4-Inch N-Type Antimony Silicon Wafer 525μm ATOMFAIR®

Price range: $199.00 through $419.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Prime CZ N-Type Sb silicon wafer, 100mm, 525μm, 0.005–0.02 Ω·cm, SSP Ra<0.5nm. SEMI M1 flats. In stock.

Diameter & Flat:
4-Inch (100.0 ± 0.3 mm)
Primary Flat 32.5 mm <110>
Substrate & Dopant:
CZ N-Type / Antimony (Sb)
<111>•0.005–0.02 Ω·cm
Thickness:
525 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
SSP (Ra < 0.5 nm)
Polished Front / Fine-Ground Back

4-Inch (100 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Antimony-doped to a verified resistivity of 0.005–0.02 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 100.0 ± 0.3 mm diameter and 525 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.

Heavily Antimony (Sb)-doped to 0.005–0.02 Ω·cm (N+) (~1.5×1018–1.2×1019 cm-3 donor concentration), Antimony exhibits very low solid-state diffusivity and exceptionally low vapor-phase out-diffusion (“autodoping”) during elevated-temperature LPCVD and epitaxial processes. It serves as an industry-standard low-resistance base for abrupt silicon epitaxy, trench power MOSFETs, discrete Schottky barriers, and buried-layer R&D.

Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D.

4-Inch (100 mm) Thickness & Process Compatibility Note: The industry-standard 525 ± 25 μm mechanical thickness offers high flexural rigidity across full-wafer photolithography steppers, PECVD/LPCVD cassettes, epitaxial susceptors, and automated handling chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Single-Side Polished (SSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)

SEMI M1 4-Inch Dimensional Precision

Standardized 100.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.

  • Diameter: 100.0 ± 0.3 mm (4.0 Inch)
  • Primary Flat: 32.5 ± 2.5 mm along <110> ± 1°
  • Secondary Flat: 18.0 ± 2.0 mm secondary flat located 45° ± 5° clockwise from primary flat (SEMI M1 100 mm N<111>)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant N-Type / Antimony (Sb) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 0.005–0.02 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <111> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 100.0 ± 0.3 mm (4-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 525 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 32.5 ± 2.5 mm SEMI M1 (100 mm)
Secondary Flat 18.0 ± 2.0 mm secondary flat located 45° ± 5° clockwise from primary flat (SEMI M1 100 mm N<111>) SEMI M1 (100 mm N<111>)
Surface Polish & Roughness Single-Side Polished (SSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Total Thickness Variation (TTV) & Bow/Warp TTV < 5 μm•Bow / Warp < 30 μm Non-Contact Optical Flatness
Surface Particle Inspection ≤ 10 particles / wafer (Cleanroom Audit) Bright-Light & Laser Surface Scan
Available Pack Sizes 10 pcs, 25 pcs cleanroom protective cassettes Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications

  • Thin-Film Deposition & Epitaxial Growth: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures clean, defect-free nucleation for Si/SiGe/III-V epitaxy, ALD, PVD sputtering, and high-resolution photolithography;
  • Hexagonal Epitaxy & UHV Surface Physics: Dense three-fold <111> crystal lattice supports lattice-matched GaN/AlN/SiC heteroepitaxy, graphene/TMDC template growth, and discrete power/bipolar prototyping;
  • Semiconductor Device & Epitaxial Prototyping: Controlled Antimony-doped (0.005–0.02 Ω·cm) base for ohmic contacts, power/RF devices, epitaxial growth, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.

Packaging, Storage & Handling Protocol

Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 4-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters, dopants, and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 4-Inch (100 mm), N-Type Antimony (111), 0.005-0.02 ohm-cm, 525 um, SSP (This Product) 4-Inch (100 mm) / SSP 525 ± 25 μm, N-Type Antimony (0.005–0.02 Ω·cm) SEMI M1 525 μm 100 mm wafer in 10 pcs / 25 pcs cassettes
4-Inch N-Type Arsenic <100> Wafer (0.001–0.005 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, N++ As <100> Low-strain, low-diffusivity As-doped epi & MOSFET substrate
4-Inch N-Type Antimony <100> Wafer (0.005–0.02 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, N+ Sb <100> Minimal autodoping Sb-doped wafer for sharp high-T epitaxy
4-Inch N-Type <110> Wafer (1–10 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, N-Type <110> Vertical-sidewall KOH MEMS & <110> lattice transport wafer
4-Inch N-Type <111> High-Res Wafer (100–1000 Ω·cm, 525 μm SSP) 4-Inch (100 mm) / SSP 525 ± 25 μm, High-Res N <111> High-resistivity hexagonal <111> wafer for RF & III-nitride epi

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 4-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Prime-grade monocrystalline silicon wafers require cleanroom-compatible handling to preserve the CMP-polished surface and prevent particulate or metallic contamination. Storage must be maintained in a dry nitrogen atmosphere or cleanroom desiccator to inhibit native oxide growth and airborne organic deposition.

