Prime-grade 4-inch (100 mm) CZ P-type/Boron silicon wafer, 100–1000 Ω·cm, 525 ± 25 μm, DSP Ra < 0.5 nm. SEMI M1 flats. In stock.

Diameter & Flat:
4-Inch (100.0 ± 0.3 mm)
Primary Flat 32.5 mm <110>
Substrate & Dopant:
CZ P-Type / Boron (B)
<111>•100–1000 Ω·cm
Thickness:
525 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
DSP (Ra < 0.5 nm)
Dual-Side Mirror-Polished (CMP)

4-Inch (100 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 100–1000 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 100.0 ± 0.3 mm diameter and 525 ± 25 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).

Lightly Boron-doped to 100–1000 Ω·cm, this high-resistivity CZ substrate substantially suppresses free-carrier conductive loss and parasitic capacitance, making it well suited for RF/microwave coplanar waveguides, THz/IR optical windows (especially DSP), photodetectors, and MEMS sensor isolation.

Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D.

4-Inch (100 mm) Thickness & Process Compatibility Note: The industry-standard 525 ± 25 μm mechanical thickness offers high flexural rigidity across full-wafer photolithography steppers, PECVD/LPCVD cassettes, tube oxidation boats, and automated handling chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Double-Side Polished (DSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)

SEMI M1 4-Inch Dimensional Precision

Standardized 100.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.

  • Diameter: 100.0 ± 0.3 mm (4.0 Inch)
  • Primary Flat: 32.5 ± 2.5 mm along <110> ± 1°
  • Secondary Flat: None (SEMI M1 standard for 100 mm P-type <111>)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant P-Type / Boron (B) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 100–1000 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <111> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 100.0 ± 0.3 mm (4-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 525 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 32.5 ± 2.5 mm SEMI M1 (100 mm)
Secondary Flat None (SEMI M1 standard for 100 mm P-type <111>) SEMI M1 (100 mm P<111>)
Surface Polish & Roughness Double-Side Polished (DSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Total Thickness Variation (TTV) & Bow/Warp TTV < 3 μm•Bow / Warp < 25 μm Non-Contact Optical Flatness
Surface Particle Inspection ≤ 10 particles / wafer (Cleanroom Audit) Bright-Light & Laser Surface Scan
Available Pack Sizes 10 pcs, 25 pcs cleanroom protective cassettes Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications

  • Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm) supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding;
  • Hexagonal Epitaxy & UHV Surface Physics: Dense three-fold <111> crystal lattice supports lattice-matched GaN/AlN/SiC heteroepitaxy, graphene/TMDC template growth, and discrete bipolar/power prototyping;
  • Semiconductor Device & Electrode Prototyping: Controlled Boron-doped (100–1000 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.

Packaging, Storage & Handling Protocol

Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 4-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters, thicknesses, and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 4-Inch (100 mm), P-Type (111), 100-1000 ohm-cm, 525 um, DSP (This Product) 4-Inch (100 mm) / DSP 525 ± 25 μm, P-Type (100–1000 Ω·cm) SEMI M1 525 μm 100 mm wafer in 10 pcs / 25 pcs cassettes
4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, P-Type <100> Standard SEMI M1 525 μm 100 mm lithography substrate
4-Inch P-Type <100> Wafer (1–10 Ω·cm, 500 μm SSP) 4-Inch (100 mm) / SSP 500 ± 15 μm, P-Type <100> 500 ± 15 μm precision thickness for MEMS & DRIE etching
4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm DSP) 4-Inch (100 mm) / DSP 525 ± 25 μm, P-Type <100> Double-side CMP polished for IR optics & fusion bonding
4-Inch P-Type <111> Wafer (1–10 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, P-Type <111> Hexagonal <111> lattice for III-nitride epitaxy & UHV growth

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 4-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Prime-grade virgin silicon wafers require cleanroom-compatible storage and edge-only handling to preserve CMP surface quality. Environmental exposure to particulates, corrosive vapors, and uncontrolled humidity must be avoided to prevent surface contamination and native oxide variability.

  • Atmospheric Storage Control: Store wafers sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.
  • Edge-Only Handling Requirement: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid contact with the polished surface.
  • Native Oxide Sensitivity: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, which must be accounted for prior to metallization or epitaxy.
  • Cassette Immobilization: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box to minimize airborne organic contamination.
  • Wet Processing Containment: Perform wet-chemical processing strictly inside an exhaust fume hood or wet bench using facility-approved EHS and SDS protocols.

Preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs. Follow sequential solvent cleaning, plasma descum, and controlled storage to maintain prime-grade surface quality.

Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Cleanroom polypropylene cassette box, Dry nitrogen cabinet or cleanroom desiccator, Exhaust fume hood or wet bench

  1. Inspect cassette and wafer edges
    Inspect the cleanroom cassette and wafer edges for particulate contamination or physical damage before opening.
  2. Transfer wafer by perimeter edge
    Transfer the wafer using a cleanroom vacuum wand or PTFE/PEEK tweezers applied strictly to the perimeter edge.
  3. Degrease in solvent sequence
    Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and DI water.
  4. Dry with nitrogen
    Dry the wafer with a nitrogen blow-dry to remove residual solvent and water.
  5. Apply mild oxygen plasma descum
    Apply a mild O2 plasma descum prior to photoresist spin coating or PVD/ALD deposition.
  6. Perform wet processing in containment
    Perform any native oxide removal or RCA standard clean strictly inside an exhaust fume hood or wet bench using facility-approved protocols.
  7. Return unused wafers to nitrogen storage
    Return unused wafers to the original cleanroom cassette box and store inside a dry nitrogen cabinet.

Why choose a high-resistivity 100–1000 Ω·cm silicon wafer over standard 1–10 Ω·cm for RF and photonic applications?

The 100–1000 Ω·cm Boron-doped CZ substrate substantially suppresses free-carrier conductive loss and parasitic capacitance, which is critical for RF/microwave coplanar waveguides, THz/IR optical windows, and high-speed photodetectors. Standard 1–10 Ω·cm wafers exhibit higher free-carrier absorption and dielectric loss, degrading signal integrity at high frequencies. This high-resistivity grade is specifically engineered for applications where minimizing substrate-related loss is paramount.

Can this <111> oriented 4-inch wafer be used for GaN or AlN epitaxy, and what are the compatibility constraints?

Yes, the <111> (± 0.5°) crystal orientation provides a hexagonal three-fold surface symmetry that supports lattice-matched III-nitride heteroepitaxy, including GaN, AlN, and SiC. The higher in-plane elastic modulus along key cleavage directions and slower wet alkaline etch kinetics compared to <100> silicon make it suitable for UHV surface reconstruction studies and discrete power/bipolar R&D. However, epitaxial growth requires prior native oxide removal (ambient ~1–2 nm SiO2) via RCA clean or in-situ UHV desorption.

What handling and storage protocols are required to maintain the DSP surface quality of these prime-grade wafers?

Wafers must be stored sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors to preserve the Ra < 0.5 nm CMP finish. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers; never touch the polished faces. The supplied cleanroom protective cassettes (10 pcs or 25 pcs) immobilize wafer edges during transit, but after opening, keep unused wafers in the original cassette box under dry nitrogen.

The 4-inch prime CZ P-type <111> silicon wafer with 100–1000 Ω·cm resistivity and dual-side CMP finish (Ra < 0.5 nm) is engineered for high-resistivity RF/microwave and hexagonal epitaxy applications, offering SEMI M1 dimensional precision and low free-carrier loss. Its operational deployment requires cleanroom handling, dry nitrogen storage, and strict wet-bench protocols to preserve surface quality and manage the native oxide.

Positive

  • High-Resistivity Substrate for RF and THz: Boron-doped to 100–1000 Ω·cm, this wafer suppresses free-carrier conductive loss and parasitic capacitance, making it suitable for RF/microwave coplanar waveguides, THz/IR optical windows, and photodetectors.
  • Dual-Side CMP for Bonding and Lithography: Double-side mirror-polished surfaces with Ra < 0.5 nm enable double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding with reproducible thin-film growth.

Trade-offs

  • Cleanroom Handling and Storage Required: Wafers must be stored in a dry nitrogen cabinet or cleanroom desiccator and handled by the perimeter edge using vacuum wands or PTFE/PEEK tweezers to prevent particulate contamination and surface damage.
  • Native Oxide Requires Wet Processing: Bare prime silicon forms a ~1–2 nm native SiO2 film in air; removal or RCA cleaning before metallization or epitaxy must be performed in an exhaust fume hood or wet bench following institutional EHS and SDS protocols.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

10 pcs, 25 pcs

Diameter

4-Inch (100.0 ± 0.3 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

P-Type / Boron (B)

Orientation

± 0.5°

Resistivity

100-1000 Ω·cm

Thickness

525 ± 25 μm

Surface Finish

Double-Side Polished (DSP, Ra < 0.5 nm)