| Diameter & Flat: 2-Inch (50.8 ± 0.2 mm) Primary Flat 15.88 mm <110> |
Substrate & Dopant: CZ P-Type / Boron (B) <100>•100–1000 Ω·cm |
Thickness: 275 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: DSP (Ra < 0.5 nm) Dual-Side Mirror-Polished (CMP) |
1. Scientific Overview & Substrate Electrical Properties
2-Inch (50.8 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 100–1000 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 50.8 ± 0.2 mm diameter and 275 ± 25 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).
Lightly Boron-doped to 100–1000 Ω·cm, this high-resistivity CZ substrate substantially suppresses free-carrier conductive loss and parasitic capacitance, making it well suited for RF/microwave coplanar waveguides, THz/IR optical windows (especially DSP), photodetectors, and MEMS sensor isolation.
Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.
2-Inch Chamber Compatibility & Surface State Note: The compact 2-inch (50.8 mm) footprint fits research-scale tube furnaces, compact ALD/PECVD chambers, R&D spin coaters, and 2-inch sputtering sample holders without dicing waste. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.
|
SEMI M1 2-Inch Dimensional PrecisionStandardized 50.8 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | P-Type / Boron (B) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 100–1000 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <100> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 50.8 ± 0.2 mm (2-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 275 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Orientation Flat | Location: <110> ± 1°•Length: 15.88 ± 1.65 mm | SEMI M1 (50.8 mm) |
| Secondary Flat | Located 90° ± 5° clockwise from primary flat (SEMI M1 50.8 mm P<100>) | SEMI M1 (50.8 mm P<100>) |
| Surface Polish & Roughness | Double-Side Polished (DSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Pack Size (MOQ) | 25 pcs (1 × 25-wafer cleanroom cassette, 25BX) | Cleanroom Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm) supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding;
- MEMS & Anisotropic Silicon Micromachining: Cleanroom <100> crystal plane supports KOH / TMAH wet anisotropic etching and Bosch deep reactive ion etching (DRIE);
- Semiconductor Device & Electrode Prototyping: Controlled Boron-doped (100–1000 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
- In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in a standard 25-wafer protective cleanroom cassette (25 pcs pack, 25BX) engineered to immobilize 2-inch wafer edges and prevent surface contact during transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 2-Inch (50.8 mm), P-Type (100), 100-1000 ohm-cm, 275 um, DSP (This Product) | 2-Inch (50.8 mm) / DSP | 275 ± 25 μm, P-Type (100–1000 Ω·cm) | SEMI M1 275 μm thickness, 25 pcs cassette for 2-inch R&D chambers |
| 2-Inch P-Type <100> Wafer (1–10 Ω·cm SSP) | 2-Inch (50.8 mm) / SSP | 275 ± 25 μm, P-Type <100> | Standard 50.8 mm P<100> bare lithography substrate |
| 2-Inch P-Type <100> Wafer (1–10 Ω·cm DSP) | 2-Inch (50.8 mm) / DSP | 275 ± 25 μm, P-Type <100> | Double-side CMP polished for IR optics & bonding |
| 2-Inch N-Type <100> Wafer (1–10 Ω·cm SSP) | 2-Inch (50.8 mm) / SSP | 275 ± 25 μm, N-Type <100> | Phosphorus-doped N<100> wafer for Schottky & diode R&D |
| 2-Inch P-Type <111> Wafer (1–10 Ω·cm SSP) | 2-Inch (50.8 mm) / SSP | 275 ± 25 μm, P-Type <111> | Hexagonal <111> lattice for III-nitride & UHV growth |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 2-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original 25-wafer polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade virgin silicon wafers require cleanroom-compatible handling to preserve sub-nanometer surface quality and prevent particulate or organic contamination. Environmental exposure must be minimized because ambient air forms a native silicon dioxide layer that alters surface chemistry prior to processing.
- Particulate and Organic Contamination Control: Store wafers sealed inside the original polypropylene cassette within a dry nitrogen cabinet or cleanroom desiccator to limit airborne molecular contamination.
- Native Oxide Formation: Bare prime silicon develops a 1–2 nm native silicon dioxide film upon air exposure, which must be removed by RCA clean or wet processing before metallization or epitaxial growth.