  • Surface Contamination Sensitivity: The Ra < 0.5 nm polished front surface is vulnerable to particulate deposition and organic contamination, which degrade epitaxial nucleation and lithographic registration.
  • Native Oxide Formation: Bare prime silicon spontaneously forms a 1–2 nm native SiO2 layer upon ambient air exposure, requiring controlled removal before metallization or epitaxial processing.
  • Edge-Handling Requirement: Direct contact with the wafer face must be avoided; handling is restricted to the perimeter edge using vacuum wands or PTFE/PEEK tweezers.
  • Atmospheric Storage Control: Unused wafers must remain sealed in the original cleanroom cassette within a dry nitrogen cabinet or desiccator to minimize moisture and organic uptake.
  • Wet-Chemical Safety Compliance: All RCA cleaning, native oxide removal, and wet etching must be performed in an exhaust fume hood or wet bench under institutional EHS and SDS protocols.

Proper handling preserves the CMP-polished surface and prevents contamination that compromises epitaxial growth and device yield. Sequential solvent cleaning, plasma descum, and controlled storage are required before thin-film deposition or lithography.

Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Cleanroom polypropylene cassette, Dry nitrogen cabinet or cleanroom desiccator, Exhaust fume hood or wet bench

  1. Inspect Cassette and Wafer Edges
    Inspect the cleanroom cassette and wafer perimeter for particulate contamination or edge damage before removing any substrate.
  2. Transfer Wafer by Edge
    Transfer the wafer using a cleanroom vacuum wand or PTFE/PEEK tweezers applied strictly to the perimeter edge.
  3. Degrease in Solvent Sequence
    Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and DI water to remove organic residues.
  4. Dry and Descum Surface
    Dry the wafer with filtered N2 and apply a mild O2 plasma descum prior to photoresist spin coating or PVD/ALD.
  5. Remove Native Oxide if Required
    Perform RCA standard clean or native oxide removal inside an exhaust fume hood or wet bench under facility-approved EHS protocols when metallization or epitaxy demands an oxide-free interface.
  6. Store Unused Wafers Under Nitrogen
    Return unused wafers to the original cleanroom cassette and store sealed within a dry nitrogen cabinet or desiccator.

Why choose antimony-doped <111> silicon wafers over arsenic-doped <100> wafers for high-temperature epitaxy?

Antimony (Sb) offers significantly lower solid-state diffusivity and vapor-phase out-diffusion (autodoping) than arsenic, making it ideal for abrupt interfaces in high-temperature LPCVD and epitaxial processes. This wafer is heavily doped to 0.005–0.02 Ω·cm (N+), providing a low-resistance base while maintaining the <111> orientation that supports hexagonal epitaxy (GaN, AlN, SiC) and UHV surface reconstruction studies. In contrast, arsenic-doped <100> wafers, while having lower strain, may exhibit higher autodoping during elevated-temperature steps.

Can this 4-inch antimony-doped <111> wafer be used for GaN epitaxy without additional buffer layers?

The <111> crystal orientation provides a hexagonal three-fold surface symmetry that is compatible with lattice-matched GaN/AlN/SiC heteroepitaxy, but direct growth without buffer layers may still face challenges due to lattice mismatch and thermal expansion differences. The wafer's mirror-polished front surface (Ra < 0.5 nm) ensures clean nucleation, and its antimony doping (0.005–0.02 Ω·cm) offers a low-resistance base. For optimal results, a nucleation or buffer layer is typically recommended, but the substrate is specifically designed to support III-nitride epitaxy R&D.

What are the storage and handling requirements to maintain the surface quality of these prime-grade silicon wafers?

Store wafers sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors to prevent contamination and native oxide growth beyond the ambient 1–2 nm. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid scratching the mirror-polished surface (Ra < 0.5 nm). The supplied cleanroom protective cassettes (10 pcs or 25 pcs) are engineered to immobilize wafer edges during transit and storage.

The 4-inch prime CZ N-type antimony-doped <111> silicon wafer with 0.005–0.02 Ω·cm resistivity and SSP finish (Ra < 0.5 nm) is engineered for low-autodoping epitaxy and hexagonal III-nitride growth, but its <111> orientation and bare surface demand orientation-specific process tuning and strict cleanroom handling to avoid contamination and native-oxide interference.

Positive

  • Low Autodoping Antimony Dopant: Antimony's low solid-state diffusivity and vapor-phase out-diffusion minimize autodoping during high-temperature LPCVD and epitaxial processes, enabling abrupt doping profiles for power MOSFETs and Schottky barriers.
  • CMP Mirror Surface for Epitaxy: Single-side polished front surface with Ra < 0.5 nm provides a defect-screened, sub-nanometer roughness platform for reproducible thin-film nucleation in ALD, PVD, and high-resolution photolithography.

Trade-offs

  • <111> Orientation Process Constraints: <111> crystal orientation exhibits slower wet alkaline etch kinetics and hexagonal surface symmetry, requiring orientation-specific adjustments in etch recipes and epitaxial growth compared to standard <100> silicon.
  • Bare Surface Native Oxide Formation: Bare prime silicon forms a ~1–2 nm native SiO2 film in ambient air, necessitating RCA clean or native oxide removal before metallization or epitaxy to ensure ohmic interface control.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

10 pcs, 25 pcs

Diameter

4-Inch (100.0 ± 0.3 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

N-Type / Antimony (Sb)

Orientation

± 0.5°

Resistivity

0.005-0.02 Ω·cm

Thickness

525 ± 25 μm

Surface Finish

Single-Side Polished (SSP, Ra < 0.5 nm)