2-Inch P-Type Silicon Wafer 10-20 Ω·cm ATOMFAIR®

$259.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Prime CZ P-Type silicon wafer, 50.8 mm, 275 μm, 10–20 Ω·cm, SSP Ra<0.5 nm. SEMI M1 flats, 25 pcs cassette. In stock.

Diameter & Flat:
2-Inch (50.8 ± 0.2 mm)
Primary Flat 15.88 mm <110>
Substrate & Dopant:
CZ P-Type / Boron (B)
<111>•10–20 Ω·cm
Thickness:
275 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
SSP (Ra < 0.5 nm)
Polished Front / Fine-Ground Back

1. Scientific Overview & Substrate Electrical Properties

2-Inch (50.8 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 10–20 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 50.8 ± 0.2 mm diameter and 275 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.

Boron-doped to 10–20 Ω·cm (~1015 cm-3 dopant density), this moderate-resistivity substrate minimizes impurity scattering and junction capacitance compared with heavily doped wafers, supporting MOS C-V gate characterization, minority-carrier diffusion studies, and photodiode test structures.

Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D.

2-Inch Chamber Compatibility & Surface State Note: The compact 2-inch (50.8 mm) footprint fits research-scale tube furnaces, compact ALD/PECVD chambers, R&D spin coaters, and 2-inch sputtering sample holders without dicing waste. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Single-Side Polished (SSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)
SEMI M1 2-Inch Dimensional Precision

Standardized 50.8 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.

  • Diameter: 50.8 ± 0.2 mm (2.0 Inch)
  • Primary Flat: 15.88 ± 1.65 mm along <110> ± 1°
  • Secondary Flat: None (SEMI M1 standard for 50.8 mm P-type <111>)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant P-Type / Boron (B) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 10–20 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <111> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 50.8 ± 0.2 mm (2-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 275 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 15.88 ± 1.65 mm SEMI M1 (50.8 mm)
Secondary Flat None (SEMI M1 standard for 50.8 mm P-type <111>) SEMI M1 (50.8 mm P<111>)
Surface Polish & Roughness Single-Side Polished (SSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Pack Size (MOQ) 25 pcs (1 × 25-wafer cleanroom cassette, 25BX) Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications
  • Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for PVD sputtering, ALD, e-beam evaporation, and high-resolution photoresist spin coating;
  • Hexagonal Epitaxy & UHV Surface Physics: Dense three-fold <111> crystal lattice supports lattice-matched GaN/AlN/SiC heteroepitaxy, graphene/TMDC template growth, and discrete bipolar/power prototyping;
  • Semiconductor Device & Electrode Prototyping: Controlled Boron-doped (10–20 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol

Wafers are supplied in a standard 25-wafer protective cleanroom cassette (25 pcs pack, 25BX) engineered to immobilize 2-inch wafer edges and prevent surface contact during transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 2-Inch (50.8 mm), P-Type (111), 10-20 ohm-cm, 275 um, SSP (This Product) 2-Inch (50.8 mm) / SSP 275 ± 25 μm, P-Type (10–20 Ω·cm) SEMI M1 275 μm thickness, 25 pcs cassette for 2-inch R&D chambers
2-Inch P-Type <100> Wafer (1–10 Ω·cm SSP) 2-Inch (50.8 mm) / SSP 275 ± 25 μm, P-Type <100> Standard 50.8 mm P<100> bare lithography substrate
2-Inch P-Type <100> Wafer (1–10 Ω·cm DSP) 2-Inch (50.8 mm) / DSP 275 ± 25 μm, P-Type <100> Double-side CMP polished for IR optics & bonding
2-Inch N-Type <100> Wafer (1–10 Ω·cm SSP) 2-Inch (50.8 mm) / SSP 275 ± 25 μm, N-Type <100> Phosphorus-doped N<100> wafer for Schottky & diode R&D
2-Inch P-Type <111> Wafer (1–10 Ω·cm SSP) 2-Inch (50.8 mm) / SSP 275 ± 25 μm, P-Type <111> Hexagonal <111> lattice for III-nitride & UHV growth

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 2-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original 25-wafer polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Bare prime silicon wafers carry a thin ambient native oxide and are sensitive to particulate, organic, and metallic contamination. Storage and processing must be controlled to preserve the CMP mirror finish and reproducible thin-film interfaces.

