| Diameter & Flat: 3-Inch (76.2 ± 0.25 mm) Primary Flat 22.22 mm <110> |
Substrate & Dopant: CZ P-Type / Boron (B) <111>•0.01–0.1 Ω·cm |
Thickness: 380 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: DSP (Ra < 0.5 nm) Dual-Side Mirror-Polished (CMP) |
1. Scientific Overview & Substrate Electrical Properties
3-Inch (76.2 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 0.01–0.1 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 76.2 ± 0.25 mm diameter and 380 ± 25 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).
Boron-doped to a low-resistivity range of 0.01–0.1 Ω·cm (P+), the wafer provides low bulk series resistance for vertical current conduction, anodic bonding, and electrochemical working electrodes while reducing free-carrier infrared absorption compared with degenerately doped P++ substrates.
Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D.
3-Inch Chamber Compatibility & Surface State Note: The 3-inch (76.2 mm) format delivers ~2.25× the usable patterning area of a 2-inch wafer while fitting standard 3-inch mask aligners, PECVD/ALD platens, tube/RTA furnaces, and multi-die sputtering chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.
|
SEMI M1 3-Inch Dimensional PrecisionStandardized 76.2 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | P-Type / Boron (B) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 0.01–0.1 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <111> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 76.2 ± 0.25 mm (3-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 380 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Orientation Flat | Location: <110> ± 1°•Length: 22.22 ± 3.17 mm | SEMI M1 (76.2 mm) |
| Secondary Flat | None (SEMI M1 standard for 76.2 mm P-type <111>) | SEMI M1 (76.2 mm P<111>) |
| Surface Polish & Roughness | Double-Side Polished (DSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Pack Size (MOQ) | 25 pcs (1 × 25-wafer cleanroom cassette, 25BX) | Cleanroom Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm) supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding;
- Hexagonal Epitaxy & UHV Surface Physics: Dense three-fold <111> crystal lattice supports lattice-matched GaN/AlN/SiC heteroepitaxy, graphene/TMDC template growth, and discrete bipolar/power prototyping;
- Semiconductor Device & Electrode Prototyping: Controlled Boron-doped (0.01–0.1 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
- In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in a standard 25-wafer protective cleanroom cassette (25 pcs pack, 25BX) engineered to immobilize 3-inch wafer edges and prevent surface contact during transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 3-Inch (76.2 mm), P-Type (111), 0.01-0.1 ohm-cm, 380 um, DSP (This Product) | 3-Inch (76.2 mm) / DSP | 380 ± 25 μm, P-Type (0.01–0.1 Ω·cm) | SEMI M1 380 μm thickness, 25 pcs cassette for 3-inch R&D tools |
| 3-Inch P-Type <100> Wafer (1–10 Ω·cm SSP) | 3-Inch (76.2 mm) / SSP | 380 ± 25 μm, P-Type <100> | Standard 76.2 mm P<100> bare lithography substrate |
| 3-Inch P-Type <100> Wafer (1–10 Ω·cm DSP) | 3-Inch (76.2 mm) / DSP | 380 ± 25 μm, P-Type <100> | Double-side CMP polished for IR optics & wafer bonding |
| 3-Inch N-Type <100> Wafer (1–10 Ω·cm SSP) | 3-Inch (76.2 mm) / SSP | 380 ± 25 μm, N-Type <100> | Phosphorus-doped N<100> substrate for Schottky & diode R&D |
| 3-Inch P-Type <111> Wafer (1–10 Ω·cm SSP) | 3-Inch (76.2 mm) / SSP | 380 ± 25 μm, P-Type <111> | Hexagonal <111> lattice for III-nitride & UHV growth |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 3-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original 25-wafer polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade monocrystalline silicon wafers require cleanroom-compatible storage and handling to preserve surface quality. Environmental exposure to particulates, corrosive vapors, and moisture must be minimized to prevent contamination and native oxide growth.
- Cleanroom Storage Requirements: Store wafers sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.
- Edge-Only Handling Protocol: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface contact.
- Native Oxide Sensitivity: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, requiring controlled wet processing for removal before metallization or epitaxy.
- Wet Processing Safety: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols.
Proper handling and pre-cleaning procedures preserve the mirror-polished CMP surface and ensure reproducible thin-film interfaces. Sequential solvent cleaning and plasma descum are required before photoresist spin coating or PVD/ALD.
