solvent pre-cleaning
    Degrease wafers sequentially in acetone, electronic-grade isopropanol, and DI water followed by N2 blow-drying.
  4. Apply plasma descum
    Subject the wafer to a mild O2 plasma descum prior to photoresist spin coating or PVD/ALD deposition.
  5. Remove native oxide if required
    Perform wet processing for native oxide removal or RCA standard clean strictly inside an exhaust fume hood or wet bench using facility-approved protocols.
  6. Store unused wafers properly
    Return unused wafers to the original cleanroom polypropylene cassette and seal within a dry nitrogen cabinet to minimize airborne organic contamination.

Why choose a 100–1000 Ω·cm high-resistivity silicon wafer instead of a standard 1–10 Ω·cm wafer?

The 100–1000 Ω·cm Boron-doped resistivity of this CZ wafer substantially suppresses free-carrier conductive loss and parasitic capacitance, which is why it is specified for RF/microwave coplanar waveguides, THz/IR optical windows, photodetectors, and MEMS sensor isolation. Standard 1–10 Ω·cm wafers are optimized for conventional device fabrication and lithography, not for low-loss RF or high-transparency IR paths. If your process requires low parasitic capacitance or high IR transmission, the high-resistivity grade is the correct choice.

Can this <111> P-type wafer be used for GaN or AlN epitaxy, and how does it differ from a <100> wafer?

Yes. The <111> (± 0.5°) orientation provides hexagonal three-fold surface symmetry that supports lattice-matched GaN/AlN/SiC heteroepitaxy and graphene/TMDC template growth. Compared with <100> silicon, the <111> plane also exhibits higher in-plane elastic modulus along key cleavage directions and slower wet alkaline etch kinetics, which is advantageous for III-nitride epitaxy and UHV surface reconstruction studies. If your process is standard CMOS lithography rather than hexagonal epitaxy, a <100> wafer is typically preferred.

What handling and storage precautions are required to preserve the SSP Ra < 0.5 nm surface before thin-film deposition?

Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers, and store unused wafers sealed inside the original cleanroom polypropylene cassette within a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Before photoresist spin coating or PVD/ALD, degrease sequentially in acetone, electronic-grade IPA, and DI water, followed by N2 blow-drying and a mild O2 plasma descum. Note that bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air; remove it via RCA standard clean or wet processing inside an exhaust fume hood or wet bench following institutional EHS and SDS protocols.

The 4-inch P-type <111> CZ silicon wafer with 100–1000 Ω·cm resistivity and 525 μm thickness provides a high-resistivity, crystallographically oriented substrate suited for RF/microwave loss reduction, III-nitride epitaxy, and UHV surface studies. Its prime-grade SSP finish (Ra < 0.5 nm) and SEMI M1 dimensional compliance support reproducible thin-film growth and lithography, though handling requires cleanroom protocols and the native oxide must be managed for critical interfaces.

Positive

  • High-Resistivity Substrate: Boron-doped to 100–1000 Ω·cm, this wafer suppresses free-carrier conductive loss and parasitic capacitance, making it suitable for RF/microwave coplanar waveguides, THz/IR optical windows, and photodetector isolation.
  • <111> Orientation for Epitaxy: The <111> (± 0.5°) crystal plane offers hexagonal three-fold symmetry and slower wet alkaline etch kinetics, supporting lattice-matched GaN/AlN/SiC heteroepitaxy and UHV surface reconstruction studies.

Trade-offs

  • Native Oxide Requires Removal: Bare prime silicon forms a ~1–2 nm native SiO2 film in air; wet processing or RCA clean must be performed in an exhaust fume hood or wet bench following institutional EHS and SDS protocols to ensure proper ohmic contacts or epitaxial interfaces.
  • Cleanroom Handling Mandatory: To preserve the CMP mirror finish (Ra < 0.5 nm) and minimize particle contamination (≤ 10 particles/wafer), wafers must be stored in a dry nitrogen cabinet and handled only by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

10 pcs, 25 pcs

Diameter

4-Inch (100.0 ± 0.3 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

P-Type / Boron (B)

Orientation

± 0.5°

Resistivity

100-1000 Ω·cm

Thickness

525 ± 25 μm

Surface Finish

Single-Side Polished (SSP, Ra < 0.5 nm)