| Diameter & Flat: 4-Inch (100.0 ± 0.3 mm) Primary Flat 32.5 mm |
Substrate & Dopant: CZ P-Type / Boron (B) <110>•0.001–0.005 Ω·cm |
Thickness: 525 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: SSP (Ra < 0.5 nm) Polished Front / Fine-Ground Back |
1. Scientific Overview & Substrate Electrical Properties
4-Inch (100 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 0.001–0.005 Ω·cm along the <110> (± 0.5°) crystal orientation. Manufactured to a 100.0 ± 0.3 mm diameter and 525 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.
Degenerately Boron-doped to 0.001–0.005 Ω·cm (P++) (~1019–1020 cm-3 hole concentration), the wafer provides metallic-like bulk conductivity suitable for low-resistance ohmic contacts, cryogenic back-gated 2D FETs, electrochemical electrodes, and high-power epitaxy.
Sliced along the high-symmetry <110> (± 0.5°) crystal plane, the substrate exposes two sets of {111} etch-stop planes intersecting perpendicular to the wafer surface (at 70.5° / 109.5° in-plane angles), enabling anisotropic KOH/TMAH wet etching of atomically smooth, near-vertical (∼90°) high-aspect-ratio trench sidewalls as well as enhanced in-plane hole mobility for strained PMOS and FinFET channel R&D.
4-Inch (100 mm) Thickness & Process Compatibility Note: The industry-standard 525 ± 25 μm mechanical thickness offers high flexural rigidity across full-wafer photolithography steppers, PECVD/LPCVD cassettes, tube oxidation boats, and automated handling chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.
|
SEMI M1 4-Inch Dimensional PrecisionStandardized 100.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | P-Type / Boron (B) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 0.001–0.005 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <110> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 100.0 ± 0.3 mm (4-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 525 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Orientation Flat | Length: 32.5 ± 2.5 mm•Axis: <111> / <110> flat (lot CoA verified) | SEMI M1 (100 mm) |
| Secondary Flat | Single-flat 100 mm <110> research wafer configuration (flat & crystal axes verified per lot CoA) | SEMI M1 (100 mm <110>) |
| Surface Polish & Roughness | Single-Side Polished (SSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Total Thickness Variation (TTV) & Bow/Warp | TTV < 5 μm•Bow / Warp < 30 μm | Non-Contact Optical Flatness |
| Surface Particle Inspection | ≤ 10 particles / wafer (Cleanroom Audit) | Bright-Light & Laser Surface Scan |
| Available Pack Sizes | 10 pcs, 25 pcs cleanroom protective cassettes | Cleanroom Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for PVD sputtering, ALD, e-beam evaporation, and high-resolution photoresist spin coating;
- Vertical-Sidewall MEMS & High Hole-Mobility Devices: Perpendicular {111} etch-stop planes in <110> silicon enable vertical high-aspect-ratio KOH/TMAH microchannels, microfluidic trenches, and high hole-mobility PMOS/FinFET studies;
- Semiconductor Device & Electrode Prototyping: Controlled Boron-doped (0.001–0.005 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
- In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 4-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters, thicknesses, and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 4-Inch (100 mm), P-Type (110), 0.001-0.005 ohm-cm, 525 um, SSP (This Product) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, P-Type (0.001–0.005 Ω·cm) | SEMI M1 525 μm 100 mm wafer in 10 pcs / 25 pcs cassettes |
| 4-Inch N-Type <100> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, N-Type <100> | Standard SEMI M1 525 μm 100 mm N-type lithography substrate |
| 4-Inch N-Type <100> Wafer (1–10 Ω·cm, 525 μm DSP) | 4-Inch (100 mm) / DSP | 525 ± 25 μm, N-Type <100> | Double-side CMP polished N-type wafer for IR optics & wafer bonding |
| 4-Inch N-Type <111> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, N-Type <111> | Hexagonal <111> N-type substrate for III-nitride epitaxy & UHV growth |
| 4-Inch P-Type <110> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, P-Type <110> | Vertical-sidewall KOH MEMS & high hole-mobility <110> lattice |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 4-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Bare prime silicon forms a native oxide layer in ambient air that must be controlled before critical metallization or epitaxy. Particulate and organic contamination degrade the CMP-polished surface and compromise thin-film nucleation.
- Native Oxide Formation: Bare prime silicon develops an ambient native SiO2 film of approximately 1–2 nm in air, requiring wet-chemical removal before ohmic contact formation or epitaxial growth.
- Particulate Contamination Control: Airborne particles and organic vapors degrade the mirror-polished surface, necessitating storage in a dry nitrogen cabinet or cleanroom desiccator.
