3-Inch N-Type Silicon Wafer 100-1000 Ω·cm ATOMFAIR®

$309.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Prime CZ N-Type silicon wafer, 76.2 mm, 380 μm, 100–1000 Ω·cm, SSP Ra<0.5 nm. 25 pcs cassette. In stock.

Diameter & Flat:
3-Inch (76.2 ± 0.25 mm)
Primary Flat 22.22 mm <110>
Substrate & Dopant:
CZ N-Type / Phosphorus (P)
<111>•100–1000 Ω·cm
Thickness:
380 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
SSP (Ra < 0.5 nm)
Polished Front / Fine-Ground Back

1. Scientific Overview & Substrate Electrical Properties

3-Inch (76.2 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Phosphorus-doped to a verified resistivity of 100–1000 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 76.2 ± 0.25 mm diameter and 380 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.

Lightly Phosphorus-doped to 100–1000 Ω·cm, this high-resistivity n-type CZ substrate suppresses conductive substrate coupling and parasitic RF loss, serving RF/microwave planar circuits, IR/THz transmission windows, radiation/particle detector prototyping, and low-noise MEMS sensors.

Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D.

3-Inch Chamber Compatibility & Surface State Note: The 3-inch (76.2 mm) format delivers ~2.25× the usable patterning area of a 2-inch wafer while fitting standard 3-inch mask aligners, PECVD/ALD platens, tube/RTA furnaces, and multi-die sputtering chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Single-Side Polished (SSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)
SEMI M1 3-Inch Dimensional Precision

Standardized 76.2 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.

  • Diameter: 76.2 ± 0.25 mm (3.0 Inch)
  • Primary Flat: 22.22 ± 3.17 mm along <110> ± 1°
  • Secondary Flat: 11.18 ± 1.52 mm secondary flat located 45° ± 5° clockwise from primary flat (SEMI M1 76.2 mm N<111>)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant N-Type / Phosphorus (P) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 100–1000 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <111> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 76.2 ± 0.25 mm (3-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 380 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 22.22 ± 3.17 mm SEMI M1 (76.2 mm)
Secondary Flat 11.18 ± 1.52 mm secondary flat located 45° ± 5° clockwise from primary flat (SEMI M1 76.2 mm N<111>) SEMI M1 (76.2 mm N<111>)
Surface Polish & Roughness Single-Side Polished (SSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Pack Size (MOQ) 25 pcs (1 × 25-wafer cleanroom cassette, 25BX) Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications
  • Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for PVD sputtering, ALD, e-beam evaporation, and high-resolution photoresist spin coating;
  • Hexagonal Epitaxy & UHV Surface Physics: Dense three-fold <111> crystal lattice supports lattice-matched GaN/AlN/SiC heteroepitaxy, graphene/TMDC template growth, and discrete bipolar/power prototyping;
  • Semiconductor Device & Electrode Prototyping: Controlled Phosphorus-doped (100–1000 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol

Wafers are supplied in a standard 25-wafer protective cleanroom cassette (25 pcs pack, 25BX) engineered to immobilize 3-inch wafer edges and prevent surface contact during transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 3-Inch (76.2 mm), N-Type (111), 100-1000 ohm-cm, 380 um, SSP (This Product) 3-Inch (76.2 mm) / SSP 380 ± 25 μm, N-Type (100–1000 Ω·cm) SEMI M1 380 μm thickness, 25 pcs cassette for 3-inch R&D tools
3-Inch P-Type <100> Wafer (1–10 Ω·cm SSP) 3-Inch (76.2 mm) / SSP 380 ± 25 μm, P-Type <100> Standard 76.2 mm P<100> bare lithography substrate
3-Inch P-Type <100> Wafer (1–10 Ω·cm DSP) 3-Inch (76.2 mm) / DSP 380 ± 25 μm, P-Type <100> Double-side CMP polished for IR optics & wafer bonding
3-Inch N-Type <100> Wafer (1–10 Ω·cm SSP) 3-Inch (76.2 mm) / SSP 380 ± 25 μm, N-Type <100> Phosphorus-doped N<100> substrate for Schottky & diode R&D
3-Inch P-Type <111> Wafer (1–10 Ω·cm SSP) 3-Inch (76.2 mm) / SSP 380 ± 25 μm, P-Type <111> Hexagonal <111> lattice for III-nitride & UHV growth

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 3-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original 25-wafer polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Prime-grade virgin silicon substrates require particulate-controlled storage and edge-only manipulation to preserve the CMP mirror finish and prevent surface contamination. Ambient native oxide growth and environmental exposure must be managed to maintain reproducible thin-film and lithography interfaces.

