| Diameter & Flat: 2-Inch (50.8 ± 0.2 mm) Primary Flat 15.88 mm <110> |
Substrate & Dopant: CZ P-Type / Boron (B) <100>•0.01–0.1 Ω·cm |
Thickness: 275 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: DSP (Ra < 0.5 nm) Dual-Side Mirror-Polished (CMP) |
1. Scientific Overview & Substrate Electrical Properties
2-Inch (50.8 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 0.01–0.1 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 50.8 ± 0.2 mm diameter and 275 ± 25 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).
Boron-doped to a low-resistivity range of 0.01–0.1 Ω·cm (P+), the wafer provides low bulk series resistance for vertical current conduction, anodic bonding, and electrochemical working electrodes while reducing free-carrier infrared absorption compared with degenerately doped P++ substrates.
Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.
2-Inch Chamber Compatibility & Surface State Note: The compact 2-inch (50.8 mm) footprint fits research-scale tube furnaces, compact ALD/PECVD chambers, R&D spin coaters, and 2-inch sputtering sample holders without dicing waste. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.
|
SEMI M1 2-Inch Dimensional PrecisionStandardized 50.8 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | P-Type / Boron (B) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 0.01–0.1 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <100> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 50.8 ± 0.2 mm (2-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 275 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Orientation Flat | Location: <110> ± 1°•Length: 15.88 ± 1.65 mm | SEMI M1 (50.8 mm) |
| Secondary Flat | Located 90° ± 5° clockwise from primary flat (SEMI M1 50.8 mm P<100>) | SEMI M1 (50.8 mm P<100>) |
| Surface Polish & Roughness | Double-Side Polished (DSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Pack Size (MOQ) | 25 pcs (1 × 25-wafer cleanroom cassette, 25BX) | Cleanroom Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm) supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding;
- MEMS & Anisotropic Silicon Micromachining: Cleanroom <100> crystal plane supports KOH / TMAH wet anisotropic etching and Bosch deep reactive ion etching (DRIE);
- Semiconductor Device & Electrode Prototyping: Controlled Boron-doped (0.01–0.1 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
- In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in a standard 25-wafer protective cleanroom cassette (25 pcs pack, 25BX) engineered to immobilize 2-inch wafer edges and prevent surface contact during transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 2-Inch (50.8 mm), P-Type (100), 0.01-0.1 ohm-cm, 275 um, DSP (This Product) | 2-Inch (50.8 mm) / DSP | 275 ± 25 μm, P-Type (0.01–0.1 Ω·cm) | SEMI M1 275 μm thickness, 25 pcs cassette for 2-inch R&D chambers |
| 2-Inch P-Type <100> Wafer (1–10 Ω·cm SSP) | 2-Inch (50.8 mm) / SSP | 275 ± 25 μm, P-Type <100> | Standard 50.8 mm P<100> bare lithography substrate |
| 2-Inch P-Type <100> Wafer (1–10 Ω·cm DSP) | 2-Inch (50.8 mm) / DSP | 275 ± 25 μm, P-Type <100> | Double-side CMP polished for IR optics & bonding |
| 2-Inch N-Type <100> Wafer (1–10 Ω·cm SSP) | 2-Inch (50.8 mm) / SSP | 275 ± 25 μm, N-Type <100> | Phosphorus-doped N<100> wafer for Schottky & diode R&D |
| 2-Inch P-Type <111> Wafer (1–10 Ω·cm SSP) | 2-Inch (50.8 mm) / SSP | 275 ± 25 μm, P-Type <111> | Hexagonal <111> lattice for III-nitride & UHV growth |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 2-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original 25-wafer polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade virgin silicon wafers require particulate-controlled storage and edge-only contact to preserve CMP surface quality. Ambient native oxide growth and moisture exposure must be managed prior to oxidation, epitaxy, or metallization steps.
- Cleanroom Storage Atmosphere: Store wafers sealed in the original polypropylene cassette inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.
- Edge-Only Contact Restriction: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid scratching the mirror-polished CMP surfaces.
- Native Oxide Sensitivity: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, requiring controlled wet processing before metallization or epitaxial growth.
- Wet-Chemical Processing Safety: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols within an exhaust fume hood or wet bench.
Preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs. Follow sequential solvent cleaning, plasma descum, and controlled storage to maintain prime-grade surface quality.
Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Dry nitrogen cabinet or cleanroom desiccator, Exhaust fume hood or wet bench, O2 plasma descum system
- Inspect cassette packaging
Verify the sealed 25-wafer polypropylene cassette is intact and store unused wafers in a dry nitrogen cabinet to minimize airborne organic contamination. - Handle by perimeter edge
Transfer wafers using cleanroom vacuum wands or PTFE/PEEK tweezers while contacting only the perimeter edge to prevent surface scratches. - Degrease sequentially
Degrease diced dies or whole 2-inch wafers sequentially in acetone, electronic-grade isopropanol, and DI water. - Dry and descum
Blow-dry with N2 and apply a mild O2 plasma descum prior to photoresist spin coating or PVD/ALD deposition. - Remove native oxide under hood
Perform native oxide removal or RCA standard clean strictly inside an exhaust fume hood or wet bench using facility-approved protocols before metallization or epitaxy.
What is the resistivity of this 2-inch P-type silicon wafer and why does the 0.01–0.1 Ω·cm range matter for device prototyping?
This wafer is Boron-doped P-type with a verified bulk resistivity of 0.01–0.1 Ω·cm, measured by four-point probe (4PP). This low-resistivity P+ range provides low bulk series resistance for vertical current conduction, anodic bonding, and electrochemical working electrodes, while reducing free-carrier infrared absorption compared with degenerately doped P++ substrates. The controlled resistivity makes it suitable for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology.
Can this 2-inch <100> DSP wafer be used for KOH anisotropic etching and double-side lithography?
Yes. The <100> (± 0.5°) crystal orientation supports predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions and Bosch deep reactive ion etching (DRIE). The dual-side mirror-polished (DSP) finish with Ra < 0.5 nm enables double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding. The 50.8 ± 0.2 mm diameter and SEMI M1 flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.
How should these prime-grade silicon wafers be stored and handled to preserve the CMP surface?
Store wafers sealed inside the original 25-wafer polypropylene cassette box within a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface contact. For pre-cleaning, degrease sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD.
This prime-grade 2-inch CZ P-type <100> silicon wafer combines a low 0.01–0.1 Ω·cm boron-doped bulk resistivity with dual-side CMP mirror polishing (Ra < 0.5 nm) and SEMI M1 dimensional tolerances, making it well suited to research-scale MEMS, anodic/fusion bonding, and electrochemical electrode prototyping. Its bare, uncoated surface and 25-wafer cassette packaging, however, impose strict cleanroom storage and edge-only handling requirements to preserve the polished interface.
Positive
- Low-Resistivity P+ Bulk Conduction: Boron doping at 0.01–0.1 Ω·cm provides low bulk series resistance for vertical current conduction, anodic bonding, and electrochemical working electrodes while reducing free-carrier IR absorption relative to degenerately doped P++ substrates.
- Dual-Side CMP Mirror Finish: Double-side polished surfaces with Ra < 0.5 nm support double-sided lithography, through-wafer IR transmission, direct fusion/anodic bonding, and reproducible thin-film growth and lithography.
- <100> Plane for Anisotropic Etching: The <100> (± 0.5°) orientation with four-fold symmetry enables predictable KOH/TMAH V-groove formation and Bosch DRIE micromachining, with clean perpendicular cleaving along <110> planes.
- SEMI M1 2-Inch Chamber Fit: Standardized 50.8 ± 0.2 mm diameter and SEMI M1 flats fit research-scale tube furnaces, compact ALD/PECVD chambers, spin coaters, and 2-inch sputtering holders without dicing waste.
Trade-offs
- Bare Surface Requires Cleanroom Handling: Uncoated prime silicon carries only a ~1–2 nm ambient native oxide and must be stored sealed in a dry nitrogen cabinet or desiccator and handled strictly by the perimeter edge with vacuum wands or PTFE/PEEK tweezers to avoid particulate and organic contamination.
- Wet Processing Needs EHS Infrastructure: Native oxide removal, RCA cleans, and KOH/TMAH etching require an exhaust fume hood or wet bench and strict adherence to institutional EHS and SDS protocols, imposing facility-level infrastructure dependencies on the user.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.