| Diameter & Flat: 3-Inch (76.2 ± 0.25 mm) Primary Flat 22.22 mm <110> |
Substrate & Dopant: CZ N-Type / Phosphorus (P) <100>•100–1000 Ω·cm |
Thickness: 380 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: SSP (Ra < 0.5 nm) Polished Front / Fine-Ground Back |
1. Scientific Overview & Substrate Electrical Properties
3-Inch (76.2 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Phosphorus-doped to a verified resistivity of 100–1000 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 76.2 ± 0.25 mm diameter and 380 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.
Lightly Phosphorus-doped to 100–1000 Ω·cm, this high-resistivity n-type CZ substrate suppresses conductive substrate coupling and parasitic RF loss, serving RF/microwave planar circuits, IR/THz transmission windows, radiation/particle detector prototyping, and low-noise MEMS sensors.
Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.
3-Inch Chamber Compatibility & Surface State Note: The 3-inch (76.2 mm) format delivers ~2.25× the usable patterning area of a 2-inch wafer while fitting standard 3-inch mask aligners, PECVD/ALD platens, tube/RTA furnaces, and multi-die sputtering chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.
|
SEMI M1 3-Inch Dimensional PrecisionStandardized 76.2 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | N-Type / Phosphorus (P) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 100–1000 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <100> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 76.2 ± 0.25 mm (3-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 380 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Orientation Flat | Location: <110> ± 1°•Length: 22.22 ± 3.17 mm | SEMI M1 (76.2 mm) |
| Secondary Flat | 11.18 ± 1.52 mm secondary flat located 180° ± 5° from primary flat (SEMI M1 76.2 mm N<100>) | SEMI M1 (76.2 mm N<100>) |
| Surface Polish & Roughness | Single-Side Polished (SSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Pack Size (MOQ) | 25 pcs (1 × 25-wafer cleanroom cassette, 25BX) | Cleanroom Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for PVD sputtering, ALD, e-beam evaporation, and high-resolution photoresist spin coating;
- MEMS & Anisotropic Silicon Micromachining: Cleanroom <100> crystal plane supports KOH / TMAH wet anisotropic etching and Bosch deep reactive ion etching (DRIE);
- Semiconductor Device & Electrode Prototyping: Controlled Phosphorus-doped (100–1000 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
- In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in a standard 25-wafer protective cleanroom cassette (25 pcs pack, 25BX) engineered to immobilize 3-inch wafer edges and prevent surface contact during transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 3-Inch (76.2 mm), N-Type (100), 100-1000 ohm-cm, 380 um, SSP (This Product) | 3-Inch (76.2 mm) / SSP | 380 ± 25 μm, N-Type (100–1000 Ω·cm) | SEMI M1 380 μm thickness, 25 pcs cassette for 3-inch R&D tools |
| 3-Inch P-Type <100> Wafer (1–10 Ω·cm SSP) | 3-Inch (76.2 mm) / SSP | 380 ± 25 μm, P-Type <100> | Standard 76.2 mm P<100> bare lithography substrate |
| 3-Inch P-Type <100> Wafer (1–10 Ω·cm DSP) | 3-Inch (76.2 mm) / DSP | 380 ± 25 μm, P-Type <100> | Double-side CMP polished for IR optics & wafer bonding |
| 3-Inch N-Type <100> Wafer (1–10 Ω·cm SSP) | 3-Inch (76.2 mm) / SSP | 380 ± 25 μm, N-Type <100> | Phosphorus-doped N<100> substrate for Schottky & diode R&D |
| 3-Inch P-Type <111> Wafer (1–10 Ω·cm SSP) | 3-Inch (76.2 mm) / SSP | 380 ± 25 μm, P-Type <111> | Hexagonal <111> lattice for III-nitride & UHV growth |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 3-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original 25-wafer polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade virgin silicon wafers require cleanroom-compatible handling to preserve the CMP-polished surface and prevent particulate or organic contamination. Storage must be maintained in a dry nitrogen cabinet or cleanroom desiccator to minimize native oxide growth and airborne molecular contamination.
- Surface Contamination Control: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid scratching or contaminating the mirror-polished front surface.
- Native Oxide Sensitivity: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, which must be removed via RCA standard clean or wet processing inside an exhaust fume hood or wet bench before metallization or epitaxy.