  • Cleanroom Storage Atmosphere: Store wafers sealed inside the original 25-wafer polypropylene cassette within a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.
  • Edge-Only Manipulation: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid contacting the polished front surface.
  • Native Oxide Sensitivity: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, which must be removed by RCA standard clean or wet processing before metallization or epitaxy where an oxide-free interface is required.
  • Wet-Chemical Processing Containment: Perform all wet-chemical or cleanroom processing strictly inside an exhaust fume hood or wet bench following institutional EHS and SDS safety protocols.
  • Organic Contamination Control: Minimize airborne organic contamination by keeping unused wafers sealed in the cassette box when not actively processed.

Sequential solvent degreasing followed by plasma descum prepares the CMP-polished surface for photoresist spin coating or PVD/ALD deposition. Native oxide removal prior to metallization or epitaxy must be performed under facility-approved wet-bench protocols.

Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Exhaust fume hood or wet bench, O2 plasma descum system, Dry nitrogen cabinet or cleanroom desiccator

  1. Inspect wafer surface
    Inspect the wafer under cleanroom lighting for particulate, scratches, or handling marks before processing.
  2. Degrease in solvent sequence
    Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and DI water.
  3. Dry with nitrogen
    Blow-dry the wafer with filtered N2 to remove residual solvent and water.
  4. Apply plasma descum
    Apply a mild O2 plasma descum to remove residual organics prior to photoresist spin coating or PVD/ALD.
  5. Remove native oxide if required
    Perform native oxide removal or RCA standard clean inside an exhaust fume hood or wet bench using facility-approved protocols where an oxide-free interface is required.
  6. Return unused wafers to storage
    Return unused wafers to the original 25-wafer cassette and store inside a dry nitrogen cabinet or cleanroom desiccator.

Why choose a high-resistivity 100–1000 Ω·cm N-type <111> silicon wafer instead of a standard 1–10 Ω·cm substrate?

The 100–1000 Ω·cm Phosphorus-doped CZ substrate is specified to suppress conductive substrate coupling and parasitic RF loss, making it suitable for RF/microwave planar circuits, IR/THz transmission windows, radiation/particle detector prototyping, and low-noise MEMS sensors. Standard 1–10 Ω·cm wafers are optimized for conventional device fabrication, whereas this high-resistivity grade prioritizes low-loss signal transmission and detector-grade isolation. The trade-off is that the lightly doped bulk is not intended as a low-resistance ground plane or backside contact layer.

Can this 3-inch N-type <111> wafer be used directly for GaN or AlN epitaxy without a buffer layer?

The <111> (± 0.5°) orientation provides a hexagonal three-fold surface symmetry that supports III-nitride/hexagonal epitaxy (GaN, AlN, SiC) and UHV surface reconstruction studies. However, the wafer is supplied bare with only a thin ambient native oxide (~1–2 nm) and no epitaxial-ready coating, so lattice mismatch and thermal expansion differences still require an appropriate nucleation or buffer strategy. Direct growth without such engineering is not claimed by the source.

What cleanroom handling and storage conditions are required to preserve the Ra < 0.5 nm SSP surface?

Wafers must be handled strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers, and unused wafers should remain sealed in the original 25-wafer polypropylene cassette inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Pre-cleaning before resist spin coating or PVD/ALD should follow sequential acetone, electronic-grade IPA, and DI water degreasing with N2 blow-drying and mild O2 plasma descum. Any wet-chemical processing, including native oxide removal or RCA clean, must be performed in an exhaust fume hood or wet bench under institutional EHS and SDS protocols.

The 3-inch N-type <111> prime CZ silicon wafer with 100–1000 Ω·cm resistivity and SSP finish (Ra < 0.5 nm) is engineered for high-resistivity RF/detector prototyping and hexagonal epitaxy, but its <111> orientation and high resistivity demand orientation-specific process calibration and contamination control to avoid parasitic leakage.

Positive

  • High-Resistivity N-Type Substrate: Phosphorus-doped to 100–1000 Ω·cm, this wafer suppresses conductive substrate coupling and parasitic RF loss, making it suitable for RF/microwave planar circuits, IR/THz windows, and low-noise MEMS sensors.
  • <111> Orientation for Hexagonal Epitaxy: The <111> (± 0.5°) crystal plane provides hexagonal three-fold surface symmetry and slower wet alkaline etch kinetics, supporting III-nitride (GaN, AlN, SiC) heteroepitaxy and UHV surface reconstruction studies.

Trade-offs

  • <111>-Specific Process Calibration Required: The <111> orientation exhibits different wet etch rates and surface chemistry than <100> silicon, requiring orientation-specific adjustments to cleaning, etching, and epitaxial recipes to avoid process drift.
  • High Resistivity Demands Contamination Control: At 100–1000 Ω·cm, the substrate is highly sensitive to ionic contamination and native oxide growth; handling must be strictly edge-only in a cleanroom environment with dry nitrogen storage to preserve resistivity and surface quality.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

25 pcs

Diameter

3-Inch (76.2 ± 0.25 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

N-Type / Phosphorus (P)

Orientation

± 0.5°

Resistivity

100-1000 Ω·cm

Thickness

380 ± 25 μm

Surface Finish

Single-Side Polished (SSP, Ra < 0.5 nm)