| Diameter & Flat: 3-Inch (76.2 ± 0.25 mm) Primary Flat 22.22 mm <110> |
Substrate & Dopant: CZ P-Type / Boron (B) <100>•10–20 Ω·cm |
Thickness: 380 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: SSP (Ra < 0.5 nm) Polished Front / Fine-Ground Back |
1. Scientific Overview & Substrate Electrical Properties
3-Inch (76.2 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 10–20 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 76.2 ± 0.25 mm diameter and 380 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.
Boron-doped to 10–20 Ω·cm (~1015 cm-3 dopant density), this moderate-resistivity substrate minimizes impurity scattering and junction capacitance compared with heavily doped wafers, supporting MOS C-V gate characterization, minority-carrier diffusion studies, and photodiode test structures.
Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.
3-Inch Chamber Compatibility & Surface State Note: The 3-inch (76.2 mm) format delivers ~2.25× the usable patterning area of a 2-inch wafer while fitting standard 3-inch mask aligners, PECVD/ALD platens, tube/RTA furnaces, and multi-die sputtering chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.
|
SEMI M1 3-Inch Dimensional PrecisionStandardized 76.2 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | P-Type / Boron (B) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 10–20 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <100> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 76.2 ± 0.25 mm (3-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 380 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Orientation Flat | Location: <110> ± 1°•Length: 22.22 ± 3.17 mm | SEMI M1 (76.2 mm) |
| Secondary Flat | 11.18 ± 1.52 mm secondary flat located 90° ± 5° clockwise from primary flat (SEMI M1 76.2 mm P<100>) | SEMI M1 (76.2 mm P<100>) |
| Surface Polish & Roughness | Single-Side Polished (SSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Pack Size (MOQ) | 25 pcs (1 × 25-wafer cleanroom cassette, 25BX) | Cleanroom Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for PVD sputtering, ALD, e-beam evaporation, and high-resolution photoresist spin coating;
- MEMS & Anisotropic Silicon Micromachining: Cleanroom <100> crystal plane supports KOH / TMAH wet anisotropic etching and Bosch deep reactive ion etching (DRIE);
- Semiconductor Device & Electrode Prototyping: Controlled Boron-doped (10–20 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
- In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in a standard 25-wafer protective cleanroom cassette (25 pcs pack, 25BX) engineered to immobilize 3-inch wafer edges and prevent surface contact during transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 3-Inch (76.2 mm), P-Type (100), 10-20 ohm-cm, 380 um, SSP (This Product) | 3-Inch (76.2 mm) / SSP | 380 ± 25 μm, P-Type (10–20 Ω·cm) | SEMI M1 380 μm thickness, 25 pcs cassette for 3-inch R&D tools |
| 3-Inch P-Type <100> Wafer (1–10 Ω·cm SSP) | 3-Inch (76.2 mm) / SSP | 380 ± 25 μm, P-Type <100> | Standard 76.2 mm P<100> bare lithography substrate |
| 3-Inch P-Type <100> Wafer (1–10 Ω·cm DSP) | 3-Inch (76.2 mm) / DSP | 380 ± 25 μm, P-Type <100> | Double-side CMP polished for IR optics & wafer bonding |
| 3-Inch N-Type <100> Wafer (1–10 Ω·cm SSP) | 3-Inch (76.2 mm) / SSP | 380 ± 25 μm, N-Type <100> | Phosphorus-doped N<100> substrate for Schottky & diode R&D |
| 3-Inch P-Type <111> Wafer (1–10 Ω·cm SSP) | 3-Inch (76.2 mm) / SSP | 380 ± 25 μm, P-Type <111> | Hexagonal <111> lattice for III-nitride & UHV growth |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 3-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original 25-wafer polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade monocrystalline silicon wafers require particulate-controlled storage and edge-only manipulation to preserve the CMP mirror finish. Ambient native oxide growth and surface contamination must be managed prior to any thin-film or lithographic processing.
- Particulate and Vapor Isolation: Store wafers sealed in the original cleanroom cassette within a dry nitrogen cabinet or desiccator away from particulate dust and corrosive vapors.
- Edge-Only Contact Restriction: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid scratching or contaminating the polished front surface.
- Native Oxide Formation: Bare prime silicon develops an ambient native SiO2 film of approximately 1–2 nm in air, which must be removed by RCA clean or wet processing before metallization or epitaxy.
