| Diameter & Flat: 4-Inch (100.0 ± 0.3 mm) Primary Flat 32.5 mm <110> |
Substrate & Dopant: CZ N-Type / Phosphorus (P) <100>•0.001–0.005 Ω·cm |
Thickness: 300 ± 20 μm Prime-Grade Virgin Wafer |
Surface Polish: SSP (Ra < 0.5 nm) Polished Front / Fine-Ground Back |
1. Scientific Overview & Substrate Electrical Properties
4-Inch (100 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Phosphorus-doped to a verified resistivity of 0.001–0.005 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 100.0 ± 0.3 mm diameter and 300 ± 20 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.
Degenerately Phosphorus-doped to 0.001–0.005 Ω·cm (N++) (~1019–1020 cm-3 electron density), the wafer delivers metallic-like bulk conductivity for low-resistance backside ohmic contacts, conductive bottom gates, III-V/GaN buffer heteroepitaxy, and high-current device testing.
Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.
4-Inch (100 mm) Thickness & Process Compatibility Note: The ultra-responsive 300 ± 20 μm substrate profile enables rapid through-wafer MEMS membrane etching, thinner optical/X-ray paths, and compliant bonded device stacks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.
|
SEMI M1 4-Inch Dimensional PrecisionStandardized 100.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | N-Type / Phosphorus (P) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 0.001–0.005 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <100> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 100.0 ± 0.3 mm (4-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 300 ± 20 μm | SEMI M1 / Capacitance Gauge |
| Primary Orientation Flat | Location: <110> ± 1°•Length: 32.5 ± 2.5 mm | SEMI M1 (100 mm) |
| Secondary Flat | 18.0 ± 2.0 mm secondary flat located 180° ± 5° from primary flat (SEMI M1 100 mm N<100>) | SEMI M1 (100 mm N<100>) |
| Surface Polish & Roughness | Single-Side Polished (SSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Total Thickness Variation (TTV) & Bow/Warp | TTV < 5 μm•Bow / Warp < 30 μm | Non-Contact Optical Flatness |
| Surface Particle Inspection | ≤ 10 particles / wafer (Cleanroom Audit) | Bright-Light & Laser Surface Scan |
| Available Pack Sizes | 10 pcs, 25 pcs cleanroom protective cassettes | Cleanroom Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for PVD sputtering, ALD, e-beam evaporation, and high-resolution photoresist spin coating;
- MEMS & Anisotropic Silicon Micromachining: Cleanroom <100> crystal plane supports KOH / TMAH wet anisotropic etching and Bosch deep reactive ion etching (DRIE);
- Semiconductor Device & Electrode Prototyping: Controlled Phosphorus-doped (0.001–0.005 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
- In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 4-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters, thicknesses, and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 4-Inch (100 mm), N-Type (100), 0.001-0.005 ohm-cm, 300 um, SSP (This Product) | 4-Inch (100 mm) / SSP | 300 ± 20 μm, N-Type (0.001–0.005 Ω·cm) | SEMI M1 300 μm 100 mm wafer in 10 pcs / 25 pcs cassettes |
| 4-Inch N-Type <100> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, N-Type <100> | Standard SEMI M1 525 μm 100 mm N-type lithography substrate |
| 4-Inch N-Type <100> Wafer (1–10 Ω·cm, 525 μm DSP) | 4-Inch (100 mm) / DSP | 525 ± 25 μm, N-Type <100> | Double-side CMP polished N-type wafer for IR optics & wafer bonding |
| 4-Inch N-Type <111> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, N-Type <111> | Hexagonal <111> N-type substrate for III-nitride epitaxy & UHV growth |
| 4-Inch P-Type <110> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, P-Type <110> | Vertical-sidewall KOH MEMS & high hole-mobility <110> lattice |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 4-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade monocrystalline silicon wafers require particulate-controlled storage and edge-only manipulation to preserve the CMP mirror finish. Ambient native oxide growth and surface contamination must be managed prior to any thin-film or lithographic processing.
- Cleanroom Storage Atmosphere: Store wafers sealed inside the original cleanroom cassette within a dry nitrogen cabinet or desiccator away from particulate dust and corrosive vapors.
- Edge-Only Contact Restriction: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid scratching or contaminating the polished front surface.
