| Diameter & Flat: 4-Inch (100.0 ± 0.3 mm) Primary Flat 32.5 mm <110> |
Substrate & Dopant: CZ P-Type / Boron (B) <111>•10–20 Ω·cm |
Thickness: 525 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: SSP (Ra < 0.5 nm) Polished Front / Fine-Ground Back |
1. Scientific Overview & Substrate Electrical Properties
4-Inch (100 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 10–20 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 100.0 ± 0.3 mm diameter and 525 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.
Boron-doped to 10–20 Ω·cm (~1015 cm-3 dopant density), this moderate-resistivity substrate minimizes impurity scattering and junction capacitance compared with heavily doped wafers, supporting MOS C-V gate characterization, minority-carrier diffusion studies, and photodiode test structures.
Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D.
4-Inch (100 mm) Thickness & Process Compatibility Note: The industry-standard 525 ± 25 μm mechanical thickness offers high flexural rigidity across full-wafer photolithography steppers, PECVD/LPCVD cassettes, tube oxidation boats, and automated handling chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.
|
SEMI M1 4-Inch Dimensional PrecisionStandardized 100.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | P-Type / Boron (B) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 10–20 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <111> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 100.0 ± 0.3 mm (4-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 525 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Orientation Flat | Location: <110> ± 1°•Length: 32.5 ± 2.5 mm | SEMI M1 (100 mm) |
| Secondary Flat | None (SEMI M1 standard for 100 mm P-type <111>) | SEMI M1 (100 mm P<111>) |
| Surface Polish & Roughness | Single-Side Polished (SSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Total Thickness Variation (TTV) & Bow/Warp | TTV < 5 μm•Bow / Warp < 30 μm | Non-Contact Optical Flatness |
| Surface Particle Inspection | ≤ 10 particles / wafer (Cleanroom Audit) | Bright-Light & Laser Surface Scan |
| Available Pack Sizes | 10 pcs, 25 pcs cleanroom protective cassettes | Cleanroom Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for PVD sputtering, ALD, e-beam evaporation, and high-resolution photoresist spin coating;
- Hexagonal Epitaxy & UHV Surface Physics: Dense three-fold <111> crystal lattice supports lattice-matched GaN/AlN/SiC heteroepitaxy, graphene/TMDC template growth, and discrete bipolar/power prototyping;
- Semiconductor Device & Electrode Prototyping: Controlled Boron-doped (10–20 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
- In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 4-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters, thicknesses, and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 4-Inch (100 mm), P-Type (111), 10-20 ohm-cm, 525 um, SSP (This Product) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, P-Type (10–20 Ω·cm) | SEMI M1 525 μm 100 mm wafer in 10 pcs / 25 pcs cassettes |
| 4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, P-Type <100> | Standard SEMI M1 525 μm 100 mm lithography substrate |
| 4-Inch P-Type <100> Wafer (1–10 Ω·cm, 500 μm SSP) | 4-Inch (100 mm) / SSP | 500 ± 15 μm, P-Type <100> | 500 ± 15 μm precision thickness for MEMS & DRIE etching |
| 4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm DSP) | 4-Inch (100 mm) / DSP | 525 ± 25 μm, P-Type <100> | Double-side CMP polished for IR optics & fusion bonding |
| 4-Inch P-Type <111> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, P-Type <111> | Hexagonal <111> lattice for III-nitride epitaxy & UHV growth |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 4-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade virgin silicon wafers require cleanroom-compatible storage and edge-only handling to preserve CMP surface quality. Ambient native oxide growth and particulate contamination must be controlled prior to lithography, deposition, or thermal processing.
- Storage Atmosphere: Store sealed wafers inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.
- Surface Contact Restriction: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid scratching the polished front surface.
- Native Oxide Sensitivity: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, which must be removed by RCA clean or wet processing before metallization or epitaxy.
- Wet Processing Containment: Perform all wet-chemical cleaning and etching strictly inside an exhaust fume hood or wet bench following institutional EHS and SDS protocols.
- Cassette Immobilization: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box to immobilize edges and prevent surface contact during transit.
Preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs. Follow sequential solvent cleaning, plasma descum, and controlled storage to maintain surface integrity.
Required Equipment: Cleanroom vacuum wand, PTFE/PEEK tweezers, Exhaust fume hood or wet bench, Dry nitrogen cabinet
- Inspect Cassette Seal
Verify the cleanroom polypropylene cassette remains sealed and undamaged before opening in a controlled environment. - Transfer Wafer by Edge
Transfer the wafer using a cleanroom vacuum wand or PTFE/PEEK tweezers applied only to the perimeter edge. - Degrease Sequentially
Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and DI water. - Dry and Descum
Blow-dry with N2 and apply a mild O2 plasma descum prior to photoresist spin coating or PVD/ALD. - Remove Native Oxide
Perform RCA standard clean or wet oxide removal inside an exhaust fume hood when native oxide removal is required before metallization or epitaxy. - Store Unused Wafers
Return unused wafers to the original cassette box and store inside a dry nitrogen cabinet to minimize airborne organic contamination.
Why choose a <111> orientation P-type silicon wafer over <100> for epitaxy or device prototyping?
The <111> orientation provides a densely packed three-fold surface symmetry that supports lattice-matched III-nitride heteroepitaxy (GaN, AlN, SiC) and UHV surface reconstruction studies, whereas <100> is preferred for standard CMOS lithography. This wafer is Boron-doped to 10–20 Ω·cm and oriented to <111> ± 0.5°, offering higher in-plane elastic modulus along key cleavage directions and slower wet alkaline etch kinetics than <100> silicon. These properties make it suitable for discrete power/bipolar R&D and hexagonal epitaxy, but less ideal for processes optimized for <100> surface chemistry.
What cleanroom handling and storage requirements apply to this 4-inch prime silicon wafer?
Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers, and store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. The wafer is supplied in cleanroom protective cassettes (10 pcs or 25 pcs options) that immobilize edges and prevent surface contact. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), so any wet processing must follow institutional EHS and SDS protocols inside an exhaust fume hood or wet bench.
Can this 525 μm thick SSP wafer be used directly in automated photolithography and tube furnace processes?
Yes, the industry-standard 525 ± 25 μm thickness provides high flexural rigidity compatible with full-wafer photolithography steppers, PECVD/LPCVD cassettes, tube oxidation boats, and automated handling chucks. The single-side polished front surface (Ra < 0.5 nm) ensures uniform nucleation for PVD, ALD, e-beam evaporation, and photoresist spin coating, while the fine-ground back allows direct in-house thermal oxidation or epitaxial growth. Total thickness variation is < 5 μm and bow/warp is < 30 μm, supporting reproducible registration on vacuum chucks and mask aligners.
The 4-inch P-type <111> prime silicon wafer with 10–20 Ω·cm resistivity and 525 μm thickness offers a well-characterized substrate for hexagonal epitaxy, UHV surface studies, and device prototyping, with SEMI M1 dimensional precision and sub-nanometer CMP finish. Its moderate resistivity and <111> orientation support specific applications but require careful handling to preserve surface quality and account for native oxide formation.
Positive
- Moderate Resistivity for Device Fabrication: Boron-doped to 10–20 Ω·cm, this substrate minimizes impurity scattering and junction capacitance compared to heavily doped wafers, supporting MOS C-V characterization, minority-carrier diffusion studies, and photodiode test structures.
- <111> Orientation for Hexagonal Epitaxy: The <111> crystal plane provides hexagonal three-fold surface symmetry and slower wet alkaline etch kinetics, enabling lattice-matched GaN/AlN/SiC heteroepitaxy and UHV surface reconstruction studies.
Trade-offs
- Native Oxide Requires Removal: Bare prime silicon forms a ~1–2 nm native SiO2 film in air; wet processing for native oxide removal or RCA clean must be performed in an exhaust fume hood or wet bench following institutional EHS protocols.
- Cleanroom Handling Mandatory: To preserve the mirror-polished CMP surface (Ra < 0.5 nm), wafers must be stored in dry nitrogen cabinets and handled only by edges with cleanroom vacuum wands or PTFE/PEEK tweezers, requiring controlled cleanroom infrastructure.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).