| Diameter & Flat: 4-Inch (100.0 ± 0.3 mm) Primary Flat 32.5 mm |
Substrate & Dopant: CZ P-Type / Boron (B) <110>•1–10 Ω·cm |
Thickness: 525 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: SSP (Ra < 0.5 nm) Polished Front / Fine-Ground Back |
1. Scientific Overview & Substrate Electrical Properties
4-Inch (100 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 1–10 Ω·cm along the <110> (± 0.5°) crystal orientation. Manufactured to a 100.0 ± 0.3 mm diameter and 525 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.
Doped with Boron to an industry-standard 1–10 Ω·cm semiconducting resistivity range, the wafer provides a well-characterized majority-hole carrier profile for MOSFET/CMOS device prototyping, Schottky barrier testing, PECVD/ALD dielectric C-V metrology, and general thin-film deposition.
Sliced along the high-symmetry <110> (± 0.5°) crystal plane, the substrate exposes two sets of {111} etch-stop planes intersecting perpendicular to the wafer surface (at 70.5° / 109.5° in-plane angles), enabling anisotropic KOH/TMAH wet etching of atomically smooth, near-vertical (∼90°) high-aspect-ratio trench sidewalls as well as enhanced in-plane hole mobility for strained PMOS and FinFET channel R&D.
4-Inch (100 mm) Thickness & Process Compatibility Note: The industry-standard 525 ± 25 μm mechanical thickness offers high flexural rigidity across full-wafer photolithography steppers, PECVD/LPCVD cassettes, tube oxidation boats, and automated handling chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.
|
SEMI M1 4-Inch Dimensional PrecisionStandardized 100.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | P-Type / Boron (B) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 1–10 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <110> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 100.0 ± 0.3 mm (4-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 525 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Orientation Flat | Length: 32.5 ± 2.5 mm•Axis: <111> / <110> flat (lot CoA verified) | SEMI M1 (100 mm) |
| Secondary Flat | Single-flat 100 mm <110> research wafer configuration (flat & crystal axes verified per lot CoA) | SEMI M1 (100 mm <110>) |
| Surface Polish & Roughness | Single-Side Polished (SSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Total Thickness Variation (TTV) & Bow/Warp | TTV < 5 μm•Bow / Warp < 30 μm | Non-Contact Optical Flatness |
| Surface Particle Inspection | ≤ 10 particles / wafer (Cleanroom Audit) | Bright-Light & Laser Surface Scan |
| Available Pack Sizes | 10 pcs, 25 pcs cleanroom protective cassettes | Cleanroom Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for PVD sputtering, ALD, e-beam evaporation, and high-resolution photoresist spin coating;
- Vertical-Sidewall MEMS & High Hole-Mobility Devices: Perpendicular {111} etch-stop planes in <110> silicon enable vertical high-aspect-ratio KOH/TMAH microchannels, microfluidic trenches, and high hole-mobility PMOS/FinFET studies;
- Semiconductor Device & Electrode Prototyping: Controlled Boron-doped (1–10 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
- In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 4-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters, thicknesses, and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 4-Inch (100 mm), P-Type (110), 1-10 ohm-cm, 525 um, SSP (This Product) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, P-Type (1–10 Ω·cm) | SEMI M1 525 μm 100 mm wafer in 10 pcs / 25 pcs cassettes |
| 4-Inch N-Type <100> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, N-Type <100> | Standard SEMI M1 525 μm 100 mm N-type lithography substrate |
| 4-Inch N-Type <100> Wafer (1–10 Ω·cm, 525 μm DSP) | 4-Inch (100 mm) / DSP | 525 ± 25 μm, N-Type <100> | Double-side CMP polished N-type wafer for IR optics & wafer bonding |
| 4-Inch N-Type <111> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, N-Type <111> | Hexagonal <111> N-type substrate for III-nitride epitaxy & UHV growth |
| 4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, P-Type <100> | Complementary Boron-doped P-type <100> 100 mm reference substrate |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 4-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade virgin silicon wafers require particulate-controlled storage and edge-only handling to preserve the CMP mirror finish. Ambient native oxide growth and surface contamination must be managed before any deposition or lithography step.