Required Equipment: Cleanroom vacuum wand, PTFE/PEEK tweezers, Dry nitrogen cabinet, O2 plasma descum system
- Inspect wafer cassette
Inspect the 25-wafer cleanroom cassette for seal integrity and edge immobilization before opening. - Transfer wafers
Transfer wafers individually using a cleanroom vacuum wand or PTFE/PEEK tweezers, handling only by the perimeter edge. - Degrease surfaces
Degrease diced dies or whole 3-inch wafers sequentially in acetone, electronic-grade isopropanol, and DI water. - Dry wafers
Dry the wafers with a nitrogen blow-dry immediately after the final DI water rinse. - Perform plasma descum
Perform a mild O2 plasma descum prior to photoresist spin coating or PVD/ALD deposition. - Store unused wafers
Store unused wafers sealed inside the original polypropylene cassette box within a dry nitrogen cabinet.
Why choose a <111> orientation P-type silicon wafer with 0.01–0.1 Ω·cm resistivity instead of a standard <100> wafer?
The <111> orientation provides a densely packed three-fold surface symmetry that supports hexagonal epitaxy (GaN, AlN, SiC) and exhibits slower wet alkaline etch kinetics than <100> silicon, which is advantageous for anisotropic etching and UHV surface reconstruction studies. The 0.01–0.1 Ω·cm boron-doped (P+) resistivity lowers bulk series resistance for vertical current conduction and anodic bonding while reducing free-carrier infrared absorption compared to degenerately doped P++ substrates. However, <111> wafers are not a drop-in replacement for <100> in standard CMOS processes, as oxidation rates and interface trap densities differ.
Can this 3-inch DSP wafer be used directly in a 3-inch mask aligner and tube furnace without additional cleaning?
Yes, the 76.2 ± 0.25 mm diameter and SEMI M1 primary flat (22.22 ± 3.17 mm along <110>) ensure compatibility with standard 3-inch mask aligners, PECVD/ALD platens, and tube/RTA furnaces. The wafer is supplied as bare prime silicon with only a thin ambient native oxide (~1–2 nm), so it can be processed directly for thermal oxidation or epitaxy. However, for reproducible thin-film interfaces, a solvent pre-clean (acetone, IPA, DI water) followed by N2 dry and mild O2 plasma descum is recommended to remove airborne organics.
What are the storage and handling requirements to maintain the Ra < 0.5 nm surface of this double-side polished wafer?
Store the wafer sealed inside the original 25-wafer polypropylene cassette within a dry nitrogen cabinet or cleanroom desiccator to minimize airborne organic contamination and particle deposition. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers; never touch the polished faces. The cassette is engineered to immobilize 3-inch wafer edges and prevent surface contact during transit, but once opened, unused wafers should be returned to the cassette and dry storage immediately.
The 3-inch P-type <111> prime CZ silicon wafer with 0.01–0.1 Ω·cm boron doping and dual-side CMP finish (Ra < 0.5 nm) is a well-characterized substrate for hexagonal epitaxy, double-side lithography, and electrochemical electrode prototyping. Its low-resistivity P+ bulk and SEMI M1 dimensional precision support reproducible device R&D, though the 25-piece minimum pack and strict cleanroom handling requirements demand appropriate institutional infrastructure.
Positive
- Low-Resistivity P+ Bulk for Vertical Conduction: Boron-doped to 0.01–0.1 Ω·cm, the substrate provides low bulk series resistance for vertical current conduction, anodic bonding, and electrochemical working electrodes while reducing free-carrier infrared absorption compared with degenerately doped P++ silicon.
- Dual-Side CMP Finish Enables Bonding and IR Optics: Double-side mirror-polished surfaces with Ra < 0.5 nm support double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion or anodic bonding without additional surface preparation.
- <111> Lattice Suits Hexagonal Epitaxy: The densely packed <111> (± 0.5°) crystal plane exhibits hexagonal three-fold surface symmetry and slower wet alkaline etch kinetics than <100> silicon, supporting lattice-matched GaN/AlN/SiC heteroepitaxy and UHV surface reconstruction studies.
Trade-offs
- Native Oxide Requires Pre-Cleaning Before Critical Interfaces: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air; where native oxide removal or RCA standard clean is required before metallization or epitaxy, wet processing must be performed strictly inside an exhaust fume hood or wet bench using facility-approved protocols.
- Strict Cleanroom Storage and Handling Mandatory: Wafers must be stored sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors, and handled strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to preserve the CMP surface.
- 25-Piece Minimum Pack Constrains Small-Batch Use: Supplied only as a 25-wafer cleanroom cassette (25BX), the minimum order quantity may exceed the needs of low-volume exploratory runs and requires appropriate dry storage capacity for unused wafers.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.