4-Inch Prime CZ Silicon Wafer P-Type 525μm DSP ATOMFAIR®

Price range: $239.00 through $519.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Prime-grade 100 mm CZ P-Type/Boron silicon wafer, 100–1000 Ω·cm, 525 ± 25 μm, DSP Ra < 0.5 nm, SEMI M1 flats. In stock.

Diameter & Flat:
4-Inch (100.0 ± 0.3 mm)
Primary Flat 32.5 mm <110>
Substrate & Dopant:
CZ P-Type / Boron (B)
<100>•100–1000 Ω·cm
Thickness:
525 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
DSP (Ra < 0.5 nm)
Dual-Side Mirror-Polished (CMP)

4-Inch (100 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 100–1000 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 100.0 ± 0.3 mm diameter and 525 ± 25 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).

Lightly Boron-doped to 100–1000 Ω·cm, this high-resistivity CZ substrate substantially suppresses free-carrier conductive loss and parasitic capacitance, making it well suited for RF/microwave coplanar waveguides, THz/IR optical windows (especially DSP), photodetectors, and MEMS sensor isolation.

Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.

4-Inch (100 mm) Thickness & Process Compatibility Note: The industry-standard 525 ± 25 μm mechanical thickness offers high flexural rigidity across full-wafer photolithography steppers, PECVD/LPCVD cassettes, tube oxidation boats, and automated handling chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Double-Side Polished (DSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)

SEMI M1 4-Inch Dimensional Precision

Standardized 100.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.

  • Diameter: 100.0 ± 0.3 mm (4.0 Inch)
  • Primary Flat: 32.5 ± 2.5 mm along <110> ± 1°
  • Secondary Flat: 18.0 ± 2.0 mm secondary flat located 90° ± 5° clockwise from primary flat (SEMI M1 100 mm P<100>)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant P-Type / Boron (B) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 100–1000 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <100> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 100.0 ± 0.3 mm (4-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 525 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 32.5 ± 2.5 mm SEMI M1 (100 mm)
Secondary Flat 18.0 ± 2.0 mm secondary flat located 90° ± 5° clockwise from primary flat (SEMI M1 100 mm P<100>) SEMI M1 (100 mm P<100>)
Surface Polish & Roughness Double-Side Polished (DSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Total Thickness Variation (TTV) & Bow/Warp TTV < 3 μm•Bow / Warp < 25 μm Non-Contact Optical Flatness
Surface Particle Inspection ≤ 10 particles / wafer (Cleanroom Audit) Bright-Light & Laser Surface Scan
Available Pack Sizes 10 pcs, 25 pcs cleanroom protective cassettes Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications

  • Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm) supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding;
  • MEMS & Anisotropic Silicon Micromachining: Cleanroom <100> crystal plane supports KOH / TMAH wet anisotropic etching and Bosch deep reactive ion etching (DRIE);
  • Semiconductor Device & Electrode Prototyping: Controlled Boron-doped (100–1000 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.

Packaging, Storage & Handling Protocol

Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 4-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters, thicknesses, and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 4-Inch (100 mm), P-Type (100), 100-1000 ohm-cm, 525 um, DSP (This Product) 4-Inch (100 mm) / DSP 525 ± 25 μm, P-Type (100–1000 Ω·cm) SEMI M1 525 μm 100 mm wafer in 10 pcs / 25 pcs cassettes
4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, P-Type <100> Standard SEMI M1 525 μm 100 mm lithography substrate
4-Inch P-Type <100> Wafer (1–10 Ω·cm, 500 μm SSP) 4-Inch (100 mm) / SSP 500 ± 15 μm, P-Type <100> 500 ± 15 μm precision thickness for MEMS & DRIE etching
4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm DSP) 4-Inch (100 mm) / DSP 525 ± 25 μm, P-Type <100> Double-side CMP polished for IR optics & fusion bonding
4-Inch P-Type <111> Wafer (1–10 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, P-Type <111> Hexagonal <111> lattice for III-nitride epitaxy & UHV growth

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 4-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Prime-grade monocrystalline silicon wafers require cleanroom-compatible handling to prevent particulate contamination and surface damage. Storage must be in a dry nitrogen cabinet or desiccator to avoid native oxide growth and organic contamination.

  • Particulate and Surface Contamination Control: Handle wafers exclusively by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid scratching the mirror-polished surfaces.
  • Native Oxide Formation: Bare prime silicon forms a 1–2 nm native SiO2 film in ambient air, which must be removed via RCA clean or wet etching before metallization or epitaxy.
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette within a dry nitrogen cabinet to minimize airborne organic contamination.
  • Wet Processing Safety: All wet-chemical processing must be performed in an exhaust fume hood or wet bench following institutional EHS and SDS safety protocols.

Proper handling and pre-cleaning of prime silicon wafers are essential to preserve surface quality and ensure reproducible thin-film interfaces. The following steps outline standard cleanroom procedures for degreasing, native oxide control, and storage.

