3-Inch P-Type Silicon Wafer 0.01-0.1 Ω·cm ATOMFAIR®

$289.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Prime CZ P-Type silicon wafer, 76.2 ± 0.25 mm, 380 ± 25 μm, 0.01–0.1 Ω·cm, SSP Ra < 0.5 nm. SEMI M1 flats, 25 pcs cassette. In stock.

Diameter & Flat:
3-Inch (76.2 ± 0.25 mm)
Primary Flat 22.22 mm <110>
Substrate & Dopant:
CZ P-Type / Boron (B)
<111>•0.01–0.1 Ω·cm
Thickness:
380 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
SSP (Ra < 0.5 nm)
Polished Front / Fine-Ground Back

1. Scientific Overview & Substrate Electrical Properties

3-Inch (76.2 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 0.01–0.1 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 76.2 ± 0.25 mm diameter and 380 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.

Boron-doped to a low-resistivity range of 0.01–0.1 Ω·cm (P+), the wafer provides low bulk series resistance for vertical current conduction, anodic bonding, and electrochemical working electrodes while reducing free-carrier infrared absorption compared with degenerately doped P++ substrates.

Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D.

3-Inch Chamber Compatibility & Surface State Note: The 3-inch (76.2 mm) format delivers ~2.25× the usable patterning area of a 2-inch wafer while fitting standard 3-inch mask aligners, PECVD/ALD platens, tube/RTA furnaces, and multi-die sputtering chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Single-Side Polished (SSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)
SEMI M1 3-Inch Dimensional Precision

Standardized 76.2 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.

  • Diameter: 76.2 ± 0.25 mm (3.0 Inch)
  • Primary Flat: 22.22 ± 3.17 mm along <110> ± 1°
  • Secondary Flat: None (SEMI M1 standard for 76.2 mm P-type <111>)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant P-Type / Boron (B) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 0.01–0.1 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <111> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 76.2 ± 0.25 mm (3-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 380 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 22.22 ± 3.17 mm SEMI M1 (76.2 mm)
Secondary Flat None (SEMI M1 standard for 76.2 mm P-type <111>) SEMI M1 (76.2 mm P<111>)
Surface Polish & Roughness Single-Side Polished (SSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Pack Size (MOQ) 25 pcs (1 × 25-wafer cleanroom cassette, 25BX) Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications
  • Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for PVD sputtering, ALD, e-beam evaporation, and high-resolution photoresist spin coating;
  • Hexagonal Epitaxy & UHV Surface Physics: Dense three-fold <111> crystal lattice supports lattice-matched GaN/AlN/SiC heteroepitaxy, graphene/TMDC template growth, and discrete bipolar/power prototyping;
  • Semiconductor Device & Electrode Prototyping: Controlled Boron-doped (0.01–0.1 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol

Wafers are supplied in a standard 25-wafer protective cleanroom cassette (25 pcs pack, 25BX) engineered to immobilize 3-inch wafer edges and prevent surface contact during transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 3-Inch (76.2 mm), P-Type (111), 0.01-0.1 ohm-cm, 380 um, SSP (This Product) 3-Inch (76.2 mm) / SSP 380 ± 25 μm, P-Type (0.01–0.1 Ω·cm) SEMI M1 380 μm thickness, 25 pcs cassette for 3-inch R&D tools
3-Inch P-Type <100> Wafer (1–10 Ω·cm SSP) 3-Inch (76.2 mm) / SSP 380 ± 25 μm, P-Type <100> Standard 76.2 mm P<100> bare lithography substrate
3-Inch P-Type <100> Wafer (1–10 Ω·cm DSP) 3-Inch (76.2 mm) / DSP 380 ± 25 μm, P-Type <100> Double-side CMP polished for IR optics & wafer bonding
3-Inch N-Type <100> Wafer (1–10 Ω·cm SSP) 3-Inch (76.2 mm) / SSP 380 ± 25 μm, N-Type <100> Phosphorus-doped N<100> substrate for Schottky & diode R&D
3-Inch P-Type <111> Wafer (1–10 Ω·cm SSP) 3-Inch (76.2 mm) / SSP 380 ± 25 μm, P-Type <111> Hexagonal <111> lattice for III-nitride & UHV growth

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 3-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original 25-wafer polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Bare prime silicon wafers carry a thin ambient native oxide and are sensitive to particulate, organic, and metallic contamination. Storage must occur in a dry nitrogen cabinet or cleanroom desiccator, and handling must be restricted to the wafer perimeter.

  • Native Oxide Formation: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, which must be removed by RCA clean or wet processing before metallization or epitaxy.
  • Particulate and Organic Contamination Control: Unused wafers must remain sealed inside the original 25-wafer polypropylene cassette within a dry nitrogen cabinet to minimize airborne organic contamination.
  • Perimeter-Only Handling: Wafers must be handled strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to preserve the mirror-polished CMP surface.
  • Wet Processing Containment: Wet-chemical processing for native oxide removal or RCA standard clean must be performed inside an exhaust fume hood or wet bench using facility-approved protocols.

Preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs. Follow sequential solvent cleaning, plasma descum, and controlled storage to prevent contamination.

Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Exhaust fume hood or wet bench, Dry nitrogen cabinet or cleanroom desiccator, O2 plasma descum system

  1. Inspect cassette and wafer edges
    Inspect the 25-wafer cleanroom cassette and wafer edges for particulate or damage before opening in a controlled environment.
  2. Handle by perimeter only
    Transfer wafers strictly by the perimeter edge using a cleanroom vacuum wand or PTFE/PEEK tweezers.
  3. Degrease sequentially
    Degrease diced dies or whole 3-inch wafers sequentially in acetone, electronic-grade isopropanol, and DI water.
  4. Blow-dry with nitrogen
    Blow-dry the wafer surface with filtered N2 to remove residual solvent and water.
  5. Perform mild O2 plasma descum
    Apply a mild O2 plasma descum prior to photoresist spin coating or PVD/ALD deposition.
  6. Remove native oxide under containment
    Perform wet processing for native oxide removal or RCA standard clean strictly inside an exhaust fume hood or wet bench using facility-approved protocols.
  7. Store unused wafers sealed
    Keep unused wafers sealed inside the original 25-wafer polypropylene cassette box within a dry nitrogen cabinet.

Why choose a <111> P-type silicon wafer with 0.01–0.1 Ω·cm resistivity instead of a standard <100> wafer for III-nitride epitaxy?

The <111> orientation provides a densely packed three-fold surface symmetry that supports lattice-matched GaN, AlN, and SiC heteroepitaxy, whereas <100> silicon does not offer the same hexagonal template. The 0.01–0.1 Ω·cm boron-doped (P+) bulk lowers series resistance for vertical current conduction and reduces free-carrier infrared absorption compared with degenerately doped P++ substrates. Additionally, <111> silicon exhibits slower wet alkaline etch kinetics than <100>, which can be advantageous for certain device fabrication flows.

Can this 3-inch P-type <111> wafer be used directly in a tube furnace for thermal oxidation without a pre-clean?

Yes, the wafer is a bare prime silicon substrate with only a thin ambient native oxide (~1–2 nm), so it can be loaded directly into a tube furnace for in-house dry or wet thermal oxidation. However, for reproducible results, the source recommends solvent pre-cleaning (acetone, IPA, DI water) and mild O2 plasma descum before critical steps like photoresist spin coating or PVD/ALD. If native oxide removal or RCA clean is required before metallization or epitaxy, perform wet processing in an exhaust fume hood or wet bench following institutional EHS protocols.

What are the storage and handling requirements to maintain the surface quality of this SSP silicon wafer?

Store the wafer sealed inside its original 25-wafer polypropylene cassette within a dry nitrogen cabinet or cleanroom desiccator to minimize airborne organic contamination and particulate dust. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers; never touch the polished front surface. The cassette is engineered to immobilize 3-inch wafer edges and prevent surface contact during transit and storage.

This prime-grade 3-inch CZ P-type <111> silicon wafer combines a low-resistivity 0.01–0.1 Ω·cm boron-doped bulk with a sub-nanometer CMP front surface, making it well-suited for hexagonal III-nitride epitaxy, electrochemical electrode prototyping, and in-house thermal oxidation. Its 380 μm SEMI M1 geometry fits standard 3-inch mask aligners and furnace platens, though the bare native oxide and edge-handling requirements impose strict cleanroom discipline.

Positive

  • Low-Resistivity P+ Bulk Conduction: Boron doping at 0.01–0.1 Ω·cm provides low bulk series resistance for vertical current conduction, anodic bonding, and electrochemical working electrodes while reducing free-carrier IR absorption relative to degenerately doped P++ substrates.
  • Dense <111> Lattice for Hexagonal Epitaxy: The <111> (± 0.5°) orientation offers three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100>, supporting GaN/AlN/SiC heteroepitaxy and UHV surface reconstruction studies.
  • Sub-Nanometer CMP Front Surface: Single-side polished front with Ra < 0.5 nm ensures uniform nucleation for PVD, ALD, e-beam evaporation, and high-resolution photoresist spin coating, with a fine-ground back for handling stability.

Trade-offs

  • Native Oxide Requires Pre-Clean: Bare prime silicon carries an ambient ~1–2 nm native SiO2 film; removal via RCA or wet processing must be performed in an exhaust fume hood or wet bench under facility-approved EHS and SDS protocols before metallization or epitaxy.
  • Strict Cleanroom Edge Handling: Wafers must be handled only by the perimeter edge using vacuum wands or PTFE/PEEK tweezers and stored sealed in a dry nitrogen cabinet or desiccator away from particulate dust and corrosive vapors to preserve CMP cleanliness.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

25 pcs

Diameter

3-Inch (76.2 ± 0.25 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

P-Type / Boron (B)

Orientation

± 0.5°

Resistivity

0.01-0.1 Ω·cm

Thickness

380 ± 25 μm

Surface Finish

Single-Side Polished (SSP, Ra < 0.5 nm)