- Mechanical Handling Restrictions: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid scratching the dual-side CMP mirror finish.
- Wet-Chemical Processing Safety: Perform all wet-chemical or cleanroom processing inside an exhaust fume hood or wet bench following institutional EHS and SDS safety protocols.
Proper handling and pre-cleaning of prime-grade CZ silicon wafers preserves the CMP mirror finish and ensures reproducible thin-film interfaces. Sequential solvent cleaning followed by plasma descum removes organic residues prior to lithography or deposition.
Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Exhaust fume hood or wet bench, O2 plasma descum system, Dry nitrogen cabinet or cleanroom desiccator
- Inspect wafer cassette
Inspect the sealed 25-wafer cleanroom cassette for physical damage or contamination before opening in a controlled environment. - Transfer wafer by edge
Transfer the wafer from the cassette using a cleanroom vacuum wand or PTFE/PEEK tweezers, contacting only the perimeter edge. - Degrease sequentially
Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and deionized water inside an exhaust fume hood. - Dry with nitrogen
Dry the wafer surface with a filtered nitrogen blow-dry to remove residual solvent and water droplets. - Perform plasma descum
Perform a mild oxygen plasma descum to remove trace organic residues prior to photoresist spin coating or PVD/ALD deposition. - Store unused wafers
Store unused wafers sealed inside the original polypropylene cassette within a dry nitrogen cabinet to minimize airborne organic contamination.
What is the resistivity range of this 2-inch P-type <100> silicon wafer, and how does it affect RF and photodetector performance?
This wafer is Boron-doped to a verified resistivity of 100–1000 Ω·cm, measured by four-point probe (4PP). This high-resistivity range substantially suppresses free-carrier conductive loss and parasitic capacitance, making the substrate well suited for RF/microwave coplanar waveguides, THz/IR optical windows, photodetectors, and MEMS sensor isolation. The lightly doped P-type <100> crystal also provides a controlled base for ohmic contacts, Schottky diodes, and C-V metrology.
Can this double-side polished (DSP) 2-inch silicon wafer be used for wafer bonding and double-sided lithography?
Yes. The wafer features a dual-side mirror-polished CMP finish with Ra < 0.5 nm on both surfaces, which supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion or anodic bonding. The 275 ± 25 μm thickness and SEMI M1 flats ensure accurate registration on vacuum chucks and mask aligners. For optimal bonding, store wafers sealed in the original 25-wafer cassette within a dry nitrogen cabinet to minimize airborne organic contamination.
How should these prime-grade 2-inch silicon wafers be stored and handled to preserve surface quality?
Store wafers sealed inside the original 25-wafer polypropylene cleanroom cassette within a dry nitrogen cabinet or cleanroom desiccator, away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface contact. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm); if native oxide removal or RCA cleaning is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench following institutional EHS and SDS safety protocols.
The 2-inch prime CZ P-type <100> silicon wafer with 100–1000 Ω·cm resistivity and dual-side CMP finish (Ra < 0.5 nm) is engineered for high-frequency and micromachining applications where low conductive loss and precise surface registration are critical. Its 275 μm thickness and SEMI M1 flats ensure compatibility with research-scale chambers, though handling requires cleanroom protocols to preserve the native oxide and mirror surfaces.
Positive
- High-Resistivity Substrate: Boron-doped to 100–1000 Ω·cm, this wafer suppresses free-carrier conductive loss and parasitic capacitance, making it suitable for RF/microwave coplanar waveguides and THz/IR optical windows.
- Dual-Side CMP Finish: Double-side polished with Ra < 0.5 nm enables double-sided lithography, direct fusion bonding, and reproducible thin-film growth for MEMS and photodetector fabrication.
Trade-offs
- Native Oxide Formation: Bare prime silicon forms a ~1–2 nm native SiO2 film in ambient air, requiring wet-chemical removal (e.g., RCA clean) before metallization or epitaxy, which must be performed in an exhaust fume hood.
- Cleanroom Handling Required: To preserve surface cleanliness and prevent particulate contamination, wafers must be stored in a dry nitrogen cabinet and handled only with cleanroom vacuum wands or PTFE/PEEK tweezers.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).