- Wet-Chemical Processing Containment: All wet-chemical or cleanroom processing must be performed inside an exhaust fume hood or wet bench following institutional EHS and SDS safety protocols.
Proper pre-cleaning and handling preserve the sub-nanometer CMP surface and ensure reproducible thin-film interfaces. Sequential solvent degreasing followed by plasma descum removes organic contamination prior to deposition or lithography.
Required Equipment: Cleanroom vacuum wand, PTFE/PEEK tweezers, O2 plasma descum system, Dry nitrogen cabinet
- Inspect Cassette Seal
Verify the 25-wafer cleanroom cassette remains sealed and undamaged before opening in a controlled environment. - Transfer by Edge
Transfer wafers individually using a cleanroom vacuum wand or PTFE/PEEK tweezers contacting only the perimeter edge. - Degrease Sequentially
Degrease wafers sequentially in acetone, electronic-grade isopropanol, and DI water to remove organic surface contamination. - Dry with Nitrogen
Blow-dry the wafer surface with filtered N2 to eliminate residual solvent and water droplets. - Descum by Plasma
Apply a mild O2 plasma descum to remove residual organics prior to photoresist spin coating or PVD/ALD deposition. - Return to Storage
Return unused wafers to the original polypropylene cassette box and store within a dry nitrogen cabinet.
What is the resistivity and dopant specification of this 3-inch P-type silicon wafer, and how does it affect MOS C-V characterization?
This wafer is Boron-doped P-type with a verified resistivity of 10–20 Ω·cm, corresponding to approximately 10^15 cm^-3 dopant density, measured by four-point probe (4PP). This moderate resistivity minimizes impurity scattering and junction capacitance compared with heavily doped wafers, making it suitable for MOS C-V gate characterization, minority-carrier diffusion studies, and photodiode test structures. The <100> (± 0.5°) orientation further provides low Si/SiO2 interface state density for reproducible gate stack measurements.
Can this 3-inch SSP wafer be used for KOH or TMAH anisotropic wet etching in MEMS fabrication?
Yes. The <100> (± 0.5°) crystal orientation supports predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions, as well as Bosch deep reactive ion etching (DRIE) for MEMS micromachining. The cubic <100> surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes. Note that all wet-chemical processing must follow institutional EHS and SDS safety protocols inside an exhaust fume hood or wet bench.
How should these bare prime silicon wafers be stored and handled to preserve the Ra < 0.5 nm CMP surface?
Wafers ship in a standard 25-wafer protective cleanroom cassette (25BX) that immobilizes edges and prevents surface contact during transit. Store unused wafers sealed inside the original polypropylene cassette box within a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers; bare prime silicon carries only a thin ambient native oxide (~1–2 nm), so any solvent pre-cleaning (acetone, IPA, DI water) followed by N2 blow-drying and mild O2 plasma descum should precede photoresist spin coating or PVD/ALD.
The 3-inch prime CZ P-type <100> silicon wafer with 10–20 Ω·cm resistivity and SSP finish (Ra < 0.5 nm) offers a balanced substrate for thin-film deposition, MEMS micromachining, and device prototyping, with SEMI M1 dimensional precision and a 25-wafer cassette. However, its bare surface requires careful native oxide management and cleanroom handling to preserve interface quality.
Positive
- Moderate resistivity reduces parasitic effects: Boron-doped to 10–20 Ω·cm (~10^15 cm^-3), this substrate minimizes impurity scattering and junction capacitance compared to heavily doped wafers, supporting MOS C-V characterization and minority-carrier diffusion studies.
- CMP mirror surface for uniform films: Single-side polished front with Ra < 0.5 nm ensures reproducible nucleation for PVD, ALD, e-beam evaporation, and high-resolution photoresist spin coating.
Trade-offs
- Native oxide requires removal before metallization: Bare prime silicon forms a ~1–2 nm ambient native SiO2 film in air; wet processing or RCA clean must be performed in an exhaust fume hood or wet bench using facility-approved protocols to ensure ohmic interfaces.
- Cleanroom handling mandatory to avoid contamination: Wafers must be stored sealed in a dry nitrogen cabinet or desiccator and handled strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to prevent particulate and organic contamination.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).