  • Native Oxide Formation: Bare prime silicon forms an ambient native SiO2 film of approximately 1–2 nm in air, which must be removed before metallization or epitaxy where an oxide-free interface is required.
  • Particulate and Vapor Contamination: Wafers must be stored sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors to prevent surface contamination.
  • Edge-Only Handling Requirement: Wafers must be handled strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid damaging the polished front surface.
  • Wet-Chemical Processing Safety: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols, with native oxide removal and RCA standard cleans performed inside an exhaust fume hood or wet bench.
  • Cassette Storage Integrity: Unused wafers should remain sealed inside the original 25-wafer polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Proper handling and pre-cleaning preserve the CMP mirror finish and ensure reproducible thin-film interfaces. Sequential solvent cleaning, plasma descum, and controlled storage are required before deposition or lithography.

Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Exhaust fume hood or wet bench, O2 plasma descum system, Dry nitrogen cabinet or cleanroom desiccator

  1. Inspect Cassette and Wafer Edges
    Inspect the sealed 25-wafer cleanroom cassette and wafer edges for transit damage or particulate before opening in a controlled environment.
  2. Transfer Wafers by Perimeter Edge
    Transfer wafers strictly by the perimeter edge using a cleanroom vacuum wand or PTFE/PEEK tweezers to avoid contacting the polished front surface.
  3. Degrease in Solvent Sequence
    Degrease whole wafers or diced dies sequentially in acetone, electronic-grade isopropanol, and DI water.
  4. Dry and Plasma Descum
    Blow-dry the wafer with N2 and apply a mild O2 plasma descum prior to photoresist spin coating or PVD/ALD deposition.
  5. Remove Native Oxide Where Required
    Perform native oxide removal or RCA standard clean inside an exhaust fume hood or wet bench using facility-approved protocols before metallization or epitaxy.
  6. Store Unused Wafers Under Nitrogen
    Store unused wafers sealed inside the original polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Why choose a <111> orientation P-type silicon wafer with 10–20 Ω·cm resistivity instead of a standard <100> wafer?

The <111> orientation provides a hexagonal three-fold surface symmetry, a higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon. The 10–20 Ω·cm boron doping (~10^15 cm⁻³) minimizes impurity scattering and junction capacitance compared to heavily doped wafers. This combination supports III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D.

Can this 2-inch P-type <111> silicon wafer be used directly for thermal oxidation or epitaxial growth without additional surface preparation?

Yes, the wafer is a bare prime silicon substrate with a single-side polished (SSP) front surface (Ra < 0.5 nm) and a fine-ground back. It carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth. For critical interfaces, standard solvent pre-cleaning (acetone, IPA, DI water) followed by N2 dry and mild O2 plasma descum is recommended to preserve CMP cleanliness.

What are the storage and handling requirements to maintain the surface quality of these prime-grade 2-inch silicon wafers?

Store wafers sealed inside the original 25-wafer polypropylene cassette within a dry nitrogen cabinet or cleanroom desiccator, away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid contaminating the mirror-polished front surface. The cassette is engineered to immobilize 2-inch wafer edges and prevent surface contact during transit.

The 2-inch P-type <111> prime CZ silicon wafer with 10–20 Ω·cm resistivity and SSP finish (Ra < 0.5 nm) is engineered for hexagonal epitaxy, UHV surface physics, and MOS C-V characterization, offering a moderate-resistivity substrate that minimizes impurity scattering. Its 275 μm thickness and SEMI M1 flats ensure compatibility with research-scale tube furnaces and spin coaters, though the bare surface requires careful native-oxide management and cleanroom handling to preserve interface quality.

Positive

  • Hexagonal <111> Lattice for Epitaxy: The densely packed <111> crystal plane provides three-fold surface symmetry and slower wet alkaline etch kinetics, supporting lattice-matched GaN/AlN/SiC heteroepitaxy and UHV surface reconstruction studies.
  • Moderate Resistivity Reduces Scattering: Boron doping at 10–20 Ω·cm (~10^15 cm^-3) minimizes impurity scattering and junction capacitance compared to heavily doped wafers, enabling sensitive MOS C-V gate characterization and minority-carrier diffusion studies.

Trade-offs

  • Native Oxide Requires Removal: Bare prime silicon forms a 1–2 nm ambient native SiO2 film that must be removed via wet processing or RCA clean before metallization or epitaxy, requiring exhaust fume hoods and facility-approved protocols.
  • Cleanroom Handling Mandatory: To preserve the Ra < 0.5 nm CMP surface, wafers must be stored in a dry nitrogen cabinet and handled only by perimeter edge with vacuum wands or PTFE/PEEK tweezers, adding infrastructure and training requirements.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

25 pcs

Diameter

2-Inch (50.8 ± 0.2 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

P-Type / Boron (B)

Orientation

± 0.5°

Resistivity

10-20 Ω·cm

Thickness

275 ± 25 μm

Surface Finish

Single-Side Polished (SSP, Ra < 0.5 nm)