- Native Oxide Sensitivity: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, which must be removed by RCA clean or wet processing before metallization or epitaxy.
- Wet-Chemical Processing Safety: Perform all wet-chemical or cleanroom processing strictly inside an exhaust fume hood or wet bench following institutional EHS and SDS safety protocols.
Proper handling preserves the sub-nanometer CMP surface and prevents contamination during device fabrication. Sequential solvent cleaning and native oxide control are required before photoresist spin coating or thin-film deposition.
Required Equipment: Cleanroom vacuum wand, PTFE/PEEK tweezers, Dry nitrogen cabinet, Exhaust fume hood or wet bench
- Inspect cassette and wafer
Inspect the cleanroom cassette and wafer edges for particulate contamination or physical damage before opening. - Transfer wafer by edge
Transfer the wafer from the cassette using a cleanroom vacuum wand or PTFE/PEEK tweezers applied only to the perimeter edge. - Degrease sequentially
Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and DI water. - Dry and descum
Dry the wafer with N2 blow-drying and apply a mild O2 plasma descum prior to photoresist spin coating or PVD/ALD. - Remove native oxide if required
Perform RCA standard clean or native oxide removal inside an exhaust fume hood or wet bench using facility-approved protocols when metallization or epitaxy is planned. - Return unused wafers to storage
Return unused wafers to the original cleanroom polypropylene cassette box and store within a dry nitrogen cabinet.
What is the resistivity of this 4-inch N-type silicon wafer and why does it matter for ohmic contacts?
This wafer is Phosphorus-doped to a verified resistivity of 0.001–0.005 Ω·cm (N++), corresponding to an electron density of approximately 10^19–10^20 cm^-3. This degenerate doping level provides metallic-like bulk conductivity, which is essential for forming low-resistance backside ohmic contacts, conductive bottom gates, and high-current device testing. The resistivity is measured by four-point probe (4PP) and documented on the Certificate of Analysis.
Can this 300 µm thick 4-inch silicon wafer be used for KOH anisotropic etching and MEMS membrane fabrication?
Yes. The <100> crystal orientation (± 0.5°) supports predictable anisotropic wet-etch V-groove formation in KOH or TMAH solutions, and the 300 ± 20 µm thickness enables rapid through-wafer MEMS membrane etching. The wafer is also compatible with Bosch deep reactive ion etching (DRIE) for high-aspect-ratio structures. For best results, use standard cleanroom masking and follow institutional EHS protocols for wet chemical processing.
How should I store and handle these prime-grade silicon wafers to maintain surface cleanliness?
Store wafers sealed inside the original cleanroom polypropylene cassette within a dry nitrogen cabinet or cleanroom desiccator, away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid contaminating the mirror-polished front surface (Ra < 0.5 nm). The wafers are shipped in cleanroom protective cassettes (10 pcs or 25 pcs options) that immobilize edges and prevent surface contact during transit.
This 4-inch prime CZ N-type silicon wafer combines degenerate phosphorus doping (0.001–0.005 Ω·cm) with a 300 μm thin profile and SSP finish, enabling low-resistance ohmic contacts and rapid through-wafer etching. Its <100> orientation and SEMI M1 flats ensure compatibility with standard cleanroom lithography and anisotropic KOH/TMAH micromachining.
Positive
- Degenerate N++ Doping for Ohmic Contacts: Phosphorus-doped to 0.001–0.005 Ω·cm (~10^19–10^20 cm^-3), providing metallic-like bulk conductivity ideal for low-resistance backside ohmic contacts, conductive bottom gates, and high-current device testing.
- Thin 300 μm Profile for Rapid Etching: The 300 ± 20 μm thickness enables faster through-wafer MEMS membrane etching and shorter optical/X-ray paths compared to standard 525 μm wafers, while maintaining TTV < 5 μm and bow/warp < 30 μm.
Trade-offs
- Native Oxide Requires Removal: Bare prime silicon forms a ~1–2 nm ambient native SiO2 film, necessitating wet-chemical removal (e.g., RCA clean or HF dip) before metallization or epitaxy to ensure reproducible ohmic interfaces.
- Cleanroom Handling and Storage Mandatory: Wafers must be stored in a dry nitrogen cabinet or desiccator and handled only by the perimeter edge with vacuum wands or PTFE/PEEK tweezers to prevent particulate contamination and surface damage.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).