- Edge-Contact Handling Requirement: Direct surface contact must be avoided; wafers require handling strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
- Wet-Chemical Processing Safety: All wet-chemical or cleanroom processing must follow institutional EHS and SDS safety protocols within an exhaust fume hood or wet bench.
Proper pre-cleaning and handling preserve the CMP-polished surface and ensure reproducible thin-film interfaces. Sequential solvent cleaning followed by plasma descum removes organic contamination prior to deposition or lithography.
Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Exhaust fume hood or wet bench, O2 plasma descum system, Dry nitrogen cabinet or cleanroom desiccator
- Inspect wafer packaging
Verify the cleanroom cassette seal is intact and inspect wafers for visible particulate contamination under bright light before opening. - Transfer wafer by edge
Transfer the wafer from the cassette using a cleanroom vacuum wand or PTFE/PEEK tweezers, contacting only the perimeter edge. - Degrease in solvent sequence
Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and DI water within an exhaust fume hood or wet bench. - Dry and descum surface
Blow-dry the wafer with N2 and apply a mild O2 plasma descum prior to photoresist spin coating or PVD/ALD deposition. - Remove native oxide if required
Perform RCA standard clean or native oxide removal inside an exhaust fume hood using facility-approved protocols when metallization or epitaxy demands an oxide-free interface. - Store unused wafers
Return unused wafers to the original cleanroom polypropylene cassette and store sealed within a dry nitrogen cabinet to minimize airborne organic contamination.
Why does this 4-inch silicon wafer use <110> crystal orientation instead of the standard <100>?
The <110> orientation is selected specifically for anisotropic KOH/TMAH wet etching and enhanced hole mobility. In <110> silicon, two sets of {111} etch-stop planes intersect perpendicular to the wafer surface at 70.5° / 109.5° in-plane angles, enabling atomically smooth, near-vertical (~90°) high-aspect-ratio trench sidewalls for MEMS and microfluidic structures. The same lattice orientation also provides enhanced in-plane hole mobility for strained PMOS and FinFET channel R&D, which is not achievable on standard <100> substrates.
Can this P++ boron-doped wafer (0.001–0.005 Ω·cm) be used directly for thermal oxidation or epitaxial growth?
Yes. The wafer is supplied as bare prime silicon with only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth without any coating removal step. The degenerately boron-doped bulk (~10^19–10^20 cm^-3 hole concentration) provides metallic-like conductivity suitable for low-resistance ohmic contacts and high-power epitaxy. For native oxide removal or RCA standard clean before metallization, wet processing must be performed in an exhaust fume hood or wet bench following institutional EHS and SDS protocols.
What cleanroom handling and storage requirements apply to these SSP prime silicon wafers?
Wafers must be handled strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to preserve the Ra < 0.5 nm CMP-polished front surface. Store unused wafers sealed inside the original cleanroom polypropylene cassette within a dry nitrogen cabinet or cleanroom desiccator, away from particulate dust and corrosive vapors. The 525 ± 25 μm thickness provides high flexural rigidity for compatibility with photolithography steppers, PECVD/LPCVD cassettes, tube oxidation boats, and automated handling chucks.
The 4-inch P-type <110> prime CZ silicon wafer with degenerate boron doping (0.001–0.005 Ω·cm) and SSP finish (Ra < 0.5 nm) is purpose-built for vertical-sidewall KOH/TMAH MEMS, high hole-mobility device studies, and low-resistance ohmic contact prototyping. Its 525 μm thickness and SEMI M1 flats ensure compatibility with standard cleanroom handling, though the bare surface and <110> orientation impose strict storage and process-specific constraints.
Positive
- Degenerate doping enables ohmic contacts: Boron-doped to 0.001–0.005 Ω·cm (P++), providing metallic-like bulk conductivity for low-resistance ohmic contacts, electrochemical electrodes, and cryogenic back-gated 2D FETs.
- <110> orientation for vertical etch profiles: The <110> crystal plane exposes perpendicular {111} etch-stop planes, enabling anisotropic KOH/TMAH wet etching of near-vertical (~90°) high-aspect-ratio trenches and enhanced in-plane hole mobility for strained PMOS/FinFET R&D.
Trade-offs
- Bare surface requires immediate processing: The wafer carries only a thin ambient native oxide (~1–2 nm) and no protective coating; it must be stored in a dry nitrogen cabinet or cleanroom desiccator and processed promptly to avoid contamination or uncontrolled oxide growth.
- <110> orientation limits standard processes: The <110> crystal orientation is non-standard for many CMOS and epitaxy processes optimized for <100>; users must verify compatibility with their specific lithography, oxidation, and thin-film growth recipes.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).