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original 25-wafer polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
- Wet-Chemical Safety Compliance: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols.
Proper handling and pre-cleaning of prime silicon wafers are essential to preserve surface quality and ensure reproducible thin-film interfaces. The following steps outline solvent cleaning, plasma descum, and safe storage practices for cleanroom processing.
Required Equipment: Cleanroom vacuum wand, PTFE/PEEK tweezers, Exhaust fume hood or wet bench, Dry nitrogen cabinet
- Inspect wafer cassette
Inspect the sealed 25-wafer cleanroom cassette for any signs of damage or contamination before opening. - Handle wafers by edge
Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers. - Degrease wafers
Degrease diced dies or whole 3-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water. - Blow-dry with nitrogen
Blow-dry the wafers with nitrogen gas to remove residual solvents and moisture. - Perform plasma descum
Perform a mild O2 plasma descum prior to photoresist spin coating or PVD/ALD deposition. - Remove native oxide if required
Remove native oxide via RCA standard clean or wet processing inside an exhaust fume hood or wet bench using facility-approved protocols. - Store unused wafers
Store unused wafers sealed inside the original 25-wafer polypropylene cassette box within a dry nitrogen cabinet.
What is the resistivity range of this 3-inch N-type silicon wafer, and how does it affect RF and detector performance?
This wafer is Phosphorus-doped to a verified bulk resistivity of 100–1000 Ω·cm, measured by four-point probe (4PP). The high-resistivity n-type CZ substrate suppresses conductive substrate coupling and parasitic RF loss, making it suitable for RF/microwave planar circuits, IR/THz transmission windows, radiation/particle detector prototyping, and low-noise MEMS sensors. The wide 100–1000 Ω·cm window provides process latitude for device designs that require low background doping.
Can this 3-inch <100> SSP wafer be used for KOH or TMAH anisotropic wet etching and DRIE?
Yes. The wafer is sliced along the <100> (± 0.5°) plane, which exhibits four-fold rotational symmetry and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions. It also supports Bosch deep reactive ion etching (DRIE) for MEMS micromachining. The primary flat is oriented along <110> ± 1° with a length of 22.22 ± 3.17 mm, and the secondary flat is 11.18 ± 1.52 mm located 180° ± 5° from the primary flat per SEMI M1 for 76.2 mm N<100> wafers.
How should these bare prime silicon wafers be stored and handled to preserve the Ra < 0.5 nm CMP surface?
Store unused wafers sealed inside the original 25-wafer polypropylene cleanroom cassette within a dry nitrogen cabinet or cleanroom desiccator, away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid contacting the single-side polished (SSP) front surface. The bare prime silicon carries only a thin ambient native oxide (~1–2 nm), so any wet-chemical cleaning or native oxide removal must follow institutional EHS and SDS protocols inside an exhaust fume hood or wet bench.
The 3-inch N-type <100> CZ silicon wafer with 100–1000 Ω·cm resistivity and SSP finish (Ra < 0.5 nm) is a prime-grade substrate suited for RF/microwave planar circuits, detector prototyping, and MEMS micromachining. Its high resistivity suppresses substrate coupling, while the 380 μm thickness and SEMI M1 flats ensure compatibility with standard 3-inch cleanroom tools.
Positive
- High-Resistivity N-Type Substrate: Phosphorus-doped to 100–1000 Ω·cm, this wafer minimizes conductive substrate coupling and parasitic RF loss, making it ideal for RF/microwave circuits and low-noise MEMS sensors.
- Precision <100> Orientation and Flats: The <100> ± 0.5° crystal orientation with SEMI M1 primary and secondary flats ensures accurate registration on mask aligners and enables predictable anisotropic KOH/TMAH V-groove etching.
Trade-offs
- Native Oxide Requires Removal: Bare prime silicon forms a 1–2 nm native SiO2 layer in ambient air, necessitating wet-chemical or plasma cleaning before metallization or epitaxy to ensure ohmic interfaces.
- Cleanroom Handling Mandatory: To preserve the Ra < 0.5 nm CMP surface, wafers must be stored in a dry nitrogen cabinet and handled only with vacuum wands or PTFE/PEEK tweezers in a cleanroom environment.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).