2-Inch P-Type Silicon Wafer 10-20 Ω·cm DSP ATOMFAIR®

$349.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Prime CZ P-Type silicon wafer, 50.8 mm, 275 μm, 10–20 Ω·cm, DSP Ra<0.5 nm. SEMI M1 flats, 25 pcs cassette. In stock.

Diameter & Flat:
2-Inch (50.8 ± 0.2 mm)
Primary Flat 15.88 mm <110>
Substrate & Dopant:
CZ P-Type / Boron (B)
<111>•10–20 Ω·cm
Thickness:
275 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
DSP (Ra < 0.5 nm)
Dual-Side Mirror-Polished (CMP)

1. Scientific Overview & Substrate Electrical Properties

2-Inch (50.8 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 10–20 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 50.8 ± 0.2 mm diameter and 275 ± 25 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).

Boron-doped to 10–20 Ω·cm (~1015 cm-3 dopant density), this moderate-resistivity substrate minimizes impurity scattering and junction capacitance compared with heavily doped wafers, supporting MOS C-V gate characterization, minority-carrier diffusion studies, and photodiode test structures.

Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D.

2-Inch Chamber Compatibility & Surface State Note: The compact 2-inch (50.8 mm) footprint fits research-scale tube furnaces, compact ALD/PECVD chambers, R&D spin coaters, and 2-inch sputtering sample holders without dicing waste. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Double-Side Polished (DSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)
SEMI M1 2-Inch Dimensional Precision

Standardized 50.8 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.

  • Diameter: 50.8 ± 0.2 mm (2.0 Inch)
  • Primary Flat: 15.88 ± 1.65 mm along <110> ± 1°
  • Secondary Flat: None (SEMI M1 standard for 50.8 mm P-type <111>)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant P-Type / Boron (B) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 10–20 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <111> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 50.8 ± 0.2 mm (2-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 275 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 15.88 ± 1.65 mm SEMI M1 (50.8 mm)
Secondary Flat None (SEMI M1 standard for 50.8 mm P-type <111>) SEMI M1 (50.8 mm P<111>)
Surface Polish & Roughness Double-Side Polished (DSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Pack Size (MOQ) 25 pcs (1 × 25-wafer cleanroom cassette, 25BX) Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications
  • Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm) supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding;
  • Hexagonal Epitaxy & UHV Surface Physics: Dense three-fold <111> crystal lattice supports lattice-matched GaN/AlN/SiC heteroepitaxy, graphene/TMDC template growth, and discrete bipolar/power prototyping;
  • Semiconductor Device & Electrode Prototyping: Controlled Boron-doped (10–20 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol

Wafers are supplied in a standard 25-wafer protective cleanroom cassette (25 pcs pack, 25BX) engineered to immobilize 2-inch wafer edges and prevent surface contact during transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 2-Inch (50.8 mm), P-Type (111), 10-20 ohm-cm, 275 um, DSP (This Product) 2-Inch (50.8 mm) / DSP 275 ± 25 μm, P-Type (10–20 Ω·cm) SEMI M1 275 μm thickness, 25 pcs cassette for 2-inch R&D chambers
2-Inch P-Type <100> Wafer (1–10 Ω·cm SSP) 2-Inch (50.8 mm) / SSP 275 ± 25 μm, P-Type <100> Standard 50.8 mm P<100> bare lithography substrate
2-Inch P-Type <100> Wafer (1–10 Ω·cm DSP) 2-Inch (50.8 mm) / DSP 275 ± 25 μm, P-Type <100> Double-side CMP polished for IR optics & bonding
2-Inch N-Type <100> Wafer (1–10 Ω·cm SSP) 2-Inch (50.8 mm) / SSP 275 ± 25 μm, N-Type <100> Phosphorus-doped N<100> wafer for Schottky & diode R&D
2-Inch P-Type <111> Wafer (1–10 Ω·cm SSP) 2-Inch (50.8 mm) / SSP 275 ± 25 μm, P-Type <111> Hexagonal <111> lattice for III-nitride & UHV growth

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 2-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original 25-wafer polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Prime-grade monocrystalline silicon wafers require particulate-controlled storage and edge-only manipulation to preserve CMP surface quality. Ambient native oxide growth and contamination risks dictate sealed dry-nitrogen storage and cleanroom-compatible handling protocols.

  • Native Oxide Formation: Bare prime silicon forms an ambient native silicon dioxide film of approximately 1–2 nm in air, which must be removed by wet processing or plasma descum prior to metallization or epitaxial growth.
  • Particulate and Vapor Contamination Control: Wafers must be stored sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors to prevent surface contamination.
  • Edge-Only Handling Requirement: Handling must be strictly limited to the wafer perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface contact and CMP finish degradation.
  • Wet Processing Safety Compliance: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols within an exhaust fume hood or wet bench.

