| Diameter & Flat: 3-Inch (76.2 ± 0.25 mm) Primary Flat 22.22 mm <110> |
Substrate & Dopant: CZ N-Type / Phosphorus (P) <100>•1–10 Ω·cm |
Thickness: 380 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: DSP (Ra < 0.5 nm) Dual-Side Mirror-Polished (CMP) |
1. Scientific Overview & Substrate Electrical Properties
3-Inch (76.2 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Phosphorus-doped to a verified resistivity of 1–10 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 76.2 ± 0.25 mm diameter and 380 ± 25 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).
Doped with Phosphorus to a standard 1–10 Ω·cm n-type semiconducting range, the wafer provides uniform majority-electron transport for Schottky rectifiers, n-channel CMOS/PMOS device R&D, dielectric C-V profiling, and cleanroom thin-film deposition.
Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.
3-Inch Chamber Compatibility & Surface State Note: The 3-inch (76.2 mm) format delivers ~2.25× the usable patterning area of a 2-inch wafer while fitting standard 3-inch mask aligners, PECVD/ALD platens, tube/RTA furnaces, and multi-die sputtering chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.
|
SEMI M1 3-Inch Dimensional PrecisionStandardized 76.2 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | N-Type / Phosphorus (P) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 1–10 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <100> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 76.2 ± 0.25 mm (3-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 380 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Orientation Flat | Location: <110> ± 1°•Length: 22.22 ± 3.17 mm | SEMI M1 (76.2 mm) |
| Secondary Flat | 11.18 ± 1.52 mm secondary flat located 180° ± 5° from primary flat (SEMI M1 76.2 mm N<100>) | SEMI M1 (76.2 mm N<100>) |
| Surface Polish & Roughness | Double-Side Polished (DSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Pack Size (MOQ) | 25 pcs (1 × 25-wafer cleanroom cassette, 25BX) | Cleanroom Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm) supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding;
- MEMS & Anisotropic Silicon Micromachining: Cleanroom <100> crystal plane supports KOH / TMAH wet anisotropic etching and Bosch deep reactive ion etching (DRIE);
- Semiconductor Device & Electrode Prototyping: Controlled Phosphorus-doped (1–10 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
- In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in a standard 25-wafer protective cleanroom cassette (25 pcs pack, 25BX) engineered to immobilize 3-inch wafer edges and prevent surface contact during transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 3-Inch (76.2 mm), N-Type (100), 1-10 ohm-cm, 380 um, DSP (This Product) | 3-Inch (76.2 mm) / DSP | 380 ± 25 μm, N-Type (1–10 Ω·cm) | SEMI M1 380 μm thickness, 25 pcs cassette for 3-inch R&D tools |
| 3-Inch P-Type <100> Wafer (1–10 Ω·cm SSP) | 3-Inch (76.2 mm) / SSP | 380 ± 25 μm, P-Type <100> | Standard 76.2 mm P<100> bare lithography substrate |
| 3-Inch P-Type <100> Wafer (1–10 Ω·cm DSP) | 3-Inch (76.2 mm) / DSP | 380 ± 25 μm, P-Type <100> | Double-side CMP polished for IR optics & wafer bonding |
| 3-Inch N-Type <100> Wafer (1–10 Ω·cm SSP) | 3-Inch (76.2 mm) / SSP | 380 ± 25 μm, N-Type <100> | Phosphorus-doped N<100> substrate for Schottky & diode R&D |
| 3-Inch P-Type <111> Wafer (1–10 Ω·cm SSP) | 3-Inch (76.2 mm) / SSP | 380 ± 25 μm, P-Type <111> | Hexagonal <111> lattice for III-nitride & UHV growth |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 3-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original 25-wafer polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade virgin silicon wafers require particulate-controlled storage and edge-only handling to preserve CMP surface quality. Ambient native oxide growth and contamination risks must be managed during cleanroom processing.
- Cleanroom Storage Environment: Store wafers sealed inside the original 25-wafer polypropylene cassette within a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.
- Edge-Only Handling Requirement: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to prevent surface contact and contamination.
- Native Oxide Formation: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, requiring controlled wet processing for native oxide removal before metallization or epitaxy.
- Wet Processing Safety Protocol: Perform all wet-chemical or cleanroom processing strictly inside an exhaust fume hood or wet bench following institutional EHS and SDS safety protocols.
Proper pre-cleaning and handling procedures preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces. Sequential solvent cleaning followed by plasma descum prepares wafers for photoresist spin coating or PVD/ALD deposition.
Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Exhaust fume hood or wet bench, O2 plasma descum system, Dry nitrogen cabinet
- Inspect wafer cassette
Verify the 25-wafer polypropylene cassette is sealed and stored within a dry nitrogen cabinet before opening. - Transfer wafer by edge
Transfer the wafer using a cleanroom vacuum wand or PTFE/PEEK tweezers contacting only the perimeter edge. - Degrease sequentially
Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and DI water. - Dry with nitrogen
Blow-dry the wafer with N2 to remove residual solvent and moisture. - Apply plasma descum
Apply mild O2 plasma descum prior to photoresist spin coating or PVD/ALD deposition. - Perform wet processing in hood
Perform native oxide removal or RCA standard clean strictly inside an exhaust fume hood or wet bench using facility-approved protocols. - Return unused wafers to storage
Return unused wafers to the original cassette and seal within a dry nitrogen cabinet to minimize airborne organic contamination.
What is the resistivity range and dopant type of this 3-inch N-type silicon wafer?
This wafer is Phosphorus-doped N-type with a verified bulk resistivity of 1–10 Ω·cm, measured by four-point probe (4PP). The controlled doping supports uniform majority-electron transport for Schottky rectifiers, n-channel CMOS/PMOS R&D, and dielectric C-V profiling. The resistivity range is documented on the lot-specific Certificate of Analysis.
Can this 3-inch DSP wafer be used for double-side lithography and wafer bonding?
Yes. The wafer is double-side polished (DSP) via CMP with Ra < 0.5 nm on both surfaces, enabling double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion or anodic bonding. The 76.2 ± 0.25 mm diameter and SEMI M1 flats ensure accurate registration on standard 3-inch mask aligners and bonding chucks.
How should these prime silicon wafers be stored and handled to preserve surface quality?
Store wafers sealed in the original 25-wafer cleanroom cassette inside a dry nitrogen cabinet or desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid contaminating the Ra < 0.5 nm CMP surfaces. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), so keep unused wafers in the cassette until processing.
The 3-inch N-type <100> DSP prime silicon wafer offers a dual-side CMP finish (Ra < 0.5 nm) and SEMI M1 dimensional precision, making it well-suited for double-side lithography, wafer bonding, and MEMS micromachining. However, its bare surface requires immediate native-oxide control and strict cleanroom handling to preserve the sub-nanometer polish.
Positive
- Dual-Side CMP Finish: Double-side polished surfaces with Ra < 0.5 nm enable double-sided lithography, direct fusion bonding, and through-wafer IR transmission.
- SEMI M1 Dimensional Precision: Standardized 76.2 mm diameter and flats ensure accurate registration on 3-inch mask aligners, vacuum chucks, and cleanroom cassettes.
Trade-offs
- Native Oxide Growth: Bare silicon forms a 1–2 nm native oxide in air, requiring wet processing in an exhaust fume hood or wet bench for removal before metallization or epitaxy.
- Cleanroom Handling Requirement: Wafers must be stored in a dry nitrogen cabinet and handled only by the perimeter edge with vacuum wands or PTFE/PEEK tweezers to prevent particulate contamination.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).