- Particulate and Vapor Exposure: Store wafers sealed in the original cleanroom cassette inside a dry nitrogen cabinet or desiccator away from particulate dust and corrosive vapors.
- Surface Contact Restriction: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid scratching the polished front surface.
- Native Oxide Formation: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air that must be removed by RCA clean or wet processing before metallization or epitaxy.
- Wet-Chemical Processing Safety: Perform all wet-chemical or cleanroom processing strictly inside an exhaust fume hood or wet bench following institutional EHS and SDS safety protocols.
Preserve the CMP mirror finish and reproducible thin-film interfaces by following a controlled pre-cleaning and handling sequence. Each step minimizes particulate contamination and native oxide interference prior to deposition or lithography.
Required Equipment: Cleanroom vacuum wand, PTFE/PEEK tweezers, Cleanroom polypropylene cassette, Dry nitrogen cabinet
- Inspect cassette and wafer edges
Inspect the cleanroom cassette and wafer edges for particulate contamination before opening the sealed container. - Transfer wafer by perimeter edge
Transfer the wafer using a cleanroom vacuum wand or PTFE/PEEK tweezers applied only to the perimeter edge. - Degrease in solvent sequence
Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and DI water followed by N2 blow-drying. - Apply mild O2 plasma descum
Apply a mild O2 plasma descum to remove residual organics prior to photoresist spin coating or PVD/ALD. - Remove native oxide if required
Remove the ambient 1–2 nm native SiO2 film by RCA standard clean or wet processing inside an exhaust fume hood when metallization or epitaxy is planned. - Return unused wafers to storage
Return unused wafers to the original cleanroom polypropylene cassette box and store inside a dry nitrogen cabinet.
Why choose a <110> silicon wafer over <100> for KOH/TMAH anisotropic etching?
The <110> orientation exposes two sets of {111} etch-stop planes that intersect perpendicular to the wafer surface, enabling anisotropic KOH/TMAH wet etching of near-vertical (~90°) high-aspect-ratio trench sidewalls. In contrast, <100> silicon produces sloped {111} sidewalls at 54.7°. This makes the <110> substrate suitable for vertical-sidewall MEMS microchannels and microfluidic trenches, as stated in the product description.
What are the handling and storage requirements for these 4-inch prime silicon wafers?
Wafers are supplied in cleanroom protective cassettes (10 pcs or 25 pcs) that immobilize the wafer edges and prevent surface contact. Store them sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to preserve the Ra < 0.5 nm polished front surface.
What surface preparation is needed before photoresist spin coating or PVD/ALD on these SSP wafers?
Perform solvent pre-cleaning by sequential degreasing in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and a mild O2 plasma descum. The bare prime silicon carries only a thin ambient native oxide (~1–2 nm); if native oxide removal or RCA clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols and institutional EHS/SDS safety guidelines.
The 4-inch P-type <110> prime CZ silicon wafer with 1–10 Ω·cm boron doping and SSP finish (Ra < 0.5 nm) is a well-characterized substrate for anisotropic KOH/TMAH micromachining, high hole-mobility device studies, and thin-film metrology. Its 525 μm thickness and SEMI M1 flats ensure compatibility with standard cleanroom handling, though the <110> orientation and single-side polish impose specific process constraints.
Positive
- Anisotropic Etch-Stop Planes: The <110> crystal orientation exposes two sets of {111} planes perpendicular to the surface, enabling KOH/TMAH wet etching of near-vertical (~90°) high-aspect-ratio trenches and microfluidic channels.
- CMP Mirror Surface for Thin Films: Single-side polished front with Ra < 0.5 nm ensures uniform nucleation for ALD, PVD, and high-resolution photoresist spin coating, supporting reproducible thin-film growth and lithography.
Trade-offs
- Single-Side Polish Limits Backside Processes: The fine-ground back surface is not polished, which may restrict processes requiring double-side alignment or backside lithography; users needing DSP must select an alternative product.
- Native Oxide Requires Removal: Bare prime silicon forms a ~1–2 nm native SiO2 film in ambient air, necessitating wet-chemical or plasma cleaning before metallization or epitaxy to ensure ohmic interfaces.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).