Proper pre-cleaning and handling preserve the dual-side CMP finish and ensure reproducible thin-film interfaces. Sequential solvent degreasing, plasma descum, and controlled storage minimize organic and particulate contamination.

Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Exhaust fume hood or wet bench, O2 plasma descum system, Dry nitrogen cabinet or cleanroom desiccator

  1. Inspect wafer cassette
    Inspect the sealed 25-wafer cleanroom cassette for integrity and verify the lot-specific Certificate of Analysis before opening.
  2. Transfer wafer by edge
    Transfer the wafer strictly by its perimeter edge using a cleanroom vacuum wand or PTFE/PEEK tweezers.
  3. Degrease sequentially
    Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and deionized water.
  4. Blow-dry with nitrogen
    Blow-dry the wafer with nitrogen gas to remove residual solvent and moisture.
  5. Perform plasma descum
    Perform a mild oxygen plasma descum to remove organic residues prior to photoresist spin coating or PVD/ALD deposition.
  6. Remove native oxide if required
    Remove the native oxide by wet processing inside an exhaust fume hood or wet bench using facility-approved protocols when metallization or epitaxy requires an oxide-free interface.
  7. Store unused wafers sealed
    Store unused wafers sealed inside the original polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Why choose a <111> orientation P-type silicon wafer with 10–20 Ω·cm resistivity instead of a standard <100> wafer?

The <111> orientation provides a densely packed three-fold surface symmetry with a higher in-plane elastic modulus along key cleavage directions and slower wet alkaline etch kinetics than <100> silicon, making it preferable for III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D. The 10–20 Ω·cm boron doping (~10^15 cm⁻³) minimizes impurity scattering and junction capacitance compared with heavily doped wafers, supporting MOS C-V gate characterization, minority-carrier diffusion studies, and photodiode test structures. Standard <100> wafers remain the default for conventional lithography, but <111> is specified when hexagonal lattice matching or anisotropic etch behavior is required.

Can this 2-inch DSP silicon wafer be used for double-side lithography and wafer bonding?

Yes. The dual-side CMP mirror finish (DSP, Ra < 0.5 nm) supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding. The 275 ± 25 μm thickness and SEMI M1 flats (50.8 ± 0.2 mm diameter, 15.88 ± 1.65 mm primary flat along <110> ± 1°) ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes. For bonding, the sub-nanometer roughness provides reproducible thin-film growth and lithography interfaces.

What handling and storage precautions are required for bare prime silicon wafers with native oxide?

Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), so wafers must be stored sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors to minimize airborne organic contamination. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers; the supplied 25-wafer polypropylene cassette immobilizes edges and prevents surface contact during transit. For native oxide removal or RCA standard clean before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols and institutional EHS/SDS safety guidelines.

The 2-inch P-type <111> prime CZ silicon wafer with 10–20 Ω·cm resistivity and dual-side CMP finish (Ra < 0.5 nm) is purpose-built for hexagonal epitaxy, double-side lithography, and UHV surface physics, while its moderate doping and 275 µm thickness suit MOS C-V and minority-carrier studies. However, deployment requires cleanroom-compatible handling, dry nitrogen storage, and wet-bench infrastructure for native oxide removal, with the 25-wafer cassette MOQ imposing a minimum batch commitment.

Positive

  • Dual-Side CMP Enables Bonding and IR Optics: Double-side mirror-polished surfaces with Ra < 0.5 nm support direct fusion/anodic bonding, double-sided MEMS patterning, and through-wafer infrared transmission without additional surface preparation.
  • <111> Lattice for Hexagonal Epitaxy: The densely packed <111> crystal plane provides three-fold surface symmetry and slower alkaline etch kinetics, facilitating lattice-matched GaN/AlN/SiC heteroepitaxy and UHV surface reconstruction studies.

Trade-offs

  • Native Oxide Requires Wet-Bench Removal: Bare prime silicon forms a 1–2 nm ambient native SiO2 layer that must be removed via RCA clean or wet etching inside an exhaust fume hood or wet bench before metallization or epitaxy, adding facility and safety infrastructure requirements.
  • Cleanroom Storage and Handling Mandate: Wafers must be stored sealed in a dry nitrogen cabinet or cleanroom desiccator and handled only by the perimeter edge with vacuum wands or PTFE/PEEK tweezers to prevent particulate contamination and surface damage.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

25 pcs

Diameter

2-Inch (50.8 ± 0.2 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

P-Type / Boron (B)

Orientation

± 0.5°

Resistivity

10-20 Ω·cm

Thickness

275 ± 25 μm

Surface Finish

Double-Side Polished (DSP, Ra < 0.5 nm)