Required Equipment: Cleanroom vacuum wand, PTFE/PEEK tweezers, Exhaust fume hood or wet bench, Dry nitrogen cabinet

  1. Inspect wafer cassette
    Verify that the cleanroom protective cassette is intact and that wafers are properly seated without edge contact.
  2. Handle wafers by edge
    Transfer wafers using a cleanroom vacuum wand or PTFE/PEEK tweezers, gripping only the perimeter edge.
  3. Degrease wafer surfaces
    Sequentially immerse wafers in acetone, electronic-grade isopropanol, and deionized water, then blow-dry with nitrogen.
  4. Perform plasma descum
    Apply a mild oxygen plasma descum to remove organic residues prior to photoresist spin coating or thin-film deposition.
  5. Remove native oxide if required
    Perform RCA standard clean or wet etching in an exhaust fume hood to remove the native SiO2 layer before metallization or epitaxy.
  6. Store unused wafers
    Seal remaining wafers in the original cleanroom cassette and place them in a dry nitrogen cabinet or desiccator.

What is the resistivity range of this 4-inch P-type silicon wafer and how does it affect RF/microwave device performance?

This wafer is Boron-doped to a verified resistivity of 100–1000 Ω·cm, measured by four-point probe (4PP). This high-resistivity range substantially suppresses free-carrier conductive loss and parasitic capacitance, making the substrate well suited for RF/microwave coplanar waveguides, THz/IR optical windows, and photodetectors. The wide tolerance accommodates applications where exact resistivity matching is less critical than low loss and high isolation.

Can this double-side polished (DSP) 4-inch silicon wafer be used for anodic or fusion bonding without additional surface preparation?

Yes, the dual-side CMP mirror finish with Ra < 0.5 nm is specifically engineered to support direct fusion and anodic bonding. The double-side polish ensures both surfaces are free of subsurface damage and microroughness that would impede intimate wafer-to-wafer contact. However, standard cleanroom pre-cleaning (solvent degrease, IPA, DI rinse, N2 dry, and optional O2 plasma descum) is recommended immediately before bonding to remove airborne organics and native oxide.

What are the storage and handling requirements to maintain the prime-grade surface quality of this 525 μm DSP silicon wafer?

Wafers must be stored sealed inside the original cleanroom protective cassette within a dry nitrogen cabinet or cleanroom desiccator, away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers; never touch the polished faces. The cassette packaging (10 pcs or 25 pcs) immobilizes wafer edges to prevent surface contact during transit and storage.

This 4-inch prime CZ P-type <100> silicon wafer combines a high 100–1000 Ω·cm boron-doped resistivity with dual-side CMP polishing (Ra < 0.5 nm) and SEMI M1 dimensional tolerances, making it a strong substrate choice for RF/microwave coplanar waveguides, THz/IR optical windows, double-side lithography, and fusion bonding. Its 525 ± 25 μm thickness and bare prime surface support direct in-house thermal oxidation, LPCVD nitride growth, and anisotropic KOH/TMAH micromachining, though the high-resistivity bulk and uncoated native oxide demand controlled cleanroom handling and wet-bench processing discipline.

Positive

  • High-Resistivity Low-Loss Substrate: Boron-doped to 100–1000 Ω·cm, the CZ bulk substantially suppresses free-carrier conductive loss and parasitic capacitance, supporting RF/microwave coplanar waveguides, THz/IR optical windows, photodetectors, and MEMS sensor isolation.
  • Dual-Side CMP Mirror Finish: DSP surfaces with Ra < 0.5 nm enable reproducible thin-film growth, double-sided MEMS patterning, through-wafer IR transmission, and direct fusion or anodic bonding without additional surface preparation.
  • SEMI M1 Dimensional Precision: 100.0 ± 0.3 mm diameter, 525 ± 25 μm thickness, TTV < 3 μm, bow/warp < 25 μm, and SEMI M1 flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.
  • <100> Anisotropic Etch Compatibility: The <100> (± 0.5°) orientation provides four-fold rotational symmetry and predictable V-groove formation in KOH/TMAH solutions, supporting anisotropic silicon micromachining and Bosch DRIE processes.

Trade-offs

  • Native Oxide Requires Removal: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air; native oxide removal or RCA standard clean before metallization or epitaxy must be performed in an exhaust fume hood or wet bench under facility-approved EHS and SDS protocols.
  • Strict Cleanroom Storage Required: Unused wafers must remain sealed in the original cleanroom polypropylene cassette within a dry nitrogen cabinet or desiccator to minimize airborne organic contamination and preserve CMP surface quality.
  • Edge-Only Handling Mandate: Wafers must be handled strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers; any surface contact risks contaminating the mirror-polished CMP finish.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

10 pcs, 25 pcs

Diameter

4-Inch (100.0 ± 0.3 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

P-Type / Boron (B)

Orientation

± 0.5°

Resistivity

100-1000 Ω·cm

Thickness

525 ± 25 μm

Surface Finish

Double-Side Polished (DSP, Ra < 0.5 nm)